POLYESTER FIBER AND METHOD FOR MANUFACTURING THE SAME

    公开(公告)号:JP2002173823A

    公开(公告)日:2002-06-21

    申请号:JP2000367243

    申请日:2000-12-01

    Abstract: PROBLEM TO BE SOLVED: To provide a new polyester self-elongative fiber having large self- elongative performance and excellent productivity and a method for manufacturing the same. SOLUTION: A polyester fiber having a birefringence of 0.015-0.070 is treated with a treating agent composed mainly of carbon dioxide in an atmosphere of a pressure of 3-50 MPa and a temperature of 0-130 deg.C to obtain a polyester fiber exhibiting a peak temperature of 100-140 deg.C and an endothermic peak having a transfer heat quantity of 3-30 J/g determined by differential scanning calorimetry(DSC).

    DYE COMPOSITION AND METHOD FOR DYEING FIBER STRUCTURE

    公开(公告)号:JP2001172524A

    公开(公告)日:2001-06-26

    申请号:JP36060999

    申请日:1999-12-20

    Abstract: PROBLEM TO BE SOLVED: To provide a dye composition which can provide a dyed article having a fastness superior to that obtained by prior art and to provide a method for dyeing a fiber structure by using the dye composition. SOLUTION: This dye composition comprises a dye having a mol.wt. of 550 or higher and contained in a supercritical fluid of which the medium is carbon dioxide. The method for dyeing a fiber structure comprises treating the fiber structure in the dye composition.

    DEVICE AND METHOD FOR MANUFACTURING HOLLOW FIBER MEMBRANE

    公开(公告)号:JP2006239643A

    公开(公告)日:2006-09-14

    申请号:JP2005061945

    申请日:2005-03-07

    Abstract: PROBLEM TO BE SOLVED: To provide the manufacturing method and the manufacturing device of a hollow fiber membrane having excellent roundness. SOLUTION: By using the manufacturing device of hollow fiber membrane which is provided with a mouth piece for ejecting a membrane forming raw liquid together with a hollow part forming fluid, a coagulation bath for coagulating the membrane forming raw liquid after ejection, and a touch roller and a first roller for changing a thread passage of a coagulated hollow fiber membrane in order to spin the hollow fiber membrane, the hollow fiber membrane is manufactured. Therein, the length of the hollow fiber membrane between the touch roller and the first roller is made to be 1.01 times to 1.5 times of the length of a tangential connecting the touch roller and the first roller so as to be shortest from a point on each of both circumferences. COPYRIGHT: (C)2006,JPO&NCIPI

    分離膜
    6.
    发明专利
    分離膜 审中-公开

    公开(公告)号:JP2019093366A

    公开(公告)日:2019-06-20

    申请号:JP2017227080

    申请日:2017-11-27

    Abstract: 【課題】精密ろ過膜、限外ろ過膜、ナノろ過膜および逆浸透膜等の分離膜を支持する際の優れた製膜性と、流体分離素子製造時に優れた加工性を有することに加え、優れた機械的強度を有しかつ剥離強度が高く、剥離抑制可能な分離膜の提供。【解決手段】熱可塑性連続フィラメントで構成された長繊維不織布からなる分離膜支持体上に、分離機能を有する膜が形成されてなる分離膜であって、前記分離膜支持体と前記膜の界面間におけるマクロボイドの割合が30%以下の分離膜であり、前記分離膜支持体の密度が0.70〜0.95g/cm3であり、かつ最大ポアサイズ径が18μm以上である。【選択図】なし