    Abstract: The present application describes a method for repairing worn portions (15) in a metal part comprising the steps of providing a metal part (13) having a worn portion (15), cleaning the worn portion (15) to remove an oxide layer, depositing a restoration alloy to cover the worn portion (15) via a deposition process selected from the group consisting of cathodic arc deposition and Low Pressure Plasma Spray (LPPS) deposition.

    NICKEL ALLOY WELDING WIRE
    3.
    发明专利

    公开(公告)号:SG136035A1

    公开(公告)日:2007-10-29

    申请号:SG2007009343

    申请日:2007-02-07

    Abstract: In accordance with a first embodiment of the present invention, a nickel alloy welding wire is made from a material comprising from about 4.75 to 5.25 wt% chromium, from about 5.5 to 5.8 wt% aluminum, from about 5.6 to 6.2 wt% tungsten, from about 8.0 to 8.3 wt% tantalum, from about 1.7 to 2.1 wt% molybdenum, from about 9.5 to 10.5 wt% cobalt, from about 2.8 to 3.2 wt% rhenium, from about 0.07 to 0.30 wt% carbon, from about 0.02 to 0.04 wt% boron, from about 0.08 to 0.12 wt% zirconium, from about 0.08 to 0.12 wt% yttrium, from about 1.0 to 1.5 wt% hafnium, and the balance nickel. In a second embodiment of the present invention, a nickel alloy welding wire is made from a material comprising from about 4.75 to 5.25 wt% chromium, from about 5.5 to 5.8 wt% aluminum, from about 5.6 to 6.2 wt% tungsten, from about 8.0 to 9.0 wt% tantalum, from about 1.7 to 2.1 wt% molybdenum, from about 9.5 to 10.5 wt% cobalt, from about 2.8 to 3.2 wt% rhenium, from about 0.18 to 0.30 wt% carbon, from about 0.02 to 0.04 wt% boron, from about 0.08 to 0.12 wt% zirconium, from about 0.08 to 0.12 wt% yttrium, from about 1.0 to 1.5 wt% hafnium, and the balance nickel.

Patent Agency Ranking