Abstract:
A toner includes a polymeric resin, a colorant, and a small molecule crystalline aromatic monoester having a molecular weight less than 1,000 g/mol. The polymeric resin may be an amorphous resin and a mixture of the amorphous resin and the crystalline aromatic monoester may be characterized by a reduction in glass transition temperature from that of the resin and by the lack of a melting point for the crystalline aromatic monoester as determined by differential scanning calorimetry, the enthalpy of fusion for the crystalline aromatic monoester in the mixture being measured to be less than 10% of the enthalpy of fusion of the crystalline aromatic monoester in pure form. Furthermore, the toner may be configured to have a crease fix minimum fusing temperature (MFT) less than or equal to the crease fix MFT of a benchmark ultra-low-melt emulsion aggregation toner. Suitable crystalline aromatic monoesters may include 2-Naphthyl benzoate.
Abstract:
A toner includes a polymeric resin, optionally a colorant, and a small molecule crystalline diester having an aromatic core and a molecular weight less than 1,000 g/mol. The polymeric resin may be an amorphous resin and a mixture of the amorphous resin and the crystalline aromatic diester may be characterized by a reduction in glass transition temperature from that of the resin and by the lack of a significant solid to liquid phase transition peak for the small molecule compound as determined by differential scanning calorimetry, the enthalpy of fusion for the small molecule compound in the mixture being measured to be less than 10% of the enthalpy of fusion of the compound in pure form. Furthermore, the toner may be configured to have a crease fix minimum fusing temperature (MFT) less than or equal to the crease fix MFT of a benchmark ultra-low-melt emulsion aggregation toner.
Abstract:
A copolymer for use in 3D printing includes about 1 to about 30 mole percent of a diacid monomer unit, a diol monomer unit, and a terephthalate monomer unit, the copolymer having a glass transition temperature (Tg) in a range from about 50° C. to about 95° C.
Abstract:
The disclosure provides pigment dispersions having an average particle size of from about 10 nm to about 500 nm prepared by employing a magnetic actuated milling process and system. In embodiments, the pigment dispersions have an average particle size of less than 100 nm.
Abstract:
A toner includes a polymeric resin, optionally a colorant, and a small molecule crystalline aromatic ether having a molecular weight less than 1,000 g/mol. The polymeric resin may be an amorphous resin and a mixture of the amorphous resin and the crystalline aromatic ether may be characterized by a reduction in glass transition temperature from that of the resin and by the lack of a melting point for the crystalline aromatic ether as determined by differential scanning calorimetry, the enthalpy of fusion for the crystalline aromatic ether in the mixture being measured to be less than 10% of the enthalpy of fusion of the crystalline aromatic ether in pure form. Furthermore, the toner may be configured to have a crease fix minimum fusing temperature (MFT) less than or equal to the crease fix MFT of a benchmark ultra-low-melt emulsion aggregation toner. Suitable crystalline aromatic ethers may include benzyl 2-naphthyl ether.
Abstract:
A polyesteramide for use in 3D printing includes about 1 to about 30 mole percent of a diamine monomer unit, a diol monomer unit, and a terephthalate monomer unit, the polyesteramide having a glass transition temperature (Tg) in a range from about 50° C. to about 95° C.
Abstract:
A toner includes a polymeric resin, a colorant, and a small molecule crystalline aromatic monoester having a molecular weight less than 1,000 g/mol. The polymeric resin may be an amorphous resin and a mixture of the amorphous resin and the crystalline aromatic monoester may be characterized by a reduction in glass transition temperature from that of the resin and by the lack of a melting point for the crystalline aromatic monoester as determined by differential scanning calorimetry, the enthalpy of fusion for the crystalline aromatic monoester in the mixture being measured to be less than 10% of the enthalpy of fusion of the crystalline aromatic monoester in pure form. Furthermore, the toner may be configured to have a crease fix minimum fusing temperature (MFT) less than or equal to the crease fix MFT of a benchmark ultra-low-melt emulsion aggregation toner. Suitable crystalline aromatic monoesters may include 2-Naphthyl benzoate.