Low-loss UV to mid IR optical tellurium oxide glass and fiber for linear, non-linear and active devices
    1.
    发明授权
    Low-loss UV to mid IR optical tellurium oxide glass and fiber for linear, non-linear and active devices 有权
    低损耗UV至中红外光学碲氧化物玻璃和光纤用于线性,非线性和有源器件

    公开(公告)号:US08805133B1

    公开(公告)日:2014-08-12

    申请号:US13745028

    申请日:2013-01-18

    Abstract: A tellurium oxide glass that is stable, strong and chemically durable exhibits low optical loss from the UV band well into the MIR band. Unwanted absorption mechanisms in the MIR band are removed or reduced so that the glass formulation exhibits optical performance as close as possible to the theoretical limit of a tellurium oxide glass. The glass formulation only includes glass constituents that provide the intermediate, modifiers and any halides (for OH— reduction) whose inherent absorption wavelength is longer than that of Tellurium (IV) oxide. The glass formulation is substantially free of Sodium Oxide and any other passive glass constituent including hydroxyl whose inherent absorption wavelength is shorter than that of Tellurium (IV) oxide. The glass formulation preferably includes only a small residual amount of halide.

    Abstract translation: 稳定,坚固和化学耐久的氧化碲玻璃表现出从UV带到MIR带的低光损耗。 去除或减少MIR带中的不需要的吸收机制,使得玻璃配方表现出尽可能接近氧化碲玻璃的理论极限的光学性能。 玻璃制剂仅包括玻璃成分,其提供其固有吸收波长比氧化碲(IV)的中间体,改性剂和任何卤化物(用于OH-还原)。 玻璃制剂基本上不含氧化钠和任何其它钝化玻璃组分,其中包括羟基的固有吸收波长比氧化碲(IV)的那些慢。 玻璃制剂优选仅包含少量的卤化物。

    PHOTONIC BAND GAP FIBERS USING A JACKET WITH A DEPRESSED SOFTENING TEMPERATURE
    8.
    发明申请
    PHOTONIC BAND GAP FIBERS USING A JACKET WITH A DEPRESSED SOFTENING TEMPERATURE 有权
    使用带有柔软温度的夹克的光子带隙纤维

    公开(公告)号:US20120141079A1

    公开(公告)日:2012-06-07

    申请号:US12960638

    申请日:2010-12-06

    Abstract: The present invention is generally directed to a photonic bad gap fiber and/or fiber preform with a central structured region comprising a first non-silica based glass and a jacket comprising a second non-silica based glass surrounding the central structured region, where the Littleton softening temperature of the second glass is at least one but no more than ten degrees Celsius lower than the Littleton softening temperature of the first glass, or where the base ten logarithm of the glass viscosity in poise of the second glass is at least 0.01 but no more than 2 lower than the base ten logarithm of the glass viscosity in poise of the first glass at a fiber draw temperature. Also disclosed is a method of making a photonic bad gap fiber and/or fiber preform.

    Abstract translation: 本发明一般涉及具有中心结构化区域的光子不良间隙纤维和/或纤维预制件,该中心结构化区域包括第一非二氧化硅基玻璃和包含围绕中心结构化区域的第二非二氧化硅基玻璃的护套,其中Littleton 第二玻璃的软化温度比第一玻璃的利特尔顿软化温度低至少一个但不超过十摄氏度,或者第二玻璃的玻璃粘度的基准十对数至少为0.01,但是没有 在纤维拉伸温度下,第一玻璃的玻璃粘度的基数为10以下的基准值低于2。 还公开了制造光子不良间隙纤维和/或纤维预制件的方法。