Abstract:
Provided is a method for recovering gold in a cyanide tailing by hierarchical ramified flotation. The method divides a cyanide tailing into coarse and fine-grained products through screen classification, making preparation for hierarchical ramified flotation. The method then conducts flotation of the coarse and fine-grained products with suitable process parameters and reagent systems, and selects a suitable coarse-grained flotation product as a carrier of fine-grained flotation to maximize the recovery efficiency of fine grains. The method improves the overall recovery rate of gold with the hierarchical ramified flotation of coarse and fine grains, series-carrier flotation and combined reagent enhanced flotation. The method has an advanced process, a good separation effect, and can effectively recover fine-grained gold in the cyanide tailing.
Abstract:
This invention relates to an composition, comprising A) at least one quaternary ammonium compound which is a collector for the reverse flotation of magnesium minerals from calcium carbonate B) at least one antifoam agent C) a solvent and its use in the reverse flotation of calcium carbonate.
Abstract:
The present invention discloses thiol compositions containing monothiotricyclodecenes, dithiotricyclodecanes, and intermolecular sulfide compounds, as well as mining chemical collector compositions containing such thiol compositions. Flotation processes for recovering metals, such as copper and molybdenum, from ores using the mining chemical collector compositions also are disclosed.
Abstract:
Cationic reverse flotation methods, systems, and processes for producing a marketable iron oxide concentrate from an iron oxide mineral slurry (“treatment slurry”), wherein the iron oxide content of the concentrate is greater than the iron oxide content of the treatment slurry, include introducing the treatment slurry into a flotation cell, together with a collector, a frother and optionally an iron oxide depressant, and recovering two flow streams from the flotation cell, namely a froth fraction (also referred to as a flotation tail fraction) and a sink material fraction (also referred to as the flotation concentrate), wherein the treatment slurry in the flotation cell is maintained at a Natural pH.
Abstract:
The present invention relates to a method for the flotation of silicates from ores in the presence of a collecting agent and an effective amount of a froth modifier/collecting booster comprising at least one of the compounds of general formula (I) or mixtures thereof: wherein X is C1-C3 alkyl; R′ is straight or branched hydrocarbyl group containing 8 to 22 carbon atoms; n is integer from 2-4; m can vary from 0 to 2 and R′ is X or —(CH2)n-N(X)2, with the proviso that when R′ is —(CH2)n-N(X)2, then m is 1.
Abstract:
Methods of enhancing recovery of value sulfide or precious minerals from an ore containing Mg-silicate, slime forming minerals, and/or clay by subjecting the ore to a flotation process performed under acidic conditions, in conjunction with the addition of a froth phase modifier agent to the ore, are provided herein.
Abstract:
The invention provides methods and compositions for improving a froth flotation type separation. The method uses a thickener to improve the effectiveness of an emulsifier. The improvement allows for low dosages of emulsifier to work well so the emulsifier does not cancel out the effectiveness of other additives in the slurry such as collectors, frothing agents, regulators, depressors, deactivators, and/or activators.
Abstract:
In a method for recovering a copper sulfide concentrate by froth flotation from an ore containing an iron sulfide, wet grinding of the ore with grinding media made of high chromium cast iron alloy having a chromium content of from 10 to 35% by weight is combined with an addition of hydrogen peroxide to the conditioned mineral pulp before or during flotation in order to improve concentrate grade and recovery of copper sulfides.