Abstract:
A higher-strength, non-grain-oriented electrical strip with high polarization, the electrical strip consisting of a steel alloy, wherein the limits of the following elements are maintained: Mn between 0.35 mass % and 0.65 mass %, Si between 2.0 mass % and 3.0 mass %, Al between 0.8 mass % and 1.4 mass %, and P between 0.14 mass % and 0.24 mass %; and a method for the production thereof.
Abstract:
In the production of a grain-oriented electrical steel sheet by hot rolling a steel slab comprising C: 0.001˜0.10 mass %, Si: 1.0˜5.0 mass %, Mn: 0.01˜0.5 mass %, sol. Al: 0.003˜0.050 mass %, N: 0.0010˜0.020 mass %, one or two selected from S and Se: 0.005˜0.040 mass % in total, cold rolling, primary recrystallization annealing, and final annealing, a heating rate S1 between a temperature T1 (° C.): 500+2×(NB−NA) and a temperature T2 (° C.): 600+2×(NB−NA) in a heating process of the primary recrystallization annealing is set to not less than 80° C./sec, and an average heating rate S2 from the temperature T2 to 750° C. is set to 0.1˜0.7 times of S1, whereby a grain-oriented electrical steel sheet having a low iron loss over a full length of a product coil is obtained.
Abstract:
A resist film is formed on a cold-rolled steel sheet so as to fabricate a groove by etching. At this point, a steel sheet exposed portion where a portion of the steel sheet is exposed is formed in the resist film, and the steel sheet exposed portion has a first region oriented in a sheet width direction, and a plurality of second regions starting from the first region, widths of the first region and the second regions being 20 μm to 100 μm, and a distance from an end portion of one of the second regions to an end portion of another of the second regions adjacent thereto being 60 μm to 570 μm.
Abstract:
When contents of Ti, V, Zr, Nb, and C (mass %) are represented as [Ti], [V], [Zr], [Nb], and [C] respectively, a value of a parameter Q represented by “Q=([Ti]/48+[V]/51+[Zr]/91+[Nb]/93)/([C]/12)” is not less than 0.9 nor more than 1.1. A matrix of a metal structure is a ferrite phase, and the metal structure does not include a non-recrystallized structure. An average grain size of ferrite grains constituting the ferrite phase is not less than 10 μm nor more than 200 μm. A precipitate containing at least one selected from the group consisting of Ti, V, Zr, and Nb exists with a density of 10 μm−3 or more in the ferrite grain. An average grain size of the precipitate is not less than 0.002 μm nor more than 0.2 μm.
Abstract:
To provide a grain oriented electrical steel sheet that can securely suppress propagation of lateral strain, and can make a product even from a portion where the lateral strain occurs. A grain oriented electrical steel sheet of the present invention has a linearly altered portion 14 generated in a glass coating film 12 at one of side edges of a steel sheet 11, in a continuous line or in a discontinuous broken line in a direction parallel with a rolling direction of the steel sheet, and having a composition different from a composition in other portions of the glass coating film. An average value of a deviation angle of a direction of an axis of easy magnetization of crystal grains relative to the rolling direction is 0° or more and 20° or less in a base metal iron portion of the steel sheet 11 at a position along a width direction of the steel sheet, the position corresponding to the linearly altered portion 14.
Abstract:
Disclosed is a hot-rolled steel sheet including, by mass %, C:0.02% to 0.5% of C, and the sum of the content of Si and the content of Al is 1.0% to 4.0%. An average pole density of an orientation group from {100} to {223} is 1.0 to 6.5, and a pole density of a crystal orientation {332} is 1.0 to 5.0. A microstructure includes, by of an area ratio, 2% to 30% of retained austenite, 20% to 50% of ferrite, and 10% to 60% of bainite. rC that is a Lankford value in a direction orthogonal to a rolling direction is 0.70 to 1.10, and r30 that is a Lankford value in a direction forming an angle of 30° with the rolling direction is 0.70 to 1.10.
Abstract:
There are provided a magnesium alloy material and a method for producing the magnesium alloy material. In a magnesium (Mg) alloy material having a sheet-shaped portion with a thickness of 1.5 mm or more, when a region having ¼ the thickness of the sheet-shaped portion in a thickness direction from a surface of the sheet-shaped portion is defined as a surface region and a remaining region is defined as an internal region, the ratio OF/OC of the basal plane peak ratio OF in the surface region to the basal plane peak ratio OC (degree of orientation of (002) planes) in the internal region satisfies 0.95≦OF/OC≦1.05. A sheet-shaped Mg alloy material is obtained by performing at least one pass of the rolling at a reduction ratio of 25% or more and the remaining passes of the rolling at a reduction ratio of 10% or more.
Abstract:
The present invention provides a nitrided steel member and manufacturing method thereof. the nitrided steel member including: an iron nitride compound layer formed on a surface of a steel member made of carbon steel for machine structural use or alloy steel for machine structural use, in which with regard to X-ray diffraction peak intensity IFe4N (111) of the (111) crystal plane of Fe4N and X-ray diffraction peak intensity IFe3N (111) of the (111) crystal plane of Fe3N obtained by measuring a surface of the nitrided steel member by X-ray diffraction, an intensity ratio represented by IFe4N(111)/{IFe4N (111)+IFe3N (111)} is 0.5 or more, and a thickness of the iron nitride compound layer is 2 to 17 μm.
Abstract:
A grain-oriented electrical steel sheet being a grain-oriented electrical steel sheet containing Si of 0.8 mass % to 7 mass %, Mn of 0.05 mass % to 1 mass %, B of 0.0005 mass % to 0.0080 mass %, each content of Al, C, N, S, and Se of 0.005 mass % or less, and a balance being composed of Fe and inevitable impurities and having a glass coating film made of composite oxide mainly composed of forsterite on the steel sheet surface, in which when glow discharge optical emission spectrometry (GDS) to the surface of a secondary coating film formed on the surface of the glass coating film under a predetermined condition is performed, a peak, of B, in emission intensity having a peak position in emission intensity different from a peak position, of Mg, in emission intensity is obtained and the peak position, of B, in emission intensity from the steel sheet surface is deeper than the peak position, of Mg, in emission intensity.
Abstract:
A method of manufacturing a grain oriented electrical steel sheet includes subjecting a steel slab to rolling to obtain a steel sheet, subjecting the steel sheet to decarburizing annealing, coating of an annealing separator mainly composed of MgO onto a surface of the steel sheet, and final annealing to obtain a grain oriented electrical steel sheet having at least 4.0 g/m2 of coating weight of forsterite coating formed on the surface of the steel sheet, 0.9 μm or less of the average grain size of the forsterite coating, and at least 1.91 T of magnetic flux density B8; and linearly irradiating a surface of the grain oriented electrical steel sheet this obtained with a laser having wavelength of 0.2 μm to 0.9 μm in a direction intersecting the rolling direction of the steel sheet.
Abstract translation:晶粒取向电工钢板的制造方法包括对钢板进行轧制以获得钢板,对钢板进行脱碳退火,将主要由MgO组成的退火分离器涂覆在钢板的表面上,最终 进行退火,得到在钢板表面形成的镁橄榄石涂层的涂层重量至少为4.0g / m 2的晶粒取向电工钢板,镁橄榄石涂层的平均粒径为0.9μm以下,至少为1.91T 的磁通密度B8; 并且在与钢板的轧制方向交叉的方向上用波长为0.2μm〜0.9μm的激光线取得的晶粒取向电工钢板的表面线性地照射。