Abstract:
The present invention relates to a process for producing moldings comprising (A) at least one lactam, (B) at least one activator, and (C) at least one catalyst, where (A) to (C) proceed through treatments comprising a) mixing of (A), (B), and (C), b) metering of (A), (B), and (C) into an apparatus for producing mixture droplets, and producing mixture droplets, and c) depositing the mixture droplets comprising (A), (B), and (C) on a belt, and d) producing moldings.
Abstract:
The present invention relates to a composite component comprising an unfoamed polymer phase and a foamed phase, and to a process for producing the same.
Abstract:
The present relates to nylon-5,10 molding compositions comprising A) from 40 to 90% by weight of a nylon-5,10, B) from 10 to 60% by weight of fiber-containing or mineral-containing fillers, C) from 0 to 20% by weight of further additives, where the total of the percentages by weight of components A) to C) is 100%. The present invention moreover relates to a process for the preparation of these molding compositions, to the use of these molding compositions for the production of moldings of any type, and to the resultant moldings, preferably motor vehicle bodywork parts or electronics components of any type, foils, and fibers.
Abstract:
Thermoplastic molding materials compriseA) from 30 to 98% by weight of a graft polymer ofa.sub.K) from 30 to 90% by weight of an elastomeric graft core, obtainable by copolymerization ofa.sub.K /1) from 80 to 99.99% by weight of a C.sub.1 -C.sub.10 -alkyl ester of acrylic acid,a.sub.K /2) from 0.01 to 20% by weight of a crosslinking monomer anda.sub.K /3) from 0 to 40% by weight of one or more further monomers, anda.sub.S) from 10 to 70% by weight of a graft shell ofa.sub.S /1) from 50 to 100% by weight of a styrene compound of the general formula ##STR1## where R.sup.1 and R.sup.2 are each hydrogen or C.sub.1 -C.sub.8 -alkyl, and/or of a C.sub.1 -C.sub.8 -alkyl ester of acrylic acid or methacrylic acid, anda.sub.S /2) from 0 to 50% by weight of one or more further monomers,B) from 1 to 50% by weight of a thermoplastic polymer ofb.sub.1) from 50 to 100% by weight of styrene and/or .alpha.-methylstyrene,b.sub.2) from 0 to 50% by weight of acrylonitrile andb.sub.3) from 0 to 50% by weight of one or more further monomers, andC) from 1 to 70% by weight of a copolymer ofc.sub.1) from 30 to 90% by weight of styrene and/or .alpha.-methylstyrene,C.sub.2) from 10 to 70% by weight of butadiene andC.sub.3) from 0 to 30% by weight of one or more further monomers,in which all or virtually all of the olefinic double bonds have been hydrogenated.
Abstract:
The present relates to nylon-5,10 molding compositions comprising A) from 40 to 90% by weight of a nylon-5,10, B) from 10 to 60% by weight of fiber-containing or mineral-containing fillers, C) from 0 to 20% by weight of further additives, where the total of the percentages by weight of components A) to C) is 100%. The present invention moreover relates to a process for the preparation of these molding compositions, to the use of these molding compositions for the production of moldings of any type, and to the resultant moldings, preferably motor vehicle bodywork parts or electronics components of any type, foils, and fibers.
Abstract:
The present invention relates to a process for the production of polymer mixtures of i) polypropylene carbonate and ii) at least one further polymer, including the following steps: (a) reaction of propylene carbonate with carbon dioxide in the presence of a zinc catalyst, cobalt catalyst, or lanthanoid catalyst—in excess propylene carbonate or in an aprotic non-water-miscible solvent, (b) addition of an aqueous acidic solution to the reaction mixture after termination of the reaction, (c) removal of the aqueous phase, (d) optionally washing of the remaining organic phase with water, (e) addition of polymer component ii), (f) degassing and drying of the resultant polymer mixture and optionally removal of the aprotic, non-water-miscible solvent, and (g) pelletization of the polymer melt.
Abstract:
The present invention relates to biodegradable polymer mixtures comprising i) 40% to 95% by weight, based on the total weight of components i to ii, of at least one polyester based on aliphatic or aliphatic and aromatic dicarboxylic acids and aliphatic dihydroxy compounds; ii) 5% to 60% by weight, based on the total weight of said components i to ii, of polyalkylene carbonate, particularly polypropylene carbonate; iii) 0% to 60% by weight, based on the total weight of said components i to iii, of at least one biodegradable homo- or copolyester selected from the group consisting of polylactic acid, polycaprolactone and polyhydroxyalkanoate, and/or of an inorganic or organic filler; iv) 0% to 10% by weight, based on the total weight of said components i to ii, of an epoxy-containing copolymer based on styrene, acrylic ester and/or methacrylic ester, and v) 0% to 15% by weight of an additive selected from the group consisting of lubricant, antiblocking agent, antistat, UV absorber, UV stabilizer, thermal stabilizer, dye, pigment, colorant, plasticizer, fertilizer and active crop protection ingredient. The present invention further relates to processes for producing biodegradable polymer mixtures, to the use of biodegradable polymer mixtures in the production of moldings, films or fibers and also moldings, films or fibers comprising biodegradable polymer mixtures.
Abstract:
Thermoplastic molding compositions comprisingA) from 10 to 99.99% by weight of at least one thermoplastic polyester, B) from 0.01 to 50% by weight of a hyperbranched polycarbonate having an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, Part 2), C) from 0 to 60% by weight of other additives, where the total of the percentages by weight of components A) to C) is 100%.
Abstract translation:热塑性模塑组合物,其包含A)10至99.99重量%的至少一种热塑性聚酯,B)0.01至50重量%的具有OH值为1至600mg KOH / g聚碳酸酯的超支化聚碳酸酯(至 DIN 53240,Part 2),C)0至60重量%的其它添加剂,其中组分A)至C)的重量百分比的总和为100%。
Abstract:
Process for preparation of block polymers of polyethylene terephthalate and of the polyamide composed of meta-xylylenediamine and adipic acid, and process for their preparation.
Abstract:
Thermoplastic molding compositions comprisingA) from 10 to 99.99% by weight of at least one thermoplastic polyester, B) from 0.01 to 50% by weight of a hyperbranched polycarbonate having an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, Part 2), C) from 0 to 60% by weight of other additives, where the total of the percentages by weight of components A) to C) is 100%.
Abstract translation:热塑性模塑组合物,其包含A)10至99.99重量%的至少一种热塑性聚酯,B)0.01至50重量%的具有OH值为1至600mg KOH / g聚碳酸酯的超支化聚碳酸酯(至 DIN 53240,Part 2),C)0至60重量%的其它添加剂,其中组分A)至C)的重量百分比的总和为100%。