公开(公告)号:US20230150865A1
公开(公告)日:2023-05-18
申请号:US18154041
申请日:2023-01-13
Applicant: OHARA INC.
Inventor: TOSHITAKA YAGI , KOHEI OGASAWARA , YUKI MOTOSHIMA , REIKA KOJIMA , YUTAKA YAMASHITA , NAOYUKI GOTO
CPC classification number: C03C10/0018 , C03C4/18 , C03C21/002 , C03C2204/00
Abstract: To provide a crystallized glass substrate including a surface with a compressive stress layer, where a stress depth DOLzero of the compressive stress layer, at which the compressive stress is 0 MPa, is 45 to 200 μm, a compressive stress CS on an outermost surface of the compressive stress layer is 400 to 1400 MPa, and a central stress CT determined by using curve analysis is 55 to 300 MPa.
-
公开(公告)号:US20210230048A1
公开(公告)日:2021-07-29
申请号:US17266111
申请日:2018-08-09
Applicant: OHARA INC.
Inventor: TOSHITAKA YAGI , KOHEI OGASAWARA , YUKI MOTOSHIMA , REIKA KOJIMA , YUTAKA YAMASHITA , NAOYUKI GOTO
Abstract: To provide a crystallized glass substrate including a surface with a compressive stress layer, where a stress depth DOLzero of the compressive stress layer, at which the compressive stress is 0 MPa, is 45 to 200 μm, a compressive stress CS on an outermost surface of the compressive stress layer is 400 to 1400 MPa, and a central stress CT determined by using curve analysis is 55 to 300 MPa.
-
公开(公告)号:US20210163339A1
公开(公告)日:2021-06-03
申请号:US17266996
申请日:2018-08-09
Applicant: OHARA INC.
Inventor: TOSHITAKA YAGI , KOHEI OGASAWARA , YUKI MOTOSHIMA , REIKA KOJIMA , YUTAKA YAMASHITA , NAOYUKI GOTO
IPC: C03C3/087
Abstract: To provide a crystallized glass substrate including a surface with a compressive stress layer, in which a compressive stress CS (MPa) on an outermost surface of the compressive stress layer is 400 to 1400 MPa, and DOL50%/DOLzero is 0.30 or more, where DOL50% (μm) is a depth at which the value of the compressive stress is 50% of the CS and DOLzero (μm) is a depth at which the value of the compressive stress is 0 MPa.
-
公开(公告)号:US20250122116A1
公开(公告)日:2025-04-17
申请号:US18834614
申请日:2023-01-31
Applicant: OHARA INC.
Inventor: NOZOMU ODA , SAYA KIKKAWA , KOHEI OGASAWARA
IPC: C03C10/00
Abstract: A crystallized inorganic composition article, comprising: an inorganic composition article having a transmittance of 50% or more at 550 nm when heated to [At+50]° C., where At (° C.) is a yield point, wherein in a raw glass, by mass % in terms of oxide, a content of a SiO2 component is 65.0% to 85.0%, a content of an Al2O3 component is 3.0% to 15.0%, a content of a P2O5 component is more than 0% to 5.0%, a content of a Li2O component is more than 5.0% to 15.0%, a content of a ZrO2 component is 0% to 10.0%, a content of a MgO component is 0% to 5.0%, [the content of the Al2O3 component/(a content of a K2O component+the content of the MgO component)] is more than 0 to 20.0, and [the content of the Li2O component/the content of the MgO component] is 8.0 or more.
-
公开(公告)号:US20230312402A1
公开(公告)日:2023-10-05
申请号:US18024490
申请日:2021-08-23
Applicant: OHARA INC.
Inventor: SAYA KIKKAWA , KOHEI OGASAWARA , TOSHITAKA YAGI
CPC classification number: C03C10/0027 , C03C10/0054 , C03C21/002 , C03C2204/00
Abstract: Provided are crystallized glass that is easy to process and in which a high compressive stress value can be obtained on a surface, and reinforced crystallized glass thereof. A crystallized glass containing at least one type selected from α-cristobalite and an α-cristobalite solid solution as a main crystal phase, in which, by mass % in terms of oxide, a content of a SiO2 component is 50.0% to 75.0%, a content of a Li2O component is 3.0% to 10.0%, a content of an Al2O3 component is 5.0% or more and less than 15.0%, and a content of a B2O3 component is more than 0% and 10.0% or less.
-
公开(公告)号:US20230312401A1
公开(公告)日:2023-10-05
申请号:US18024489
申请日:2021-08-23
Applicant: OHARA INC.
Inventor: SAYA KIKKAWA , KOHEI OGASAWARA , TOSHITAKA YAGI
IPC: C03C10/00
CPC classification number: C03C10/0027 , C03C10/0054 , C03C2204/00
Abstract: Provided is reinforced crystallized glass that has a high strength and is less likely to break. The reinforced crystallized glass includes a compressive stress layer on a surface, and [CS50 μm*(DOLzero−50)]/2 is 2000 or more, where CS50 μm (MPa) is a compressive stress at a depth of 50 μm from an outermost surface, and DOLzero (μm) is a stress depth when the compressive stress is 0 MPa.
-
公开(公告)号:US20230242439A1
公开(公告)日:2023-08-03
申请号:US18011187
申请日:2021-06-07
Applicant: OHARA INC.
Inventor: KOHEI OGASAWARA , TOSHITAKA YAGI
CPC classification number: C03C10/0045 , C03C10/0054 , C03C21/002 , C03C2204/00
Abstract: Reinforced crystallized glass characterized including crystallized glass as a base material, the crystallized glass containing, as expressed in terms of mol % on an oxide basis, 30.0% to 70.0% of an SiO2 component, 8.0% to 25.0% of an Al2O3 component, 2.0% to 25.0% of an Na2O component, 1.0% to 6.0% of an Li2O component, 0 % to 25.0% of an MgO component, 0% to 30.0% of a ZnO component, and 0% to 10.0% of a TiO2 component, in which a surface of the reinforced crystallized glass is formed with a compressive stress layer, and a depth (DOLzero) of the compressive stress layer is 60 μm or more.
-
公开(公告)号:US20230159384A1
公开(公告)日:2023-05-25
申请号:US18154042
申请日:2023-01-13
Applicant: OHARA INC.
Inventor: TOSHITAKA YAGI , KOHEI OGASAWARA , YUKI MOTOSHIMA , REIKA KOJIMA , YUTAKA YAMASHITA , NAOYUKI GOTO
CPC classification number: C03C21/002 , C03C4/18 , C03C10/0018 , C03C2204/00
Abstract: To provide a crystallized glass substrate including a surface with a compressive stress layer, in which a stress depth DOLzero of the compressive stress layer, at which the compressive stress is 0 MPa, is 45 to 200 μm, a compressive stress CS on an outermost surface of the compressive stress layer is 400 to 1400 MPa, and CS×DOLzero, which is a product of the compressive stress CS on the outermost surface and the stress depth DOLzero (μm), is 4.8×104 or more.
-
公开(公告)号:US20210139362A1
公开(公告)日:2021-05-13
申请号:US17043759
申请日:2019-03-13
Applicant: OHARA INC.
Inventor: MORIJI NOZAKI , TOSHITAKA YAGI , KOHEI OGASAWARA
Abstract: To obtain a crystallized glass member having a curved shape and provide a method for producing the same. A method for producing a crystallized glass member having a curved shape, including a deformation step for adjusting the temperature of a plate glass to a first temperature zone from higher than [At+40]° C. to [At+146]° C. or lower, where At is the yield point (° C.) of the plate glass and deforming at least part of the plate glass into a curved shape by external force acting on the plate glass while precipitating crystals from the plate glass.
-
-
-
-
-
-
-
-