Abstract:
This invention relates to an composition, comprising A) at least one quaternary ammonium compound which is a collector for the reverse flotation of magnesium minerals from calcium carbonate B) at least one antifoam agent C) a solvent and its use in the reverse flotation of calcium carbonate.
Abstract:
A stabilization process for an arsenic solution comprising thiosulfates, the process comprising: acidifying the arsenic solution to decompose the thiosulfates, to yield an acidified solution; oxidizing the acidified solution to oxidize residual As3+ to As5+ and reduced sulfur species to sulfates, to yield a slurry comprising elemental sulfur; separating elemental sulfur from the slurry to yield a liquid; oxidizing the liquid to oxidize residual reduced sulfur species, to yield an oxidized solution; and forming a stable arsenic compound from the oxidized solution.
Abstract:
This invention relates to a collector composition for the direct froth flotation of nonsulfide ores comprising a) 50-99 wt.-% of a mixture of fatty acids and b) 1-50 wt.-% of an N-acyl derivative of sarcosine of the formula (I) wherein R is a saturated or unsaturated hydrocarbon chain with 7 to 21 carbon atoms, wherein the mixture of comprises 10.0-35.0 wt.-% of fatty acid having a saturated C11 hydrocarbon group, 2.5-15.0 wt.-% of fatty acid having a saturated C13 hydrocarbon group, 10.0-25.0 wt.-% fatty acid having a monounsaturated C17 hydrocarbon group and 20.0-45.0 wt.-% fatty acid having a bisunsaturated C17 hydrocarbon group.
Abstract:
The present invention discloses water-based mining collector compositions containing dodecylmethyl sulfide. Floatation processes for recovering metals, such as copper and molybdenum, from ores using the mining chemical collector compositions also are disclosed.
Abstract:
A process is provided for separation of at least one metal sulfide from a mixed sulfide concentrate. The process includes: subjecting the mixed sulfide concentrate to flotation in which at least one sulfide including antimony, arsenic and a first metal is floated and at least one sulfide including a second metal is depressed. The flotation yields a first metal concentrate having the at least one sulfide including antimony, arsenic and the first metal and a second metal concentrate having the at least one sulfide including the second metal. The first metal concentrate is leached to yield a further concentrate and a leach solution. The further concentrate includes the first metal and the leach solution includes soluble antimony and soluble arsenic. The process further includes oxidizing the leach solution to yield an antimony precipitate and an arsenic solution, and forming a stable arsenic compound from the arsenic solution.
Abstract:
The present invention discloses thiol compositions containing monothiotricyclodecenes, dithiotricyclodecanes, and intermolecular sulfide compounds, as well as mining chemical collector compositions containing such thiol compositions. Flotation processes for recovering metals, such as copper and molybdenum, from ores using the mining chemical collector compositions also are disclosed.
Abstract:
The present invention relates to the use of branched fatty alcohol-based compounds selected from the group of fatty alcohols with 12-16 carbon atoms having a degree of branching of 1-3, and their alkoxylates with a degree of ethoxylation of up to 3, as secondary collectors for the froth flotation of non-sulfidic ores, incombination with a primary collector selected from the group of amphoteric and anionic surface active compounds.
Abstract:
Cationic reverse flotation methods, systems, and processes for producing a marketable iron oxide concentrate from an iron oxide mineral slurry (“treatment slurry”), wherein the iron oxide content of the concentrate is greater than the iron oxide content of the treatment slurry, include introducing the treatment slurry into a flotation cell, together with a collector, a frother and optionally an iron oxide depressant, and recovering two flow streams from the flotation cell, namely a froth fraction (also referred to as a flotation tail fraction) and a sink material fraction (also referred to as the flotation concentrate), wherein the treatment slurry in the flotation cell is maintained at a Natural pH.
Abstract:
Compounds of the formulae: RO—X—NH2 (Ia); RO—X—NH3+Y− (Ib); RO—X—NH—Z—NH2 (IIa); and RO—X—NH—Z—NH3+Y− (IIb), in which X is an aliphatic alkylene group containing 2 to 6 carbon atoms; Z is an aliphatic alkylene group containing 2 to 6 carbon atoms; Y− is an anion; and R is an aliphatic iso C13H27-group with average branching degree ranging from 1.5 to 3.5. The compounds are particularly suitable as flotation collectors for enriching an iron mineral from a silicate-containing iron ore.
Abstract:
The present invention relates to a method for the flotation of silicates from ores in the presence of a collecting agent and an effective amount of a froth modifier/collecting booster comprising at least one of the compounds of general formula (I) or mixtures thereof: wherein X is C1-C3 alkyl; R′ is straight or branched hydrocarbyl group containing 8 to 22 carbon atoms; n is integer from 2-4; m can vary from 0 to 2 and R′ is X or —(CH2)n-N(X)2, with the proviso that when R′ is —(CH2)n-N(X)2, then m is 1.