Abstract:
Disclosed is a method of making an optical fiber preform having at least one annular region of depressed refractive index. A tube of silica doped with fluorine and/or boron is overclad with silica soot. A core rod is inserted into the overclad tube and the resultant assembly is heated while chlorine flows between the tube and the core rod to clean the adjacent surfaces. When the soot sinters, the tube collapses onto and fuses to the rod. The resultant tubular structure is formed into an optical fiber which exhibits low attenuation as a result of the low seed count at the interface between the inner core and the region that is doped with florine and/or boron.
Abstract:
An optical transmission fiber comprising (1) a core of high refractive index composed of SiO.sub.2 -based glass containing at least one of GeO.sub.2, As.sub.2 O.sub.3, Sb.sub.2 O.sub.5, SnO.sub.2, TiO.sub.2, PbO and Bi.sub.2 O.sub.3, (2) a clad of low refractive index composed of SiO.sub.2 -based glass containing at least one of B.sub.2 O.sub.3, F, F/B.sub.2 O.sub.3 and F/P.sub.2 O.sub.5, and (3) an outermost jacket layer composed of SiO.sub.2 and/or SiO.sub.2 -based glass containing at least one of Al.sub.2 O.sub.3, TiO.sub.2, ZrO.sub.2 and HfO.sub.2.
Abstract translation:一种光传输光纤,包括(1)由包含GeO 2,As 2 O 3,Sb 2 O 5,SnO 2,TiO 2,PbO和Bi 2 O 3中的至少一种的SiO 2基玻璃构成的高折射率芯,(2)低折射率的包层,由 含有B 2 O 3,F,F / B 2 O 3和F / P 2 O 5中的至少一种的SiO 2系玻璃,以及(3)由SiO 2和/或SiO 2系玻璃构成的最外层,所述玻璃含有Al 2 O 3,TiO 2,ZrO 2和 HfO2。
Abstract:
Incorporation of fluorine into a porous silica body, such as an unsintered body produced by a sol-gel method, by VAD or OVPO, reduces or eliminates bubble or pore formation upon re-heating of the glass formed by sintering of the porous material. Effective fluorine concentrations are between 0.01 and 5% by weight. The invention can be used advantageously in producing preforms and optical fiber.
Abstract:
Glass preforms for optical fibers or the like having refractive index profiles which vary in stepped or graded fashion across the preform, are made from porous glass preforms by introducing a first dopant into the porous preform during manufacture, partially sintering the preform to selectively modify the internal surface area thereof, introducing a second vapor-infusible dopant into the selectively sintered preform to cause selective doping of the porous glass, and then consolidating the resulting doped preform to clear glass.
Abstract:
Technique for making glass having a predetermined refractive index profile using fluorine doping and fluorine etching. A substrate glass body is coated with a plurality of successively applied vapor deposited glass layers wherein each succeeding layer is built with a larger quantity of fluorine than the adjacent preceding layer. The amount of the doping in each layer is such as to achieve the desired refractive index profile. Fluorine etching is employed to provide a uniform core before the glass body is heat fused into a rod-like structure suitable for the preparation of light waveguides for use in optical communications technology.
Abstract:
A fluorine containing silicate glass substrate is heated to a temperature sufficiently high to permit fluorine to out-diffuse from the surface thereof. A surface region is formed having a gradient fluorine concentration in a direction perpendicular to the substrate surface, the region of lowest fluorine concentration having the highest refractive index. The resultant device is capable of functioning as an optical waveguide.
Abstract:
According to one example of the invention an optical fiber comprises: (i) silica based, rare earth doped core having a first index of refraction n1; (ii) at least one silica based cladding surrounding the core and having a second index of refraction n2, such that n1>n2; wherein at least one of the core or cladding is doped with Al2O3, such that the ratio of max wt % to min wt % of Al2O3 concentration is less than 2:1.
Abstract translation:根据本发明的一个示例,光纤包括:(i)具有第一折射率n1的二氧化硅基稀土掺杂的核; (ii)至少一个围绕所述芯并且具有第二折射率n2的基于二氧化硅的包层,使得n1> n2; 其中所述芯或包层中的至少一个掺杂有Al 2 O 3,使得最大wt%与Al 2 O 3浓度的最小重量%的比率小于2:1。
Abstract:
According to one example of the invention an optical fiber comprises: (i) silica based, rare earth doped core having a first index of refraction n1; (ii) at least one silica based cladding surrounding the core and having a second index of refraction n2, such that n1>n2; wherein at least one of the core or cladding is doped with Al2O3, such that the ratio of max wt % to min wt % of Al2O3 concentration is less than 2:1.
Abstract translation:根据本发明的一个示例,光纤包括:(i)具有第一折射率n 1的二氧化硅基稀土掺杂的核; (ii)至少一个二氧化硅基包层,其围绕所述芯并具有第二折射率n 2 2,使得n 1/2 2 n 2 ; 其中所述芯或包层中的至少一个掺杂有Al 2 O 3 3,使得Al 2 O 3的最大重量%与最小重量%的比例< / 3 3 3浓度小于2:1。
Abstract:
An optical fiber including: (i) a silica based, rare earth doped core having a first index of refraction n1; (ii) a silica based inner cladding surrounding the core and having a second index of refraction n2, such that n1>n2, said inner cladding having a plurality of air holes extending longitudinally through the length of said optical fiber; (iii) a silica based outer cladding surrounding said inner cladding and having a third index of refraction n3, such that n2>n3, wherein said optical fiber supports a single polarization mode within the operating wavelength range.
Abstract translation:一种光纤,包括:(i)具有第一折射率n 1的二氧化硅基稀土掺杂的芯; (ii)围绕所述芯并且具有第二折射率n 2 2的基于二氧化硅的内包层,使得n 1,N 2, 所述内包层具有沿所述光纤的长度纵向延伸的多个气孔; (iii)围绕所述内包层并具有第三折射率n 3 3的基于二氧化硅的外包层,使得n 2 N 3 N 3 其中所述光纤在工作波长范围内支持单一偏振模式。
Abstract:
An optical fiber including: (i) a silica based, rare earth doped core having a first index of refraction n1; (ii) a silica based inner cladding surrounding the core and having a second index of refraction n2, such that n1>n2, said inner cladding having a plurality of air holes extending longitudinally through the length of said optical fiber; (iii) a silica based outer cladding surrounding said inner cladding and having a third index of refraction n3, such that n2>n3, wherein said optical fiber supports a single polarization mode within the operating wavelength range.
Abstract translation:一种光纤,包括:(i)具有第一折射率n 1的二氧化硅基稀土掺杂的芯; (ii)围绕所述芯并且具有第二折射率n 2 2的基于二氧化硅的内包层,使得n 1,N 2, 所述内包层具有沿所述光纤的长度纵向延伸的多个气孔; (iii)围绕所述内包层并具有第三折射率n 3 3的基于二氧化硅的外包层,使得n 2 N 3 N 3 其中所述光纤在工作波长范围内支持单一偏振模式。