Glass ceramics having low rhodium levels
    34.
    发明授权
    Glass ceramics having low rhodium levels 有权
    具有低铑含量的玻璃陶瓷

    公开(公告)号:US09403715B2

    公开(公告)日:2016-08-02

    申请号:US14286307

    申请日:2014-05-23

    Abstract: A glass ceramic precursor glass and a glass ceramic having low levels of rhodium and a method of controlling the amount of rhodium in such glasses and glass ceramics. The precursor glass and glass ceramic contain from about 1 ppm to about 10 ppm and, in certain embodiments, from about 1 ppm to about 6 ppm rhodium. The method of controlling of reducing rhodium dissolution from a rhodium-containing material such as, for example, an alloy into a glass melt comprises controlling and/or lowering the partial pressure of oxygen at the rhodium-containing vessel/glass interface by imposing a high humidity condition around the external (non-glass-contact) surface of the rhodium-containing material. The lower concentration of rhodium minimizes its coloring effect on the white color of the glass ceramic.

    Abstract translation: 玻璃陶瓷前体玻璃和具有低水平铑的玻璃陶瓷和控制这种玻璃和玻璃陶瓷中铑的量的方法。 前体玻璃和玻璃陶瓷含有约1ppm至约10ppm,在某些实施方案中含有约1ppm至约6ppm的铑。 控制从含铑材料(例如合金)将铑溶解还原成玻璃熔体的方法包括通过施加高的温度控制和/或降低含铑容器/玻璃界面处的氧的分压 含铑材料的外部(非玻璃接触)表面附近的湿度条件。 较低浓度的铑使其对玻璃陶瓷的白色的着色效果最小化。

    GLASS CERAMICS HAVING LOW RHODIUM LEVELS
    35.
    发明申请
    GLASS CERAMICS HAVING LOW RHODIUM LEVELS 有权
    具有低铑水平的玻璃陶瓷

    公开(公告)号:US20140356628A1

    公开(公告)日:2014-12-04

    申请号:US14286307

    申请日:2014-05-23

    Abstract: A glass ceramic precursor glass and a glass ceramic having low levels of rhodium and a method of controlling the amount of rhodium in such glasses and glass ceramics. The precursor glass and glass ceramic contain from about 1 ppm to about 10 ppm and, in certain embodiments, from about 1 ppm to about 6 ppm rhodium. The method of controlling of reducing rhodium dissolution from a rhodium-containing material such as, for example, an alloy into a glass melt comprises controlling and/or lowering the partial pressure of oxygen at the rhodium-containing vessel/glass interface by imposing a high humidity condition around the external (non-glass-contact) surface of the rhodium-containing material. The lower concentration of rhodium minimizes its coloring effect on the white color of the glass ceramic.

    Abstract translation: 玻璃陶瓷前体玻璃和具有低水平铑的玻璃陶瓷和控制这种玻璃和玻璃陶瓷中铑的量的方法。 前体玻璃和玻璃陶瓷含有约1ppm至约10ppm,在某些实施方案中含有约1ppm至约6ppm的铑。 控制从含铑材料(例如合金)将铑溶解还原成玻璃熔体的方法包括通过施加高的温度控制和/或降低含铑容器/玻璃界面处的氧的分压 含铑材料的外部(非玻璃接触)表面附近的湿度条件。 较低浓度的铑使其对玻璃陶瓷的白色的着色效果最小化。

    COMPOSITIONS COMPRISING BIOACTIVE GLASS AND AMINO ACID

    公开(公告)号:US20240325264A1

    公开(公告)日:2024-10-03

    申请号:US18613904

    申请日:2024-03-22

    Abstract: A composition comprising an amino acid and a bioactive glass, in which the bioactive glass comprises 15-55 wt. % SiO2, 20-60 wt. % CaO, 0.1-15 wt. % ZrO2, and 5-30 wt. % P2O5, in which, when the composition is subjected to artificial saliva at 37° C., a bioactive crystalline phase is formed within 7 days. In some aspects, the bioactive crystalline phase is apatite, and the composition is a dentifrice or skin care composition. Methods comprising making the composition, making the bioactive glass, and applying the composition to a tooth or the skin. In some aspects, applying the composition to a tooth remineralizes enamel of the tooth, treats caries of the tooth, and/or treats dentin hypersensitivity of the tooth, and applying the composition to skin treats or reduces the appearance of one or more skin defects, such as wrinkles and blemishes.

Patent Agency Ranking