1.
公开(公告)号:US3785093A
公开(公告)日:1974-01-15
申请号:US3785093D
申请日:1970-12-21
Applicant: VERESCHAGIN L , KONYAFV J , DOVBNYA A , ASANNURI A , PALY P , POLYAKOV E , STEPANOVICH A , GEVORKOV G , OBLASTI L
Inventor: VERESCHAGIN L , KONYAFV J , STEPANOVICH A , ASANNURI A , DOVBNYA A , POLYAKOV E , OBLASTI L , PALY P , GEVORKOV G
CPC classification number: B24D3/08 , B01J3/062 , B01J2203/062 , B01J2203/0655 , B01J2203/0685
Abstract: The diamond and cement materials to be sintered are placed in a hermetic graphite sheathing which is, in turn, arranged inside a sheathing of some low-melting metal. The latter is to be made from a metal whose melting point is lower than the temperature at which diamond will be sintered with the cermet material. The filled-up graphite sheathing is placed into a high-pressure reaction chamber and heated up until the low-melting metal gets soft. Thereafter the temperature and the pressure are raised until they are adequate for diamond to be sintered with cermet material. The softened sheathing of the low-melting material is a hydrostatic medium which provides for a uniform distribution of pressure and temperature over the entire volume of materials being sintered.
Abstract translation: 将待烧结的金刚石和水泥材料放置在密封石墨护套中,其又布置在一些低熔点金属的护套内。 后者由熔点低于金刚石与金属陶瓷材料烧结的温度的金属制成。 将填充的石墨护套放入高压反应室中并加热直到低熔点金属变软。 此后,温度和压力升高直到它们足以使金刚石与金属陶瓷材料烧结。 低熔点材料的软化护套是静压介质,其在整个烧结材料的体积上提供均匀的压力和温度分布。