Abstract:
The present invention provides a process for producing pellet of EVOH comprising the steps of introducing an EVOH solution containing alcohol into an apparatus, contacting the solution with water in the apparatus to let out the alcohol with water and then letting out an EVOH hydrous composition from the above-mentioned apparatus (step 1); cutting the EVOH hydrous composition let out therefrom to obtain EVOH hydrous composition pellets (step 2); introducing the obtained EVOH hydrous composition pellets into a dryer to reduce a water content thereof (step 3); melt-kneading the pellets, whose water content is reduced, in an extruder (step 4); and cutting EVOH discharged from the extruder to obtain the pellet of EVOH (step 5). Thus, the EVOH hydrous composition obtained by removing alcohol without deteriorating the environment can be efficiently dried, and pellets having less thermal degradation in drying and a uniform shape can be obtained.
Abstract:
The present invention provides a resin composition having an oxygen scavenging function. The resin composition comprises 70 to 99.9 wt % of a polyvinyl alcohol resin (A) and 0.1 to 30 wt % of a thermoplastic resin (B) other than the polyvinyl alcohol resin (A), wherein the thermoplastic resin (B) has a carbon-carbon double bond and a functional group including a hetero atom, and an oxygen absorption rate of the resin composition is 0.001 ml/m2·day or more.
Abstract translation:本发明提供了具有除氧功能的树脂组合物。 树脂组合物包含聚乙烯醇树脂(A)70至99.9重量%和聚乙烯醇树脂(A)以外的热塑性树脂(B)0.1至30重量%,其中热塑性树脂(B)具有碳 碳双键和包含杂原子的官能团,并且树脂组合物的氧吸收速率为0.001ml / m 2·天或更多。
Abstract:
To provide a resin composition including: an ethylene-vinyl alcohol copolymer (A) having an ethylene content of from 15 to 65 mol % and a saponification degree of at least 95 mol %, a phosphoric acid salt (B) which can form a hydrate, and a conjugated polyene compound (C) having a boiling point of at least 150° C., wherein the resin composition comprises from 50 to 99 parts by weight of (A), from 1 to 50 parts by weight of (B) and from 0.00001 to 1 parts by weight of (C), based on 100 parts by weight of the total amounts of (A) and (B). This resin composition excels in gas barrier property and also in moisture resistance at high temperatures and high humidities. Therefore, it is suitable for food packaging containers to be retorted.
Abstract:
The present invention provides a resin composition having an oxygen scavenging function. The resin composition comprises 70 to 99.9 wt % of a polyvinyl alcohol resin (A) and 0.1 to 30 wt % of a thermoplastic resin (B) other than the polyvinyl alcohol resin (A), wherein the thermoplastic resin (B) has a carbon-carbon double bond and a functional group including a hetero atom, and an oxygen absorption rate of the resin composition is 0.001 ml/m2·day or more.
Abstract translation:本发明提供了具有除氧功能的树脂组合物。 树脂组合物包含聚乙烯醇树脂(A)70至99.9重量%和聚乙烯醇树脂(A)以外的热塑性树脂(B)0.1至30重量%,其中热塑性树脂(B)具有碳 碳双键和包含杂原子的官能团,并且树脂组合物的氧吸收速率为0.001ml / m 2以上。
Abstract:
The present invention provides a process for producing pellet of EVOH comprising the steps of introducing an EVOH solution containing alcohol into an apparatus, contacting the solution with water in the apparatus to let out the alcohol with water and then letting out an EVOH hydrous composition from the above-mentioned apparatus (step 1); cutting the EVOH hydrous composition let out therefrom to obtain EVOH hydrous composition pellets (step 2); introducing the obtained EVOH hydrous composition pellets into a dryer to reduce a water content thereof (step 3); melt-kneading the pellets, whose water content is reduced, in an extruder (step 4); and cutting EVOH discharged from the extruder to obtain the pellet of EVOH (step 5). Thus, the EVOH hydrous composition obtained by removing alcohol without deteriorating the environment can be efficiently dried, and pellets having less thermal degradation in drying and a uniform shape can be obtained.
Abstract:
The present invention provides a multilayered structure where an A layer made of an ethylene-vinyl alcohol copolymer resin (A) and a C layer made of a polypropylene resin (C) are laminated via a B layer made of an adhesive resin (B). The ethylene content of the ethylene-vinyl alcohol copolymer resin (A) is 20 to 60 mol %, and the saponification degree of the resin (A) is at least 90%. The melt flow rate (MFR) of the polypropylene resin (C) at 230° C. under a load of 2160 g is in the range from 0.1 to 100 g/10 min, and the stereoregularity index [M5] of the polypropylene resin (C) is at least 0.950. Such a multilayered structure has excellent gas barrier properties and moldability.
Abstract:
The present invention provides a multilayered pipe for hot water circulation having excellent oxygen barrier properties and anti-crack properties, in particular, excellent anti-crack properties at low temperatures by using a thermoplastic resin composition comprising 50 to 99% by weight of an ethylene-vinyl alcohol copolymer (A) and 1 to 50% by weight of multilayered polymer particles (B).
Abstract:
A laminated structure comprising a base material comprising polyvinyl chloride resin, polystyrene resin, polyacrylic resin, polycarbonate resin and polyamide resin; having provided on at least one surface thereof a layer of a blend of a polyesteramide and an EVOH. In this laminated structure the base material layer and the EVOH layer adhere firmly to each other, and the structure is exhibits excellent gas barrier properties, prevention of plasticizer bleeding and soil prevention, and is useful as wall paper, portfolio, desk mat, etc.
Abstract:
To provide a resin composition comprising an ethylene-vinyl alcohol copolymer (A) having an ethylene content of from 15 to 65 mol % and a degree of saponification of 95 mol % or more, a phosphoric acid salt (B) which can form a hydrate, and a dispersing agent (C), wherein the dispersing agent (C) comprises at least one species selected from the group consisting of aliphatic acid salts, glycerol aliphatic acid esters and aliphatic acid amides, the resin composition comprises (A) and (B) in amounts of from 50 to 99 parts by weight and from 1 to 50 parts by weight, respectively, based on 100 parts by weight of (A) and (B) in total, and the resin composition comprises (C) in an amount of from 1 to 20 parts by weight based on 100 parts by weight of (B). This resin composition excels in gas barrier property and also in moisture resistance at high temperatures and high humidities. Therefore, it is suitable for food packaging containers to be retorted.
Abstract:
A resin composition comprising 70 to 99.9% by weight of ethylene-vinyl alcohol copolymer (A) and 0.1 to 30% by weight of a thermoplastic resin (B) other than the ethylene-vinyl alcohol copolymer (A) is provided. In the resin composition, an ethylene content ETa (mol %) and a degree of saponification SDa (%) of the ethylene-vinyl alcohol copolymer (A) satisfy the following equations (1) and (2): 25≦ETa≦55 (1) 90≦SDa