Laminated film
    1.
    发明授权
    Laminated film 有权
    层压膜

    公开(公告)号:US09200126B2

    公开(公告)日:2015-12-01

    申请号:US13636871

    申请日:2011-03-02

    Abstract: A laminated film includes a resin layer provided on at least one surface of a thermoplastic resin film substrate, wherein the resin layer comprises an acrylic-modified polyester whose acrylic resin component has a glass-transition temperature of not lower than 67° C. and a sugar alcohol and/or a sugar alcohol derivative; the mass ratio of the acrylic-modified polyester to the sugar alcohol and the sugar alcohol derivative (the mass of the acrylic-modified polyester/the total mass of the sugar alcohol and the sugar alcohol derivative) is from 75/25 to 97/3; the total content of the acrylic-modified polyester and the sugar alcohol and sugar alcohol derivative is 65% by mass or more based on the total resin layer; and the haze value of the laminated film is not more than 2.0%.

    Abstract translation: 层压膜包括设置在热塑性树脂膜基材的至少一个表面上的树脂层,其中树脂层包含丙烯酸改性聚酯,其丙烯酸树脂组分的玻璃化转变温度不低于67℃, 糖醇和/或糖醇衍生物; 丙烯酸改性聚酯与糖醇和糖醇衍生物的质量比(丙烯酸改性聚酯的质量/糖醇和糖醇衍生物的总质量)为75/25至97/3 ; 丙烯酸改性聚酯和糖醇和糖醇衍生物的总含量相对于总树脂层为65质量%以上; 并且层压膜的雾度值不大于2.0%。

    LAMINATED FILM
    2.
    发明申请
    LAMINATED FILM 有权
    层压膜

    公开(公告)号:US20130011613A1

    公开(公告)日:2013-01-10

    申请号:US13636871

    申请日:2011-03-02

    Abstract: A laminated film includes a resin layer provided on at least one surface of a thermoplastic resin film substrate, wherein the resin layer comprises an acrylic-modified polyester whose acrylic resin component has a glass-transition temperature of not lower than 67° C. and a sugar alcohol and/or a sugar alcohol derivative; the mass ratio of the acrylic-modified polyester to the sugar alcohol and the sugar alcohol derivative (the mass of the acrylic-modified polyester/the total mass of the sugar alcohol and the sugar alcohol derivative) is from 75/25 to 97/3; the total content of the acrylic-modified polyester and the sugar alcohol and sugar alcohol derivative is 65% by mass or more based on the total resin layer; and the haze value of the laminated film is not more than 2.0%.

    Abstract translation: 层压膜包括设置在热塑性树脂膜基材的至少一个表面上的树脂层,其中树脂层包含丙烯酸改性聚酯,其丙烯酸树脂组分的玻璃化转变温度不低于67℃, 糖醇和/或糖醇衍生物; 丙烯酸改性聚酯与糖醇和糖醇衍生物的质量比(丙烯酸改性聚酯的质量/糖醇和糖醇衍生物的总质量)为75/25至97/3 ; 丙烯酸改性聚酯和糖醇和糖醇衍生物的总含量相对于总树脂层为65质量%以上; 并且层压膜的雾度值不大于2.0%。

    ANTIREFLECTION MEMBER AND MANUFACTURE METHOD FOR THE SAME
    3.
    发明申请
    ANTIREFLECTION MEMBER AND MANUFACTURE METHOD FOR THE SAME 有权
    抗反射构件及其制造方法

    公开(公告)号:US20120162774A1

    公开(公告)日:2012-06-28

    申请号:US13394359

    申请日:2010-09-08

    Abstract: An antireflection member comprising an antireflection layer includes two adjacent layers with different refractive indices, the antireflection layer formed at least on a first surface of a support substrate, and one of the two adjacent layers with different refractive indices located farther from the support substrate is a first layer, and another of the two adjacent layers is a second layer, wherein the antireflection layer contains two or more kinds of particles of different constituent elements and one or more kinds of binders, and a ratio b/a is more than 1.10 and less than 1.45, where “a” denotes a length of the line segment A1A2 connecting two arbitrarily-selected points A1 and A2 located on an interface between said first layer and said second layer and apart from each other by a linear distance of 500 nm or more, and “b” denotes a length of a line formed by projecting the line segment A1A2 in a direction perpendicular to the first surface of the support substrate onto the interface between the first layer and the second layer.

    Abstract translation: 包括抗反射层的防反射构件包括具有不同折射率的两个相邻层,至少在支撑衬底的第一表面上形成抗反射层,并且位于离支撑衬底更远的不同折射率的两个相邻层之一是 第一层,并且两个相邻层中的另一层是第二层,其中抗反射层包含两种或更多种不同组成元素和一种或多种粘合剂的颗粒,并且比率b / a大于1.10以下 大于1.45,其中“a”表示连接位于所述第一层和所述第二层之间的界面上的两个任意选择的点A1和A2的线段A1A2的长度,并且彼此间隔500nm以上的直线距离 而“b”表示通过将线段A1A2沿垂直于支撑基板的第一表面的方向投影到t上而形成的线的长度 他在第一层和第二层之间进行界面。

    HARD-COATED FILM, METHOD FOR PRODUCTION THEREOF AND ANTIREFLECTION FILM
    5.
    发明申请
    HARD-COATED FILM, METHOD FOR PRODUCTION THEREOF AND ANTIREFLECTION FILM 有权
    硬涂膜,其生产方法和抗反射膜

    公开(公告)号:US20100028600A1

    公开(公告)日:2010-02-04

    申请号:US12444497

    申请日:2007-08-31

    Abstract: There is provided a hard-coated film that includes a thermoplastic film and a hard coat layer placed thereon, has high surface hardness, is prevented from forming interference iris patterns, does not reduce image sharpness when used for antireflection films, and is prevented from causing screen glittering, external light reflection, or coloration irregularity of reflected light. The hard-coated film includes a polyester film and a hard coat layer placed on at least one side of the polyester film, wherein the hard coat layer has a surface with irregularities, an interface between the polyester film and the hard coat layer has irregularities, and the surface of the hard coat layer has 3D surface roughness parameters including an arithmetical mean deviation of surface Sa of from 15 nm to less than 150 nm and a kurtosis of surface height distribution Sku of from 1.5 to 5.

    Abstract translation: 提供了一种硬涂层,其包括热塑性膜和置于其上的硬涂层,具有高的表面硬度,防止形成干涉虹膜图案,当用于防反射膜时不会降低图像清晰度,并且防止引起 屏幕闪烁,外部光反射或反射光的着色不规则。 所述硬涂膜包括聚酯膜和设置在所述聚酯膜的至少一面上的硬涂层,其中所述硬涂层具有不规则的表面,所述聚酯膜和所述硬涂层之间的界面具有不规则性, 并且硬涂层的表面具有3D表面粗糙度参数,包括表面Sa的从15nm到小于150nm的算术平均偏差,以及1.5至5的表面高度分布Sku的峰度。

    Antireflection member and manufacture method for the same
    6.
    发明授权
    Antireflection member and manufacture method for the same 有权
    防反射构件及其制造方法

    公开(公告)号:US09423531B2

    公开(公告)日:2016-08-23

    申请号:US13394359

    申请日:2010-09-08

    Abstract: An antireflection member comprising an antireflection layer includes two adjacent layers with different refractive indices, the antireflection layer formed at least on a first surface of a support substrate, and one of the two adjacent layers with different refractive indices located farther from the support substrate is a first layer, and another of the two adjacent layers is a second layer, wherein the antireflection layer contains two or more kinds of particles of different constituent elements and one or more kinds of binders, and a ratio b/a is more than 1.10 and less than 1.45, where “a” denotes a length of the line segment A1A2 connecting two arbitrarily-selected points A1 and A2 located on an interface between said first layer and said second layer and apart from each other by a linear distance of 500 nm or more, and “b” denotes a length of a line formed by projecting the line segment A1A2 in a direction perpendicular to the first surface of the support substrate onto the interface between the first layer and the second layer.

    Abstract translation: 包括抗反射层的防反射构件包括具有不同折射率的两个相邻层,至少在支撑衬底的第一表面上形成抗反射层,并且位于离支撑衬底更远的不同折射率的两个相邻层之一是 第一层,并且两个相邻层中的另一层是第二层,其中抗反射层包含两种或更多种不同组成元素和一种或多种粘合剂的颗粒,并且比率b / a大于1.10以下 大于1.45,其中“a”表示连接位于所述第一层和所述第二层之间的界面上的两个任意选择的点A1和A2的线段A1A2的长度,并且彼此间隔500nm以上的直线距离 而“b”表示通过将线段A1A2沿垂直于支撑基板的第一表面的方向投影到t上而形成的线的长度 他在第一层和第二层之间进行界面。

    Hard-coated film, method for production thereof and antireflection film
    7.
    发明授权
    Hard-coated film, method for production thereof and antireflection film 有权
    硬涂膜,其制造方法和抗反射膜

    公开(公告)号:US08309202B2

    公开(公告)日:2012-11-13

    申请号:US12444497

    申请日:2007-08-31

    Abstract: There is provided a hard-coated film that includes a thermoplastic film and a hard coat layer placed thereon, has high surface hardness, is prevented from forming interference iris patterns, does not reduce image sharpness when used for antireflection films, and is prevented from causing screen glittering, external light reflection, or coloration irregularity of reflected light. The hard-coated film includes a polyester film and a hard coat layer placed on at least one side of the polyester film, wherein the hard coat layer has a surface with irregularities, an interface between the polyester film and the hard coat layer has irregularities, and the surface of the hard coat layer has 3D surface roughness parameters including an arithmetical mean deviation of surface Sa of from 15 nm to less than 150 nm and a kurtosis of surface height distribution Sku of from 1.5 to 5.

    Abstract translation: 提供了一种硬涂层,其包括热塑性膜和置于其上的硬涂层,具有高的表面硬度,防止形成干涉虹膜图案,当用于防反射膜时不会降低图像清晰度,并且防止引起 屏幕闪烁,外部光反射或反射光的着色不规则。 所述硬涂膜包括聚酯膜和设置在所述聚酯膜的至少一面上的硬涂层,其中所述硬涂层具有不规则的表面,所述聚酯膜和所述硬涂层之间的界面具有不规则性, 并且硬涂层的表面具有3D表面粗糙度参数,包括表面Sa的从15nm到小于150nm的算术平均偏差,以及1.5至5的表面高度分布Sku的峰度。

Patent Agency Ranking