公开(公告)号:US11920032B2
公开(公告)日:2024-03-05
申请号:US17280272
申请日:2019-09-26
Applicant: Apollo Tyres Global R&D B.V.
Inventor: Anup Mondal , Henrik Stevens , Louis Reuvekamp
IPC: C08L7/00 , B60C1/00 , C08F222/06 , C08J3/24 , C08K3/013 , C08K3/04 , C08L9/00 , C08L19/00 , C08L23/08
CPC classification number: C08L7/00 , B60C1/0016 , C08F222/06 , C08J3/24 , C08K3/013 , C08K3/04 , C08L9/00 , C08L23/0869 , C08L2205/03
Abstract: The present invention relates to a cross-linkable rubber composition, the cross-linkable rubber composition comprising a natural rubber (NR), a filler, and a resin. The resin is a terpolymer of ethylene, acrylic ester and maleic anhydride and is present in an amount ranging from ≥5 to ≤20 phr.
-
公开(公告)号:US20220153966A1
公开(公告)日:2022-05-19
申请号:US17437529
申请日:2020-03-13
Applicant: Apollo Tyres Global R&D B.V.
Inventor: Vikram Singh , Louis Reuvekamp , Tharik Mohamed , Hendrik Stevens
Abstract: The present invention relates to a a cross-linkable rubber composition, the cross-linkable rubber composition comprising, based upon parts by weight per 100 parts by weight rubber (phr): ≥60 phr to ≤80 phr of a butadiene rubber, a syndiotactic 1,2-polybutadiene, coupling agent, a filler, and a resin, wherein the composition co?prises ≥10 phr to ≤20 phr of the sy?diotactic 1,2-polybutadiene, and wherein the composition comprises ≥1 phr to ≤20 phr of at least two coupling agents wherein one of the coupling agents is or comprises a mercapto based silane and wherein the ratio of the mercapto based silane to the second coupling agent is in the range of ≥2:1 to ≤:10:1.
-
公开(公告)号:US12286537B2
公开(公告)日:2025-04-29
申请号:US17760696
申请日:2020-09-15
Applicant: Apollo Tyres Global R&D B.V.
Inventor: Carmela Mangone , Michel Klein Gunnewiek , Louis Reuvekamp , Wisut Kaewsakul , Anke Blume
IPC: C08L9/00 , B60C1/00 , H10N30/063
Abstract: The present invention relates to a method for chemically adhering a diene rubber to a piezoelectric polymer, the method comprising the steps of: a) providing a piezoelectric polymer having at least one surface, b) providing a rubber component having at least one surface and comprising a sulfur cross-linkable rubber composition, c) introducing oxygen-containing functional groups on the at least one surface of the piezoelectric polymer, d) reacting the oxygen-containing functional groups with a compound comprising thiocyanate groups, and e) contacting the surface of the piezoelectric polymer obtained of step d) with the surface of the rubber component, and cross-linking.
-
-