THIN ALUMINUM FLAKES
    1.
    发明申请
    THIN ALUMINUM FLAKES 有权
    薄铝板

    公开(公告)号:US20150033987A1

    公开(公告)日:2015-02-05

    申请号:US14379336

    申请日:2013-02-27

    Applicant: BASF SE

    Abstract: Described are thin plane-parallel aluminum flakes illustrated in FIG. 1 having a thickness of up to 200 nm and comprising an inner layer of oxidized aluminium having a thickness of 0.5-30 nm, a process for the manufacture thereof and the use thereof, e.g. in formulations, like paints, electrostatic coatings, printing inks, plastics materials, and cosmetics. Surprisingly, due to the inner layer of oxidized aluminum the aluminum flakes have an improved shear stability as evidenced e.g. by the difference in lightness before and after shear stress.

    Abstract translation: 描述的是图1所示的薄平面平行铝薄片。 1,其厚度高达200nm,并且包含厚度为0.5-30nm的氧化铝内层,其制造方法及其用途,例如, 在制剂中,如油漆,静电涂料,印刷油墨,塑料材料和化妆品。 令人惊奇的是,由于氧化铝的内层,铝薄片具有改善的剪切稳定性, 通过剪切应力前后的亮度差。

    Process for preparing metal oxide coated aluminium effect pigments

    公开(公告)号:US09701844B2

    公开(公告)日:2017-07-11

    申请号:US14397721

    申请日:2013-05-10

    Applicant: BASF SE

    Abstract: The present invention relates to a process for preparing a colored effect pigment, comprising: (i) coating aluminum-based substrate particles in an aqueous coating medium with at least one metal oxide layer, wherein the metal oxide is selected from a titanium oxide, an iron oxide, or any mixture thereof, (ii) providing a mixture of the coated aluminum-based substrate particles and a particulate inorganic non-metallic material in the aqueous coating medium by adding the particulate inorganic non-metallic material to the aqueous coating medium, and (iii) separating the mixture of the coated aluminum-based substrate particles and the particulate inorganic non-metallic material from the aqueous coating medium and subjecting the separated mixture to a thermal drying step so as to obtain a dry colored effect pigment material.

    Process for preparing an effect pigment

    公开(公告)号:US09631064B2

    公开(公告)日:2017-04-25

    申请号:US14385932

    申请日:2013-04-05

    Applicant: BASF SE

    Abstract: The present invention relates to a process for preparing a coloured effect pigment, comprising the steps of (a) preparing in an aqueous coating medium at least one layer of a hydroxyl-containing metal oxide on a substrate, thereby obtaining in the aqueous coating medium a first coloured pigment material CPM1 comprising the substrate coated with the hydroxyl-containing metal oxide, wherein the substrate is made of aluminium or aluminium alloy which optionally comprises at least one passivating layer, and wherein the hydroxyl-containing metal oxide is a hydroxyl-containing iron oxide or a hydroxyl-containing titanium oxide or a mixture thereof, (b) providing the first coloured pigment material CPM1 in a liquid post-treatment medium comprising one or more high boiling organic liquids, and (c) heating the liquid post-treatment medium to a temperature of at least 90° C. so as to convert the first coloured pigment material CPM1 to a second coloured pigment material CPM2.

    PROCESS FOR PREPARING AN EFFECT PIGMENT
    7.
    发明申请
    PROCESS FOR PREPARING AN EFFECT PIGMENT 有权
    制备效果色素的方法

    公开(公告)号:US20150020712A1

    公开(公告)日:2015-01-22

    申请号:US14385932

    申请日:2013-04-05

    Applicant: BASF SE

    Abstract: The present invention relates to a process for preparing a coloured effect pigment, comprising the steps of (a) preparing in an aqueous coating medium at least one layer of a hydroxyl-containing metal oxide on a substrate, thereby obtaining in the aqueous coating medium a first coloured pigment material CPM1 comprising the substrate coated with the hydroxyl-containing metal oxide, wherein the substrate is made of aluminium or aluminium alloy which optionally comprises at least one passivating layer, and wherein the hydroxyl-containing metal oxide is a hydroxyl-containing iron oxide or a hydroxyl-containing titanium oxide or a mixture thereof, (b) providing the first coloured pigment material CPM1 in a liquid post-treatment medium comprising one or more high boiling organic liquids, and (c) heating the liquid post-treatment medium to a temperature of at least 90° C. so as to convert the first coloured pigment material CPM1 to a second coloured pigment material CPM2.

    Abstract translation: 本发明涉及一种着色效应颜料的制备方法,包括以下步骤:(a)在水性涂料介质中制备至少一层含羟基的金属氧化物在基材上,从而在水性涂料介质中获得 第一着色颜料材料CPM1,其包含涂覆有含羟基金属氧化物的基材,其中所述基材由铝或铝合金制成,其任选地包含至少一个钝化层,并且其中所述含羟基的金属氧化物是含羟基的铁 氧化物或含羟基的氧化钛或其混合物,(b)在包含一种或多种高沸点有机液体的液体后处理介质中提供第一着色颜料材料CPM1,和(c)加热液体后处理介质 至少90℃的温度,以将第一着色颜料CPM1转化为第二着色颜料CPM2。