Aluminum oxide fibers and their production
    1.
    发明授权
    Aluminum oxide fibers and their production 失效
    氧化铝纤维及其生产

    公开(公告)号:US3865599A

    公开(公告)日:1975-02-11

    申请号:US31631172

    申请日:1972-12-18

    Applicant: BAYER AG

    Abstract: Aluminum oxide fibers of the approximate percent composition by weight: Al2O3 61-98% preferably 76-96% SiO2 1-20% preferably 3-15% P2O5 0-10% preferably 0- 5% B2O3 0-10% preferably 0- 5% MgO 0- 5% preferably 0- 1% C 0.1- 4% preferably 0.5-2.8% The fibers are produced by dry spinning a solution containing a neutral or basic aluminum salt of a monobasic lower carboxylic acid, a hydrolyzed silicic acid ester or organoalkoxysilane and polyethylene oxide having a degree of polymerization of at least about 2,000. The product is then heat treated at a temperature between about 400* and 1,800*C. Phosphorus, boron and magnesium may also be present in the solution and end up in the fiber as oxides.

    Abstract translation: 氧化铝纤维的重量百分比:

Patent Agency Ranking