公开(公告)号:US12030789B2
公开(公告)日:2024-07-09
申请号:US17523734
申请日:2021-11-10
Applicant: Battelle Memorial Institute , Albemarle Corporation
Inventor: Jie Xiao , Ran Yi , Yujing Bi , Job T. Rijssenbeek , Xiaoguang Hao , Subramanian Venkatachalam , Liu Luo
CPC classification number: C01G53/50 , H01B1/08 , H01M4/505 , H01M4/525 , C01P2002/72 , C01P2004/03 , C01P2004/04 , C01P2006/40 , H01M2004/021 , H01M2004/028
Abstract: Methods for synthesizing crystalline Ni-rich cathode materials are disclosed. The Ni-rich cathode material may have a formula LiNixMnyMzCo1-x-y-zO2, where M represents one or more dopant metals, x≥0.6, 0.01≤y
-
公开(公告)号:US12211999B2
公开(公告)日:2025-01-28
申请号:US18514508
申请日:2023-11-20
Applicant: Battelle Memorial Institute
Abstract: Methods for synthesizing single crystalline Ni-rich cathode materials are disclosed. The Ni-rich cathode material may have a formula LiNiXMnyMzCol1-x-y-zO2, where M represents one or more dopant metals, x≥0.6, 0.01≤y
-
公开(公告)号:US20240088382A1
公开(公告)日:2024-03-14
申请号:US18514508
申请日:2023-11-20
Applicant: Battelle Memorial Institute
IPC: H01M4/525 , C01G53/00 , H01B1/08 , H01M4/505 , H01M10/0525
CPC classification number: H01M4/525 , C01G53/50 , H01B1/08 , H01M4/505 , H01M10/0525 , C01P2002/85 , H01M2004/028
Abstract: Methods for synthesizing single crystalline Ni-rich cathode materials are disclosed. The Ni-rich cathode material may have a formula LiNixMnyMzCol1-x-y-zO2, where M represents one or more dopant metals, x≥0.6, 0.01≤y
-
公开(公告)号:US11862794B2
公开(公告)日:2024-01-02
申请号:US16951868
申请日:2020-11-18
Applicant: Battelle Memorial Institute
CPC classification number: H01M4/525 , C01G53/50 , H01B1/08 , H01M4/505 , H01M10/0525 , C01P2002/52 , C01P2002/72 , C01P2002/85 , C01P2002/90 , C01P2004/03 , C01P2004/04 , C01P2004/61 , C01P2004/62 , C01P2006/40 , H01M2004/021 , H01M2004/028
Abstract: Methods for synthesizing single crystalline Ni-rich cathode materials are disclosed. The Ni-rich cathode material may have a formula LiNiXMnyMzCo1-x-y-zO2, where M represents one or more dopant metals, x≥0.6, 0.01≤y
-
公开(公告)号:US20220112094A1
公开(公告)日:2022-04-14
申请号:US17523734
申请日:2021-11-10
Applicant: Battelle Memorial Institute , Albemarle Corporation
Inventor: Jie Xiao , Ran Yi , Yujing Bi , Job T. Rijssenbeek , Xiaoguang Hao , Subramanian Venkatachalam , Liu Luo
Abstract: Methods for synthesizing crystalline Ni-rich cathode materials are disclosed. The Ni-rich cathode material may have a formula LiNixMnyMzCo1−x−y−zO2, where M represents one or more dopant metals, x≥0.6, 0.01≤y
-
公开(公告)号:US20210351404A1
公开(公告)日:2021-11-11
申请号:US16951868
申请日:2020-11-18
Applicant: Battelle Memorial Institute
IPC: H01M4/525 , H01M4/505 , H01M10/0525 , C01G53/00
Abstract: Methods for synthesizing single crystalline Ni-rich cathode materials are disclosed. The Ni-rich cathode material may have a formula LiNiXMnyMzCo1-x-y-zO2, where M represents one or more dopant metals, x≥0.6, 0.01≤y
-
7.
公开(公告)号:US20240356096A9
公开(公告)日:2024-10-24
申请号:US17974022
申请日:2022-10-26
Applicant: Battelle Memorial Institute
Inventor: Jie Xiao , Ran Yi , Bingbin Wu , Yujing Bi
CPC classification number: H01M10/54 , C01G53/50 , H01M4/364 , H01M4/505 , H01M4/525 , C01P2002/50 , C01P2002/72 , C01P2004/03 , C01P2006/40 , H01M2004/028
Abstract: A solid-state method for recycling spent and/or scrap cathode material includes heating a cathode material comprising lithium nickel manganese cobalt oxide in an oxygen-containing atmosphere at a temperature T1 for an effective period of time t1 to convert the cathode material to a solid precursor, combining the solid precursor with a lithium compound, and heating the solid precursor and the lithium compound in an oxygen-containing atmosphere at a temperature T2 for an effective period of time t2 to form a product comprising monocrystalline lithium nickel manganese cobalt oxide having a formula LiNixMnyMzCo1-x-y-zO2, where M represents one or more dopant metals, x≥0.33, 0.01≤y
-
公开(公告)号:US20240351913A1
公开(公告)日:2024-10-24
申请号:US18651340
申请日:2024-04-30
Applicant: Battelle Memorial Institute , Albemarle Corporation
Inventor: Jie Xiao , Ran Yi , Yujing Bi , Job T. Rijssenbeek , Xiaoguang Hao , Subramanian Venkatachalam , Liu Luo
CPC classification number: C01G53/50 , H01B1/08 , H01M4/505 , H01M4/525 , C01P2002/72 , C01P2004/03 , C01P2004/04 , C01P2006/40 , H01M2004/021 , H01M2004/028
Abstract: Methods for synthesizing crystalline Ni-rich cathode materials are disclosed. The Ni-rich cathode material may have a formula LiNiXMnyMzCo1-x-y-zO2, where M represents one or more dopant metals, x≥0.6, 0.01≤y
-
9.
公开(公告)号:US20240145801A1
公开(公告)日:2024-05-02
申请号:US17974022
申请日:2022-10-26
Applicant: Battelle Memorial Institute
Inventor: Jie Xiao , Ran Yi , Bingbin Wu , Yujing Bi
Abstract: A solid-state method for recycling spent and/or scrap cathode material includes heating a cathode material comprising lithium nickel manganese cobalt oxide in an oxygen-containing atmosphere at a temperature T1 for an effective period of time t1 to convert the cathode material to a solid precursor, combining the solid precursor with a lithium compound, and heating the solid precursor and the lithium compound in an oxygen-containing atmosphere at a temperature T2 for an effective period of time t2 to form a product comprising monocrystalline lithium nickel manganese cobalt oxide having a formula LiNixMnyMzCo1-x-y-zO2, where M represents one or more dopant metals, x≥0.33, 0.01≤y
-
-
-
-
-
-
-
-