Abstract:
Processes for coating substrates and the related substrates are disclosed herein. A one-component base coating composition is applied onto a substrate and a one-component top coating composition is applied wet-on-wet onto the applied base coating composition. The coating compositions are based on aqueous acrylate/polyurethane dispersions. The top coating composition is applied after the applied base coating composition develops a pendulum hardness of at least 50% of the pendulum hardness that would be exhibited by the base coating composition after UV cure. The applied coatings exposed to UV radiation to simultaneously cure both the base coating composition and the top coating composition.
Abstract:
Two-component waterborne coating compositions that form crosslinked polyurethane films exhibiting soft feel effect and high chemical resistance are disclosed. The two-component waterborne coating compositions include rubber particles and reaction products of hydroxy-functional polyacrylic polyol dispersions and water-dispersible polyisocyanates.
Abstract:
Two-component water-based coating compositions are described. The coating compositions include a mixture of components that includes: (a) an aqueous dispersion of a resin comprising functional groups reactive with isocyanates; and (b) a hydrophilicized polyisocyanate. The mixture includes (i) propylene carbonate that is present in the mixture in an amount of greater than 2 percent by weight, based on the total weight of the mixture; and (ii) a ratio of isocyanate groups to functional groups reactive with isocyanates of 0.8 to 3.0:1.
Abstract:
Processes for coating substrates and the related substrates are disclosed herein. A one-component base coating composition is applied onto a substrate and a one-component top coating composition is applied wet-on-wet onto the applied base coating composition. The coating compositions are based on aqueous acrylate/polyurethane dispersions. The top coating composition is applied after the applied base coating composition develops a pendulum hardness of at least 50% of the pendulum hardness that would be exhibited by the base coating composition after UV cure. The applied coatings exposed to UV radiation to simultaneously cure both the base coating composition and the top coating composition.