Abstract:
Provided are non-breathable films including specific polymer blends, and methods for making such films. The films comprise an anhydride and/or carboxylic acid functionalized ethylene/alpha-olefin interpolymer, a linear low density polyethylene, and an inorganic filler. The method of manufacturing the film comprises extruding an anhydride and/or carboxylic acid functionalized ethylene/alpha-olefin interpolymer, a linear low density polyethylene, and an inorganic filler to form the film and stretching the film. The films according to embodiments disclosed herein can exhibit low WVTR values and improved modulus while also incorporating significant amounts of inorganic filler at low gauges.
Abstract:
A composition comprises: (A) a polypropylene polymer; (B) a polyolefin elastomer; (C) a compound having the formula (I) defined herein; and (D) an additive component. And an article made from the composition.
Abstract:
A coating composition comprising: an aqueous dispersion comprising: the melt-kneading product of (A) a base polymer which comprises one or more thermoplastic polymers, (B) a stabilizing agent which comprises at least one component selected from the group consisting of acrylic acid grafted ethylene-based polymers and maleic anhydride grafted polyolefins; (C) a neutralizing agent; and (D) water; wherein the aqueous dispersion has a volume average particle size of less than about 5 μm is provided.
Abstract:
A method for making a copolymer polyol includes (a) forming a pre-compounded thermoplastic polymeric composition by compounding from 10 wt % to 90 wt % of a solid functional additive component with from 10 wt % to 90 wt % of a polystyrene component, (b) melting the pre-compounded thermoplastic polymeric composition to form a melted thermoplastic polymeric composition, (c) combining the melted thermoplastic polymeric composition with a carrier polyol component in the presence of a stabilizer component to form a pre-mixture that includes the pre-compounded thermoplastic polymeric composition dispersed within a continuous phase of the carrier polyol component, and (d) cooling the pre-mixture to form the copolymer polyol.
Abstract:
A composition comprises (A) an ethylene/alpha-olefin/diene interpolymer; (B) a peroxide comprising at least one peroxide bond; and (C) a bis-TEMPO compound having the Structure (I), wherein R1-4 are each independently H or a C1-C6 alkyl group; X is S, O, N, P, Se, a carbonyl group, a carboxyl group, an amide group, an azo group, an imino group, a carbamate group, a peroxy group, a phosphono group, a phosphate group, a sulfonyl group, a sulfinyl group, a sulfonate ester group, a sulfonate ester group, or combinations thereof; Y is a substitute or unsubstituted aliphatic alkyl group or aromatic alkyl group, a heterocyclic group, a siloxane group, an ethylene glycol group, an imide group, or combinations thereof; and n is greater than 1. The ratio of the molar amount of nitroxide groups of component (C) to the molar amount of the peroxide bonds of component (B) is from 0.100:1.000 to 2.000:1.000.
Abstract:
The present disclosure provides a composition comprising: A) a propylene/C4-C10 alpha-olefin interpolymer; (i)) a total unsaturation per mole of propylene from 0.010% to 0.030%, (ii) a density from 0.855 g/cc to 0.890 g/cc, and (iii) a melt viscosity, at 177 C, from 500 cP to 200,000 cP.
Abstract:
The present disclosure provides a composition. In an embodiment a composition is provided and includes: (A) a carboxylic-functionalized ethylene/a-olefin interpolymer having (i) a density from 0.855 g/cc to 0.895 g/cc; and (ii) a melt viscosity, at 177° C., less than, or equal to, 50,000 mPa·s; and (B) a propylene-based interpolymer having (i) a density from 0.870 g/cc to 0.890 g/cc; and (ii) a melt viscosity, at 177° C., less than, or equal to, 50,000 mPa·s.
Abstract:
A composition comprises: (A) a polypropylene polymer; (B) a polyolefin elastomer; (C) a compound having the formula (I) defined herein; and (D) an additive component. And an article made from the composition.
Abstract:
A composition comprises (A) an ethylene/alpha-olefin/diene interpolymer; (B) a peroxide comprising at least one peroxide bond; and (C) a bis-TEMPO compound having the Structure (I), wherein R1-4 are each independently H or a C1-C6 alkyl group; X is S, O, N, P, Se, a carbonyl group, a carboxyl group, an amide group, an azo group, an imino group, a carbamate group, a peroxy group, a phosphono group, a phosphate group, a sulfonyl group, a sulfinyl group, a sulfonate ester group, a sulfonate ester group, or combinations thereof; Y is a substitute or unsubstituted aliphatic alkyl group or aromatic alkyl group, a heterocyclic group, a siloxane group, an ethylene glycol group, an imide group, or combinations thereof; and n is greater than 1. The ratio of the molar amount of nitroxide groups of component (C) to the molar amount of the peroxide bonds of component (B) is from 0.100:1.000 to 2.000:1.000.
Abstract:
The present disclosure provides a composition comprising: A) a propylene/C4-C10 alpha-olefin interpolymer; (i)) a total unsaturation per mole of propylene from 0.010% to 0.030%, (ii) a density from 0.855 g/cc to 0.890 g/cc, and (iii) a melt viscosity, at 177 C, from 500 cP to 200,000 cP.