Three electrode ceramic metal halide lamp
    1.
    发明申请
    Three electrode ceramic metal halide lamp 失效
    三电极陶瓷金属卤化物灯

    公开(公告)号:US20030234613A1

    公开(公告)日:2003-12-25

    申请号:US10179695

    申请日:2002-06-25

    CPC classification number: H01J61/545 H01J9/247 H01J61/30

    Abstract: A ceramic body (14) for a discharge vessel (12) includes a central barrel portion (60) and two end plus (64, 66), which close opposite ends of the barrel. Main electrode (32, 34) and an initiator electrode 50 are supplied with power via conductors in leg members (70, 76, 72). In one embodiment, a first electrode 32 and the initiator electrode are supplied with current through two separate leg members. In another embodiment, a dual electrode leg member is provided with two bores (124, 126).

    Abstract translation: 用于放电容器(12)的陶瓷体(14)包括中心筒体部分(60)和两端部(64,66),该端部端部封闭筒体的相对端部。 主电极(32,34)和引发电极50在腿部构件(70,76,72)中被供电。 在一个实施例中,第一电极32和引发器电极通过两个单独的腿部元件供应电流。 在另一个实施例中,双电极腿构件设置有两个孔(124,126)。

    Metal halide lamp fabrication
    2.
    发明申请
    Metal halide lamp fabrication 审中-公开
    金属卤化物灯制造

    公开(公告)号:US20020153028A1

    公开(公告)日:2002-10-24

    申请号:US09782632

    申请日:2001-02-13

    CPC classification number: B08B7/0071 H01J9/022 H01J61/827

    Abstract: The present invention concerns a process of treating an energizing electrode for use in a metal halide lamp. Lamp energizing electrodes are placed into a support container and the support container is then placed within an oven that bakes the electrodes at an elevated temperature. Hydrogen is caused to flow through the support container at a rate of from 5 to 60 liters per minute while the temperature is maintained within the oven between 2000 and 3200 degrees C. In accordance with an exemplary embodiment of the invention, the temperature is maintained within the oven at 2400 and 2600 degrees C., the dew point of the hydrogen is less than minus 40 degrees C. and the electrodes are baked for a period of 10 to 240 minutes. This process treats the electrodes in the support container and results in lamps having superior maintenance of lamp output as measured in lumens of output.

    Abstract translation: 本发明涉及处理用于金属卤化物灯的激励电极的方法。 灯泡通电电极放置在支撑容器中,然后将支撑容器放置在烘箱中,烘箱在升高的温度下烘烤电极。 使氢气以5至60升/分钟的速率流过支撑容器,同时将温度保持在烘箱内的温度在2000至3200摄氏度之间。根据本发明的示例性实施方案,温度保持在 烘箱在2400和2600摄氏度,氢的露点小于零下40摄氏度,电极烘烤10至240分钟。 该过程处理支撑容器中的电极,并且导致具有以输出流明度测量的灯输出的优异维护的灯。

Patent Agency Ranking