Maraging steel and process for manufacturing a strip or a part cut out of a strip of cold-rolled maraging steel
    2.
    发明申请
    Maraging steel and process for manufacturing a strip or a part cut out of a strip of cold-rolled maraging steel 有权
    马氏体时效钢和制造一条钢带或由一条冷轧马氏体时效钢切割的部件的工艺

    公开(公告)号:US20020059967A1

    公开(公告)日:2002-05-23

    申请号:US09988134

    申请日:2001-11-19

    Inventor: Lucien Coutu

    Abstract: A maraging steel strip or part and process for manufacture of a strip or of a part cut out of a strip of cold-rolled maraging steel and hardened by a hardening heat treatment. In the process, before the hardening heat treatment is performed, the strip or the part is subjected to cold plastic deformation with a degree of working greater than 30% and the strip or the part is subjected to recrystallization annealing in order to obtain a fine-grained structure with ASTM index higher than 8. The composition by weight of the maraging steel is: 12%nullNinull24.5%; 2.5%nullMonull12%; 4.17%nullConull20%, Al%null0.15%; Tinull0.1%; Nnull0.003%; Sinull0.1%; Mnnull0.1%; Cnull0.005%; Snull0.001%; Pnull0.005%; Hnull0.0003%; Onull0.001%; iron and impurities resulting from smelting, the chemical composition also satisfying the relationships: 20%nullNinullMonull27%; 50nullConullMonull200; TinullNnull2null10null4.

    Abstract translation: 一种马氏体时效钢带或其制造方法,用于制造由冷轧马氏体时效钢带切割出的钢带或部分切割并通过硬化热处理硬化的部件。 在该过程中,在进行硬化热处理之前,将带材或部件进行冷塑性变形,其加工程度大于30%,并对带材或部件进行再结晶退火, ASTM指数高于8的颗粒结构。马氏体时效钢的重量组成为:12%<= Ni <= 24.5%; 2.5%<= Mo <= 12%; 4.17%<= Co <= 20%,Al%<= 0.15%; Ti <= 0.1%; N <= 0.003%; Si <= 0.1%; Mn <= 0.1%; C <= 0.005%; S <= 0.001%; P <= 0.005% H <= 0.0003%; O <= 0.001%; 铁和冶炼产生的杂质,化学成分也满足关系:20%<= Ni + Mo <= 27%; 50 <= CoxMo <= 200; TixN <= 2×10-4。

    Iron-cobalt alloy, in particular for electromagnetic actuator mobile core and method for making same
    3.
    发明申请
    Iron-cobalt alloy, in particular for electromagnetic actuator mobile core and method for making same 有权
    铁钴合金,特别是用于电磁致动器的移动铁芯及其制造方法

    公开(公告)号:US20040099347A1

    公开(公告)日:2004-05-27

    申请号:US10275814

    申请日:2003-02-14

    Abstract: The invention concerns an iron-cobalt alloy, characterised in that it comprises in weight percentages: 10 to 22% of Co; traces to 2.5% of Si; traces to 2% of Al; 0.1 to 1% of Mn; traces to 0.0100% of C; a total of O, N and S content ranging between traces and 0.0070%; a total of Si, Al, Cr, Mo, V, Mn content ranging between 1.1 and 3.5%; a total of Cr, Mo and V content ranging between traces and 3%; a total of Ta and Nb content ranging between traces and 1%; the rest being iron and impurities resulting from production; and in that: 1.23null(AlnullMo) %null0.84 (SinullCrnullV) %null0.15null(Co %null15)null2.1 and in that 14.5null. (AlnullCr) %null12null(VnullMo) %null25nullSi %null21. The inventive alloy is useful for making electromagnetic actuator mobile cores.

    Abstract translation: 本发明涉及一种铁 - 钴合金,其特征在于其包含重量百分比:10至22%的Co; 痕量至2.5%的Si; 追溯到Al的2% 0.1〜1%的Mn; 痕量至0.0100%C; O,N和S含量总和在0.0070%之间; Si,Al,Cr,Mo,V,Mn含量在1.1和3.5%之间; Cr,Mo和V含量总计在痕量和3%之间; 总计Ta和Nb含量在痕量和1%之间; 其余的是由生产产生的铁和杂质; 其中:1.23x(Al + Mo)%+ 0.84(Si + Cr + V)%-0.15x(Co%-15)<= 2.1,在14.5倍。 (Al + Cr)%+ 12x(V + Mo)%+ 25×Si%> = 21。 本发明合金可用于制造电磁致动器移动芯。