公开(公告)号:US20140318414A1
公开(公告)日:2014-10-30
申请号:US14295347
申请日:2014-06-04
Applicant: Industrial Technology Research Institute
Inventor: Kuo-Chan Chiou , Hong-Ching Lin , Szu-Po Huang , Chun-An Lu
IPC: C09D7/12
CPC classification number: C09D7/61 , B22F1/0022 , B22F7/04 , B22F2998/10 , B82Y30/00 , C08K3/08 , C08K9/02 , C09D1/00 , C09D7/62 , C09D7/67 , B22F9/24 , B22F9/305
Abstract: A nano-metal solution, nano-metal complex grains, and a manufacturing method of a metal film are provided. The nano-metal solution includes metal grains having an amount of 0.1˜30 wt %, metallic-organic self-decomposition molecules having an amount of 0.1˜50 wt % and having formula 1, and a solvent having an amount of 20˜99.8 wt %: wherein M represents a metal ion. The metallic-organic self-decomposition molecules and the metal grains are evenly mixed in the solvent, and the metallic-organic self-decomposition molecules are adsorbed on surfaces of the metal grains.
Abstract translation: 提供纳米金属溶液,纳米金属络合物颗粒和金属膜的制造方法。 纳米金属溶液包含0.1〜30重量%的金属颗粒,0.1〜50重量%的金属有机自分解分子,具有式1的溶剂和20〜99.8重量%的溶剂 %:其中M表示金属离子。 金属有机自分解分子和金属颗粒在溶剂中均匀混合,金属有机自分解分子被吸附在金属颗粒的表面上。