公开(公告)号:US20230340211A1
公开(公告)日:2023-10-26
申请号:US18304997
申请日:2023-04-21
Applicant: Jabil Inc.
Inventor: Thomas Fry , Michael Frye , Nicholas John Dippel
IPC: C08J3/16 , C08J3/11 , C09D5/03 , C09D167/00 , C09D175/04
CPC classification number: C08J3/16 , C08J3/11 , C09D5/031 , C09D167/00 , C09D175/04 , C08J2367/00 , C08J2375/00
Abstract: Spherical thermoplastic polymer powders useful for additive manufacturing may be made at high throughputs by a method comprising polymer in a dispersing medium at a temperature above the polymer melting temperature (Tm) under shear for short times (e.g., less than 30 minutes) to form a mixture that is then rapid (faster than ambient cooling) cooled below Tm. The method is particularly useful for thermoplastic polymers having a high melt flow index (MFI) or low capillary viscosity at high shear (˜1000 s−1) within 20 or 30° C. of the polymer's melt temperature. The method may also include a crystallizing temperature below Tm and above the glass transition temperature Tg of the polymer to crystallize amorphous polymers or increase the crystallinity of semi-crystalline polymers.