    Abstract: A method of making a fiber composite having high strength at 2000* to 2200* F. by slip casting a nickel alloy matrix slurry into an array of tungsten fibers. The slip is dried and sintered in dry hydrogen at 1500* F. for one hour. The resulting body is isostatically hot pressed at 20,000 p.s.i. and 1500* F. for one hour, followed by a second isostalic hot pressing at 2000* F. for 1 hour.

    Abstract translation: 通过将镍合金基质浆料滑入铸造成钨丝阵列的方法,制造在2000°至2200°F具有高强度的纤维复合材料。 将该纸干燥并在干燥氢气中在1500°F下烧结1小时。 所得体在20,000 p.s.i等温热压。 和1500°F下1小时,然后在2000°F下进行第二次等压热压1小时。