Abstract:
Filter bodies are made by mixing borosilicate glass powder, potassium sulphate and 30% aqueous polyethylene glycol solution per kilogram of mixture. The mixture is filtered and dried and glass particles of a different size are mixed into the dried granulate. The resulting mixture is compressed at a pressure of 1000 bar to form blanks and sintered at about 860.degree. C. After cooling, the potassium sulphate is washed out of the blanks.
Abstract:
The invention relates to a process for producing high-strength construction and decoration materials which resemble natural stone, are in the form of panels and are used for cladding facades, walls and floors, both indoors and outdoors, from mixtures of broken glass, mineral components and finely divided additives, with a specified composition. A sintering aid, in the form of a solution of metal oxychlorides or metal alkoxides or tetrachlorides, preferably titanium tetrachloride, is added to the mixture, which is then introduced into a heat-resistant mould. In this mould, the mixture is subjected to a conventional sintering operation. The sintering aid which has been added makes it possible in particular to reduce the maximum sintering temperature and to improve the quality of the surface considerably.
Abstract:
A process for producing tabular building and decorative materials similar to natural stone and having high strength for the facing of facades, walls and floors in interior and exterior applications from thermally treated mixtures of crushed glass, ceramic components and finely divided additives and materials produced by the process.