公开(公告)号:US20230242762A1
公开(公告)日:2023-08-03
申请号:US18014774
申请日:2021-06-22
Applicant: POLYPLASTICS CO., LTD.
Inventor: Hidekazu IDEI , Katsuhei OHNISHI
CPC classification number: C08L81/02 , B29C45/0001 , B29C45/0005 , C08K3/041 , C08K7/14 , B29K2081/04
Abstract: Provided is a method of suppressing burrs that occur during injection-molding of a polyarylene sulfide resin composition, including: adding at least 0.01 to 5 parts by mass of a carbon nanostructure to 100 parts by mass of a polyarylene sulfide resin and melt-kneading at least the carbon nanostructure and the polyarylene sulfide resin.
-
公开(公告)号:US20240043620A1
公开(公告)日:2024-02-08
申请号:US18258664
申请日:2021-12-06
Applicant: Polyplastics Co., Ltd.
Inventor: Katsuhei OHNISHI
IPC: C08G75/0204 , C08K3/36 , G02B6/38
CPC classification number: C08G75/0204 , C08K3/36 , G02B6/38 , C08K2201/005 , C08K2201/014
Abstract: Provided are a polyarylene sulfide resin composition which yields a molded article with excellent toughness, as well as a molded article and an optical ferrule, which are produced using the polyarylene sulfide resin composition. In a polyarylene sulfide resin composition containing a polyarylene sulfide resin (A) and silica particles (B), a specific amount of a polyarylene sulfide resin (A) having a melt viscosity of 35 to 80 Pa·s, and a specific amount of silica particles (B) having a lower content of coarse powders with a particle size of 45 μm or more are employed.
-
公开(公告)号:US20170096557A1
公开(公告)日:2017-04-06
申请号:US15128015
申请日:2015-03-17
Applicant: Polyplastics Co., Ltd.
Inventor: Katsuhei OHNISHI , Tatsuya KANEZUKA , Sei WAKATSUKA
CPC classification number: C08L81/02 , B29B9/06 , B29C45/0001 , B29C45/14 , B29C48/022 , B29C48/04 , B29C48/15 , B29C48/402 , B29K2081/04 , B29K2705/00 , B32B15/08 , B32B27/20 , B32B27/286 , B32B2250/02 , B32B2262/101 , B32B2264/104 , B32B2457/00 , B32B2605/00 , C08J5/043 , C08J2381/04 , C08J2423/08 , C08K2003/265 , C08L2201/08 , C08L2203/20 , C08L2205/06
Abstract: A polyarylene sulfide-derived resin composition which has flowability optimal for insert molding and which can impart superior high- and low-temperature impact properties to a molded body, and an insert-molded body using the resin composition. The resin composition includes a polyarylene sulfide resin having carboxylic terminal groups, an olefin-derived copolymer, glass fibers and calcium carbonate. The weight-average molecular weight of the polyarylene sulfide resin is 15,000-40,000; as copolymerization components, the olefin-derived copolymer includes α-olefins, glycidyl esters of α,β-unsaturated acids, and acrylic esters, and the content of the copolymerization component derived from the glycidyl esters in the resin composition is 0.2-0.6 mass %. Further, the fiber diameter of the glass fibers is 9-13 μm, the average particle diameter of the calcium carbonate is 10-50 μm, and the total content of glass fibers and the calcium carbonate is 45-55 mass % of the resin composition.
-
-