公开(公告)号:US11196003B2
公开(公告)日:2021-12-07
申请号:US16714336
申请日:2019-12-13
Inventor: Hugo Bronstein , Mohammed Al-Hashimi , Tobin J. Marks , Kealan Fallon
Abstract: The organic semiconductor polymers relate to polymers containing an indolo-naphthyridine-6,13-dione thiophene (INDT) chromophore. The organic semiconductor polymers are formed by polymerizing INDT monomer with thiophene to obtain a conjugated polymer of the chromophore linked by thiophene monomers (INDT-T), with phenyl to obtain a conjugated polymer of the chromophore linked by phenyl monomers (INDT-P), with selenophene to obtain a conjugated polymer of the chromophore linked by selenophene monomers (INDT-S), or with benzothiadazole to obtain a conjugated polymer of the chromophore linked by benzothiadazole monomers (INDT-BT).
-
公开(公告)号:US10927214B2
公开(公告)日:2021-02-23
申请号:US15928944
申请日:2018-03-22
Inventor: Mohammed Al-Hashimi , Hugo Bronstein
Abstract: The method of making a pyrrolo bisthiazole homopolymer starts with dissolving a dibrominated pyrrolo[3,2-d:4,5-d′]bisthiazole monomer having the formula: where R is an alkyl group, in anhydrous tetrahydrofuran (THF). Then, the solvated monomer is treated with 1 equivalent of a Turbo-Grignard reagent complex having the formula iPrMgCl.LiCl at 0° C. to form a reaction mixture. The reaction mixture is stirred for 1 hour at room temperature, and after stirring, the reaction mixture is refluxed for 24 hours. A conjugated homopolymer product having the formula: where n is the number of repeating units of pyrrolo[3,2-d:4,5-d′]bisthiazole, is recovered from the reaction mixture. The PBTz-based homopolymers showed broad absorption from 450 to 850 nm in thin film and excellent photochemical and thermal stability, making the polymers suitable for lightweight, low cost plastic electronic devices.
-