公开(公告)号:US20150209772A1
公开(公告)日:2015-07-30
申请号:US14366739
申请日:2012-12-20
Applicant: SHELL OIL COMPANY
Inventor: Cornelis Ouwehand , Marcello Stefano Rigutto , Arend Jan Van Welsenes
CPC classification number: B01J31/04 , B01J21/12 , B01J23/883 , B01J23/888 , B01J27/049 , B01J27/19 , B01J29/061 , B01J31/0204 , B01J31/34 , B01J35/023 , B01J37/0036 , B01J37/0203 , B01J37/0236 , B01J37/18 , B01J37/20 , B01J37/32 , B01J2229/42 , C10G47/12 , C10G65/00
Abstract: Process for preparing a sulphided hydrocracking catalyst comprising the steps of (a) treating an amorphous silica alumina carrier with one or more Group VIB metal components, one or more Group VIII metal components and a C3-C12 polyhydric compound, (b) drying the treated catalyst carrier at a temperature of at most 200° C. to form an impregnated carrier, and (c) sulphiding the impregnated carrier to obtain a sulphided catalyst.
Abstract translation: 制备硫化加氢裂化催化剂的方法,包括以下步骤:(a)用一种或多种VIB族金属组分,一种或多种VIII族金属组分和C 3 -C 12多羟基化合物处理无定形二氧化硅氧化铝载体,(b) 催化剂载体在至多200℃的温度下形成浸渍的载体,和(c)硫化浸渍的载体以获得硫化催化剂。
-
公开(公告)号:US10279340B2
公开(公告)日:2019-05-07
申请号:US14366739
申请日:2012-12-20
Applicant: SHELL OIL COMPANY
Inventor: Cornelis Ouwehand , Marcello Stefano Rigutto , Arend Jan Van Welsenes
IPC: B01J21/12 , B01J29/06 , C10G65/00 , C10G47/12 , B01J31/04 , B01J23/883 , B01J37/02 , B01J37/18 , B01J37/20 , B01J37/32 , B01J23/888 , B01J27/19 , B01J35/02 , B01J37/00 , B01J27/049 , B01J31/02 , B01J31/34
Abstract: Process for preparing a sulphided hydrocracking catalyst comprising the steps of (a) treating an amorphous silica alumina carrier with one or more Group VIB metal components, one or more Group VIII metal components and a C3-C12 polyhydric compound, (b) drying the treated catalyst carrier at a temperature of at most 200° C. to form an impregnated carrier, and (c) sulphiding the impregnated carrier to obtain a sulphided catalyst.
-