公开(公告)号:US12209153B2
公开(公告)日:2025-01-28
申请号:US17127597
申请日:2020-12-18
Applicant: SWIMC LLC
Inventor: Allen Bulick , Chris Fredrickson , Mary Jane Hibben , Robert Sandoval , Ashley Rodgers , Glenn Frazee
IPC: C08F220/18 , C09J133/06 , E04D7/00 , E04D11/02
Abstract: A latex emulsion that includes an aqueous carrier liquid and a latex copolymer formed from reactants comprising butyl methacrylate, wherein the reactants comprise at least 20 wt. % a vinyl monomer, based on the total weight of ethylenically unsaturated monomers in the latex copolymer. A homopolymer formed from the vinyl monomer preferably exhibits a glass transition temperature of between about −10° C. and about 30° C. A coating formed from the latex emulsion preferably exhibits a dry adhesion of greater than about 4 pounds per linear inch when applied between a thermoplastic polyolefin roofing membrane and a plywood roofing substrate at an average coat weight of about 6 lbs/100 ft2 and subjected to 180° peel testing according to ASTM D903 with a 2-inch per minute pull rate. The latex emulsion may include a second latex copolymer or stage, and may be used as part of an aqueous adhesive composition.
-
公开(公告)号:US20210102098A1
公开(公告)日:2021-04-08
申请号:US17127597
申请日:2020-12-18
Applicant: SWIMC LLC
Inventor: Allen Bulick , Chris Fredrickson , Mary Jane Hibben , Robert Sandoval , Ashley Rodgers , Glenn Frazee
IPC: C09J133/06 , C08F220/18 , E04D11/02 , E04D7/00
Abstract: A latex emulsion that includes an aqueous carrier liquid and a latex copolymer formed from reactants comprising butyl methacrylate, wherein the reactants comprise at least 20 wt. % a vinyl monomer, based on the total weight of ethylenically unsaturated monomers in the latex copolymer. A homopolymer formed from the vinyl monomer preferably exhibits a glass transition temperature of between about −10° C. and about 30° C. A coating formed from the latex emulsion preferably exhibits a dry adhesion of greater than about 4 pounds per linear inch when applied between a thermoplastic polyolefin roofing membrane and a plywood roofing substrate at an average coat weight of about 6 lbs/100 ft2 and subjected to 180° peel testing according to ASTM D903 with a 2-inch per minute pull rate. The latex emulsion may include a second latex copolymer or stage, and may be used as part of an aqueous adhesive composition.
-
公开(公告)号:US20190316011A1
公开(公告)日:2019-10-17
申请号:US16383398
申请日:2019-04-12
Applicant: SWIMC LLC
Inventor: Allen Bulick , Chris Fredrickson , Mary Jane Hibben , Robert Sandoval , Ashley Rodgers , Glenn Frazee
IPC: C09J133/06 , C08F220/18 , E04D7/00 , E04D11/02
Abstract: A latex emulsion that includes an aqueous carrier liquid and a latex copolymer formed from reactants comprising butyl methacrylate, wherein the reactants comprise at least 20 wt. % a vinyl monomer, based on the total weight of ethylenically unsaturated monomers in the latex copolymer. A homopolymer formed from the vinyl monomer preferably exhibits a glass transition temperature of between about −10° C. and about 30° C. A coating formed from the latex emulsion preferably exhibits a dry adhesion of greater than about 4 pounds per linear inch when applied between a thermoplastic polyolefin roofing membrane and a plywood roofing substrate at an average coat weight of about 6 lbs/100 ft2 and subjected to 180° peel testing according to ASTM D903 with a 2-inch per minute pull rate. The latex emulsion may include a second latex copolymer or stage, and may be used as part of an aqueous adhesive composition.
-
-