A PROCESS OF PRODUCING A DUPLEX STAINLESS STEEL TUBE

    公开(公告)号:US20190010569A1

    公开(公告)日:2019-01-10

    申请号:US16066156

    申请日:2016-12-28

    Abstract: A process of producing a duplex stainless steel tube comprises the steps of: a) producing an ingot or a continuous casted billet of said duplex stainless steel; b) hot extruding the ingot or the billet obtained from step a) into a tube; and c) cold rolling the tube obtained from step b) to a final dimension thereof. The outer diameter D and the wall thickness t of the cold rolled tube is 50-250 mm respectively is 5-25 mm, and, for the cold rolling step, R and Q are set such that the following formula is satisfied: Rp0.2target=416.53+113.26·log Q+4.0479·R+2694.9·C %−82.750·(log Q)2−0.04279·R2−2.2601·log Q·R+16.9·Cr %+26.1·Mo %+83.6·N %+Z  (1) wherein Rp0.2target is targeted yield strength and is 800-1100 MPa and 0

    A PROCESS OF PRODUCING AN AUSTENITIC STAINLESS STEEL TUBE

    公开(公告)号:US20190017134A1

    公开(公告)日:2019-01-17

    申请号:US16066721

    申请日:2016-12-28

    Abstract: A process of producing an austenitic stainless steel tube comprises the steps of: a) producing an ingot or a continuous casted billet of the austenitic stainless steel, b) hot extruding the ingot or the billet obtained from step a) into a tube, c) cold rolling the tube obtained from step b) to a final dimension thereof. The outer diameter D of the cold rolled tube is 70-250 mm and the thickness t thereof is 6-25 mm, and the cold rolling step is performed such that the following formula is satisfied: (2.5×Rc+1.85×Rh−17.7×Q)=(Rp0.2target+49.3−1073×C−21Cr−7.17×Mo−833.3×N)±Z   (1) wherein Rp0.2target is targeted yield strength and is 750≤Rp0.2target≤1000 MPa, 30≤Rc≤75%, 50%≤Rh≤90%, 1≤Q≤3.6, and Z is 65.

Patent Agency Ranking