公开(公告)号:US20150352909A1
公开(公告)日:2015-12-10
申请号:US14655448
申请日:2013-12-23
Applicant: Sik BOEN
Inventor: Sik BOEN
CPC classification number: B60C17/009 , B60C5/00 , B60C17/0009 , B60C2001/0033 , C08K3/04 , C08L7/00 , C08L9/00
Abstract: Run-flat tires having a sidewall support that is manufactured from particular rubber composition. These compositions are based upon a cross-linkable elastomer composition having, per 100 parts by weight of rubber, a polybutadiene rubber having a Mooney viscosity of between 55 and 85 and a low-surface area, high-structure carbon black. An additional second rubber component may also be included in the elastomer composition. The low-surface area, high-structure carbon black may be characterized as having a nitrogen surface area of between 15 m2/g and 25 m2/g and a COAN of between 65 ml/100 g and 85 ml/100 g.
Abstract translation: 具有由特定橡胶组合物制造的侧壁支撑件的润滑轮胎。 这些组合物基于可交联的弹性体组合物,每100重量份橡胶,门尼粘度为55至85的聚丁二烯橡胶和低表面积的高结构炭黑。 弹性体组合物中还可以包含另外的第二橡胶组分。 低表面积的高结构炭黑可以表征为具有15m 2 / g至25m 2 / g的氮表面积和65ml / 100g和85ml / 100g之间的COAN。
-
公开(公告)号:US20150344680A1
公开(公告)日:2015-12-03
申请号:US14654885
申请日:2013-12-23
Applicant: Sik BOEN
Inventor: Sik BOEN
CPC classification number: C08L9/00 , B60C17/0009 , B60C2001/0033 , C08K3/04 , C08K2201/006 , C08K2201/014 , C08L7/00 , C08L15/00
Abstract: Particular embodiments include run-flat tires having sidewall supports that are manufactured from a rubber composition that is based upon a tin end-functionalized polybutadiene rubber as well as an additional second rubber component and a mixture of carbon blacks. The first carbon black may be characterized as being a low-surface area, high-structure carbon black and the second carbon black may be characterized as a low-surface area carbon black. The low-surface area, high-structure carbon black may be added to the rubber composition in an amount that provides a modulus of elongation at 10% measured at 23° C. of between 8 MPa and 10 MPa.
Abstract translation: 具体实施方案包括具有侧壁支撑件的平底轮胎,其由基于锡末端官能化聚丁二烯橡胶的橡胶组合物以及另外的第二橡胶组分和炭黑混合物制成。 第一炭黑可以表征为低表面积,高结构炭黑,第二炭黑可以表征为低表面积炭黑。 可以将低表面积的高结构炭黑以在23℃下测得的10%的伸长模量提供在8MPa和10MPa之间的量加入橡胶组合物中。
-