Abstract:
An object of the present invention is to provide a positive electrode mixture capable of conducting stable charging and discharging with a less amount of gasses generated which has an operating voltage or an initial crystal phase transition voltage of not less than 4.5 V on the basis of lithium. The present invention relates to a positive electrode mixture comprising carbon black having a bulk density of not more than 0.1 g/cm3, a crystallite size of 10 to 40 Å, an iodine adsorption of 1 to 150 mg/g, a volatile content of not more than 0.1% and a metal impurity content of not more than 20 ppm, and a positive electrode active substance having an operating voltage or an initial crystal phase transition voltage of not less than 4.5 V on the basis of lithium.
Abstract:
The present invention relates to Li-Ni composite oxide particles that exhibit a high initial discharge capacity and are excellent in thermal stability when used as a positive electrode active substance for non-aqueous electrolyte secondary batteries, and a process for producing the Li-Nicomposite oxide particles. The Li-Ni composite oxide particles of the present invention have a composition of LixNi1−y−a−bCoyM1aM2bO2 wherein x, y, a and b represent 1.00≦x≦1.10; 0
Abstract:
The present invention relates to Li—Ni composite oxide particles that exhibit a high initial discharge capacity and are excellent in thermal stability when used as a positive electrode active substance for non-aqueous electrolyte secondary batteries, and a process for producing the Li—Ni composite oxide particles. The Li—Ni composite oxide particles of the present invention have a composition of LixNi1-y-a-bCoyM1aM2bO2 wherein x, y, a and b represent 1.00≦x≦1.10; 0