Abstract:
The present invention relates to vinyl polymers having certain characteristics which confer flame-retardant properties to the polymer and their polymeric compositions with other vinyl polymers.
Abstract:
The present invention relates to a concentrated polymeric composition which comprises: a) vinyl aromatic polymers and/or copolymers in an amount ranging from 10% to 90% by weight, calculated with respect to the overall composition, with respect to the overall composition, b) at least one compound containing epoxy functional groups in an amount ranging from 0.01% to 5% by weight, calculated with respect to the overall composition, with respect to the overall composition, c) at least one infrared absorbing agent, in an amount ranging from 10% to 90% by weight, calculated with respect to the overall composition, with respect to the overall composition.
Abstract:
The present invention relates to a concentrated polymeric composition which comprises: a) vinyl aromatic polymers and/or copolymers in an amount ranging from 10% to 90% by weight, calculated with respect to the overall composition, with respect to the overall composition, b) at least one compound containing epoxy functional groups in an amount ranging from 0.01% to 5% by weight, calculated with respect to the overall composition, with respect to the overall composition, c) at least one infrared absorbing agent, in an amount ranging from 10% to 90% by weight, calculated with respect to the overall composition, with respect to the overall composition.
Abstract:
A mixture comprising: a) from 0% to 95% of aromatic compounds and/or polycyclic aromatic compounds, said polycyclic aromatic compounds, if present, always being in an amount less than 10% with respect to component (a); b) from 0% to 85% of a mixture containing aliphatic compounds and a content of aromatic compounds lower than 30% with respect to (b); c) from 0% to 20% of an acetate component; d) from 1% to 50% of a mixture of compounds containing keto groups; with the proviso that said solvent mixture contains at least three components, one of which is (d) and the other two selected from (a), (b) or (c) and that their sum is always 00%; and with the proviso that said mixture has a solubility, measured with the Hansen parameters, characterized in that the dispersion force component of the solubility δd varies from 17 to 20 Mpa{circumflex over ( )}0.5 the polar force component of the solubility δp varies from 0.65 to 5 Mpa{circumflex over ( )}0.5, and the strength of the hydrogen bond component of the solubility δh varies from 0.65 to 5 MPa{circumflex over ( )}0.5.