公开(公告)号:US4485200A
公开(公告)日:1984-11-27
申请号:US345295
申请日:1982-02-03
Applicant: Witold Perlinski , Irwin J. Davis , John F. Romanick
Inventor: Witold Perlinski , Irwin J. Davis , John F. Romanick
IPC: C08L7/00 , C08G59/00 , C08G59/40 , C08K3/18 , C08K3/22 , C08L11/02 , C08L21/00 , C08L57/00 , C08L57/02 , C08L63/00 , C08L93/00 , C09J113/02 , C09J121/00 , C08L61/04
CPC classification number: C09J113/02
Abstract: Conventional carboxylated neoprene latex adhesives are improved with respect to their metal adhesion, heat and water resistance and bonding range by the addition thereto of an epoxy resin, preferably an epoxy resin prepared by the reaction of para-aminophenol with epichlorohydrin.
Abstract translation: 通过添加环氧树脂,优选通过对氨基苯酚与表氯醇的反应制备的环氧树脂,常规的羧化氯丁橡胶胶乳粘合剂相对于其金属粘附性,耐热性和耐水性以及粘合范围得到改善。
-
公开(公告)号:US4342843A
公开(公告)日:1982-08-03
申请号:US237791
申请日:1981-02-24
Applicant: Witold Perlinski , Irwin J. Davis , John F. Romanick
Inventor: Witold Perlinski , Irwin J. Davis , John F. Romanick
IPC: C09J111/02 , C08L63/00 , C08L9/10
CPC classification number: C09J111/02
Abstract: The metal adhesion and heat and water resistance of conventional neoprene latex adhesives are improved by the addition thereto of a polyamine and an epoxy resin wherein for every 100 parts by weight of dry neoprene, the epoxy is added in an amount of 10-40 parts and the amine is added in an amount sufficient to provide 50-150% of the stoichiometric amount required to cure the epoxy.
Abstract translation: 通过添加多胺和环氧树脂,改善了常规氯丁橡胶胶乳粘合剂的金属粘合性和耐热性和耐水性,其中对于每100重量份干氯丁橡胶,环氧树脂加入量为10-40份, 以足以提供固化环氧树脂所需化学计量的50-150%的量加入胺。
-
公开(公告)号:US5821294A
公开(公告)日:1998-10-13
申请号:US708106
申请日:1996-08-30
Applicant: Witold Perlinski
Inventor: Witold Perlinski
IPC: C08L79/02 , C08F8/30 , C08G73/00 , C08J5/12 , C09J5/00 , C09J11/06 , C09J123/08 , C09J133/00 , C09J175/04 , C09J175/06 , C09J179/02 , C09J201/00 , C08J3/00 , C08K3/20 , C08L75/00
CPC classification number: C08J5/127 , C08F8/30 , C09J175/06 , C08G2170/80
Abstract: A water-based adhesive that is delivered in a stable one-part system comprises (i) an emulsion of a vinyl and/or acrylic polymer; (ii) a water-dispersed ionic or nonionic polyurethane; (iii) a polyethylenimine; and (iv) a carbodiimide.
Abstract translation: 在稳定的一部分系统中输送的水性粘合剂包括(i)乙烯基和/或丙烯酸类聚合物的乳液; (ii)水分散的离子或非离子聚氨酯; (iii)聚乙烯亚胺; 和(iv)碳二亚胺。
-
公开(公告)号:US5403884A
公开(公告)日:1995-04-04
申请号:US3765
申请日:1993-01-13
Applicant: Witold Perlinski
Inventor: Witold Perlinski
IPC: B05D1/16 , C08J7/04 , C09J123/08 , D04H11/00 , C08L9/00
CPC classification number: D04H11/00 , B05D1/16 , C08J7/047 , C09J123/08 , C08J2323/16 , C08J2423/00
Abstract: A process for flocking cured or uncured elastomeric substrates comprising the steps of applying to the substrate an aqueous adhesive comprising 10 to 100% (dry weight) of an alkaline dispersion of an ethylene carboxylic acid copolymer and 0 to 90% of an aqueous elastomeric dispersion; electrostatically applying flocking fibers thereto; and drying the thus flocked substrate.
Abstract translation: 一种用于植入固化或未固化的弹性体基材的方法,包括以下步骤:向基材施加包含10至100%(干重)的乙烯羧酸共聚物的碱性分散体和0至90%的弹性体分散体的水性粘合剂的步骤; 将植绒纤维静电应用于其上; 并干燥由此植绒的基底。
-
公开(公告)号:US4463110A
公开(公告)日:1984-07-31
申请号:US349803
申请日:1982-02-18
Applicant: Witold Perlinski , Irwin J. Davis , John F. Romanick
Inventor: Witold Perlinski , Irwin J. Davis , John F. Romanick
IPC: C09J111/02 , C08L9/00 , C08L61/04 , C08L63/00
CPC classification number: C09J111/02
Abstract: The metal adhesion and heat and water resistance of conventional neoprene latex adhesives are improved by the addition thereto of a polyfunctional amine and an epoxy resin wherein for every 100 parts by weight of dry neoprene, the epoxy is added in an amount of 10-40 parts and the amine is added in an amount sufficient to provide 50-150% of the stoichiometric amount required to cure the epoxy.
Abstract translation: 通过添加多官能胺和环氧树脂,改善了常规氯丁橡胶胶乳粘合剂的金属粘附性和耐热性和耐水性,其中对于每100重量份干氯丁橡胶,环氧树脂的加入量为10-40份 并且胺的加入量足以提供固化环氧树脂所需的化学计量量的50-150%。
-
-
-
-