公开(公告)号:US20140374670A1
公开(公告)日:2014-12-25
申请号:US13921785
申请日:2013-06-19
Applicant: Xerox Corporation
Inventor: Mahya Mokhtari , Tila Tahmoures-Zadeh , Roger E. Gaynor
IPC: C09D11/00
Abstract: In an embodiment, there is a method of preparing a conductive ink formulation. The method can include dissolving a stabilizer in a first solvent, adding a reducing agent to the first solvent, adding a metal salt to the first solvent and forming a slurry by precipitating stabilized metal nanoparticles in the first solvent. The method can also include forming a wet cake of the stabilized metal nanoparticles and adding the wet cake to a second solvent. The second solvent can include at least one of a polyvinyl alcohol derivative. The wet cake may not be actively dried prior to being added to the second solvent.
Abstract translation: 在一个实施方案中,存在制备导电油墨制剂的方法。 该方法可以包括将稳定剂溶解在第一溶剂中,向第一溶剂中加入还原剂,向第一溶剂中加入金属盐并通过在第一溶剂中沉淀稳定的金属纳米颗粒而形成浆料。 该方法还可以包括形成稳定的金属纳米颗粒的湿滤饼并将湿滤饼加入到第二溶剂中。 第二溶剂可以包括聚乙烯醇衍生物中的至少一种。 在添加到第二溶剂之前,湿饼可能不会被主动干燥。
-
公开(公告)号:US09105373B2
公开(公告)日:2015-08-11
申请号:US13921785
申请日:2013-06-19
Applicant: XEROX CORPORATION
Inventor: Mahya Mokhtari , Tila Tahmoures-Zadeh , Roger E. Gaynor
Abstract: In an embodiment, there is a method of preparing a conductive ink formulation. The method can include dissolving a stabilizer in a first solvent, adding a reducing agent to the first solvent, adding a metal salt to the first solvent and forming a slurry by precipitating stabilized metal nanoparticles in the first solvent. The method can also include forming a wet cake of the stabilized metal nanoparticles and adding the wet cake to a second solvent. The second solvent can include at least one of a polyvinyl alcohol derivative. The wet cake may not be actively dried prior to being added to the second solvent.
Abstract translation: 在一个实施方案中,存在制备导电油墨制剂的方法。 该方法可以包括将稳定剂溶解在第一溶剂中,向第一溶剂中加入还原剂,向第一溶剂中加入金属盐并通过在第一溶剂中沉淀稳定的金属纳米颗粒而形成浆料。 该方法还可以包括形成稳定的金属纳米颗粒的湿滤饼并将湿滤饼加入到第二溶剂中。 第二溶剂可以包括聚乙烯醇衍生物中的至少一种。 在添加到第二溶剂之前,湿饼可能不会被主动干燥。
-