Abstract:
The disclosure describes a process for making a polyester resin of defined acid value using a temperature-sensitive reaction and dipropylene glycol as a reagent.
Abstract:
The disclosure provides sustainable toner particles of from about 180 nm to about 250 nm in a sustainable toner composition having a hot offset temperature of from about 190° C. to about 220° C.
Abstract:
The disclosure describes a one reaction process for making a bio-based polyester resin. The resultant polyester resin retains thermal properties as compared to a similar resin but made using previous multi-step processes conducted in separate vessels.
Abstract:
The disclosure provides sustainable toner particles of from about 180 nm to about 250 nm in a sustainable toner composition having a hot offset temperature of from about 190° C. to about 220° C.
Abstract:
The disclosure provides sustainable toner particles of from about 180 nm to about 250 nm in a sustainable toner composition having a hot offset temperature of from about 190° C. to about 220° C.