公开(公告)号:US20240360345A1
公开(公告)日:2024-10-31
申请号:US18646359
申请日:2024-04-25
Applicant: tesa SE
Inventor: Marco Kupsky , Francisco Lossada , Bastian Kruskop , Christian Schuh , Lena-Marie Naujoks , Nadine Wedel
IPC: C09J7/38 , C09J133/06
CPC classification number: C09J7/385 , C09J133/068 , C09J2203/326 , C09J2301/302 , C09J2301/416 , C09J2301/50 , C09J2433/00 , C09J2463/00
Abstract: A chemical-resistant, reactive, pressure-sensitive adhesive tape with a reactive adhesive compound comprising at least one epoxide compound, at least one initiator for curing the epoxide compound, and a poly(meth)acrylate which contains a high fraction of at least 55 percent by weight of monomers having aromatic radicals.
-
公开(公告)号:US20230287249A1
公开(公告)日:2023-09-14
申请号:US18119942
申请日:2023-03-10
Applicant: tesa SE
Inventor: Christian Schuh , Nadine Wedel , Bastian Kruskop , Lena-Marie Naujoks , Nora Erben
IPC: C09J151/00 , C09J7/10
CPC classification number: C09J151/006 , C09J7/10
Abstract: The invention relates to a curable adhesive comprising, based on the mass of the curable adhesive: a) one or more (meth)acrylate block copolymers of the structure A-B-A in a combined mass fraction of 25% or more, where the A blocks independently of one another stand for a poly(meth)acrylate having a glass transition temperature Tg of 50° C. or more which is preparable by polymerization of an A monomer composition composed of A monomers, where the B block stands for a poly(meth)acrylate having a glass transition temperature Tg of less than 50° C. which is preparable by polymerization of a B monomer composition composed of B monomers, b) one or more polymerizable first epoxide compounds E1 in a combined mass fraction of 5% or more, where the first epoxide compound E1 at 25° C. is a solid or a high-viscosity substance, and c) one or more polymerizable second epoxide compounds E2 in a combined mass fraction of 5% or more, where the second epoxide compound E2 at 25° C. is a liquid, where the amount-of-substance-weighted polar component of the Hansen solubility parameters of the monomer units derived from A monomers in the A blocks, (A), is in the range from 9.0 to 11.0 MPa0.5, and where the amount-of-substance-weighted polar component of the Hansen solubility parameters of the monomer units derived from B monomers in the B blocks, (B) is less than 9 MPa0.5.
-