公开(公告)号:DK0623630T3
公开(公告)日:1997-06-16
申请号:DK94106624
申请日:1994-04-28
Applicant: BASF AG
Inventor: SCHNEIDER KARL-HEINRICH DR , MOENCH DIETMAR DR , HARTMANN HEINRICH DR , GEBHARDT NORBERT DR
Abstract: Water-in-oil polymer emulsions, characterised in that they contain water-soluble polymers having a mean particle size of from 0.1 to 20 mu m emulsified in a continuous oil phase comprising at least 50% by weight of an oil of vegetable or animal origin with the aid of from 0.5 to 15% by weight, based on the total emulsion, of an emulsifier mixture comprising a) from 5 to 95% by weight of a block or graft copolymer of the formula (A-COO)m-B, in which A is a hydrophobic polymer having a molecular weight of > 500 g/mol based on a poly(hydroxycarboxylic acid), B is a bifunctional hydrophilic polymer having a molecular weight of > 500 g/mol based on a polyalkylene oxide, and m is at least 2, and b) from 5 to 95% by weight of another water-in-oil emulsifier having a molecular weight of
-
公开(公告)号:DE4428597A1
公开(公告)日:1996-02-15
申请号:DE4428597
申请日:1994-08-12
Applicant: BASF AG
Abstract: Disclosed is a method for producing condensation polymers of aspartic acid by means of condensation polymerization of aspartic acid at temperatures of 140 DEG C in the presence of, relative to aspartic acid, from 1 to less than 5 mol % phosphorous acid or hypophosphorous acid catalyst, and the use of the resulting condensation polymers of aspartic acid as additives in washing and cleaning products, amounting to 0.1 to 10 wt % relative to the washing and cleaning products.
-
公开(公告)号:DE4315172A1
公开(公告)日:1994-11-10
申请号:DE4315172
申请日:1993-05-07
Applicant: BASF AG
Inventor: SCHNEIDER KARL-HEINRICH DR , MOENCH DIETMAR DR , HARTMANN HEINRICH DR , GEBHARDT NORBERT DR
IPC: C02F1/52 , C02F1/56 , C02F11/14 , C08F2/32 , C09K23/52 , D21H17/34 , D21H21/10 , B01F17/52 , B01D21/01
Abstract: Water-in-oil polymer emulsions, characterised in that they contain water-soluble polymers having a mean particle size of from 0.1 to 20 mu m emulsified in a continuous oil phase comprising at least 50% by weight of an oil of vegetable or animal origin with the aid of from 0.5 to 15% by weight, based on the total emulsion, of an emulsifier mixture comprising a) from 5 to 95% by weight of a block or graft copolymer of the formula (A-COO)m-B, in which A is a hydrophobic polymer having a molecular weight of > 500 g/mol based on a poly(hydroxycarboxylic acid), B is a bifunctional hydrophilic polymer having a molecular weight of > 500 g/mol based on a polyalkylene oxide, and m is at least 2, and b) from 5 to 95% by weight of another water-in-oil emulsifier having a molecular weight of
-
公开(公告)号:DE19707221A1
公开(公告)日:1998-08-27
申请号:DE19707221
申请日:1997-02-24
Applicant: BASF AG
Inventor: RUPANER ROBERT DR , LEY GREGOR DR , ZELLER DIETER DR , GEBHARDT NORBERT DR , MENDERA PETER , HEINZ GERHART , NEUTZNER JOSEF DR , BAUER GERHARD DR
Abstract: In order to prepare an antibacterial and fungicidal polymer dispersion, a polymer dispersion is mixed with an amount of a protective polymer which is dispersible in the polymer dispersion, said amount being sufficient to attain an antibacterial and fungicidal effect. The protective polymer comprises: between 3 and 60 wt %, relative to the total weight of components a) and b) without metallic ions, of at least one C3 to C7 alpha, beta-monoethylenically unsaturated mono or dicarboxylic acid which is partially or completely neutralized or can be present as an anhydride, as component a); between 97 and 40 wt %, relative to the total weight of components a) and b) without metallic ions, of at least one C1 to C20 alkyl(meth)acrylate, of a C1 to C20 carboxylic acid vinyl ester, of a vinyl aromatic containing up to 20 carbon atoms, of an ethylenically unsaturated C3 to C6 nitrile, of a vinyl halide or a non-aromatic C4 to C8 hydrocarbon and at least two conjugated double bonds or ethylene or propylene as component b); between 0 and 50 wt %, relative to the total weight of components a) and b) without metallic ions, of at least one further ethylenically unsaturated monomer, as component c); and between 0 and 20 wt %, relative to the total weight of components a), b) and c) without metallic ions, of at least one cross-linking polyfunctional monomer, as component d). Between 1 and 100 mol % of the acid groups are converted into salts of at least one antibacterial and/or fungicidal metallic ion.
-
公开(公告)号:DE59401442D1
公开(公告)日:1997-02-13
申请号:DE59401442
申请日:1994-04-28
Applicant: BASF AG
Inventor: SCHNEIDER KARL-HEINRICH DR , MOENCH DIETMAR DR , HARTMANN HEINRICH DR , GEBHARDT NORBERT DR
Abstract: Water-in-oil polymer emulsions, characterised in that they contain water-soluble polymers having a mean particle size of from 0.1 to 20 mu m emulsified in a continuous oil phase comprising at least 50% by weight of an oil of vegetable or animal origin with the aid of from 0.5 to 15% by weight, based on the total emulsion, of an emulsifier mixture comprising a) from 5 to 95% by weight of a block or graft copolymer of the formula (A-COO)m-B, in which A is a hydrophobic polymer having a molecular weight of > 500 g/mol based on a poly(hydroxycarboxylic acid), B is a bifunctional hydrophilic polymer having a molecular weight of > 500 g/mol based on a polyalkylene oxide, and m is at least 2, and b) from 5 to 95% by weight of another water-in-oil emulsifier having a molecular weight of
-
-
-
-