公开(公告)号:JPH0911230A
公开(公告)日:1997-01-14
申请号:JP7288296
申请日:1996-03-27
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , HOFMANN JUERGEN , OHLIG HILMAR , MAILAHN ELMAR , BUS KLAUS , CZAUDERNA BERNHARD , GRABOWSKI SVEN
IPC: C08J5/18 , B29B7/48 , B29B7/58 , B29C47/40 , B29C48/76 , C08J3/20 , C08J3/205 , C08L25/04 , C08L27/06 , C08L33/04 , C08L33/12 , C08L51/00 , C08L51/04 , C08L55/02 , D01F6/00
Abstract: PROBLEM TO BE SOLVED: To produce an impact-resistant thermoplastic resin composed of a wet elastomer component and a fragile thermoplastic polymer in an industrially simple manner by one treatment process if possible. SOLUTION: An elastomer component A is supplied to a twin-screw extruder formed from a distribution section, a crushing section, a, section supplying a thermoplastic polymer B to the extruder, a section equipped with a mixing element, a kneading element and/or a separate plasticizing element, a degassing section and a feed-out zone in a feed direction and equipped with screws rotated in the same way and the water discharged from a dehydration opening is allowed to be present as a liquid phase partially or wholly. Therefore, the residual water contained in rubber partially dehydrated at first is already removed as water in the first crushing section and the feed amt. of rubber is 3-8wt.% of the amt. of the wet rubber in the first crushing section and below 1wt.% in a second crushing section.
-
公开(公告)号:JPH091546A
公开(公告)日:1997-01-07
申请号:JP7288396
申请日:1996-03-27
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , HOFMANN JUERGEN , OHLIG HILMAR , MAILAHN ELMAR , BUS KLAUS , CZAUDERNA BERNHARD , GRABOWSKI SVEN
IPC: B29B7/88 , B29B7/48 , B29B7/58 , B29B13/06 , B29C47/40 , B29C48/395 , B29C48/76 , C08G85/00 , C08J3/20 , C08J3/205 , C08L25/04 , C08L27/06 , C08L33/04 , C08L33/12 , C08L33/18 , C08L33/20 , C08L51/00 , C08L51/04 , C08L55/02 , C08L101/00
Abstract: PROBLEM TO BE SOLVED: To manufacture impact resistant thermoplastic in a single step as far as possible by supplying elastomer composition containing residual moisture up to specific wt.% to a biaxial extruder having double threaded screws rotating in the same direction so that the moisture from a dehydration part partly or entirely becomes a liquid state. SOLUTION: The zones of a biaxial extruder are arranged as follows toward the axial direction of the extruder. The zones include the metering supply zone 2 of elastomer composition A containing the residual moisture up to 60wt.%, first compression zone 3, second compression zone 3', intermediate site feeding screw zone 0, zone 4 supplied with melted material of thermoplastic B, first plasticizing zone 5, second plasticizing zone 5', first deaerating zone 6, second deaerating zone 6' and discharge zone 7. The two screws of the extruder are formed as deeply engraved threads and double threads. The extruder is operated by the number of revolutions of the screw from 50 to 600min , and shearing speed of 20 to 240s .
-
公开(公告)号:DE50104988D1
公开(公告)日:2005-02-03
申请号:DE50104988
申请日:2001-10-04
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , HOFMANN JUERGEN , MAILAHN ELMAR , OHLIG HILMAR
Abstract: The present invention relates to a mixing apparatus at least composed of a screw-based machine S 1 and a screw-based machine S 2 , where S 1 has heating equipment, at least in the plasticizing and homogenizing zone, and where the outlet from S 2 has been connected to the screw-containing barrel of S 1 , within the plasticizing or homogenizing zone of S 1 , a substantive feature of which is that the connection between S 1 and S 2 is brought about by a connector which has cooling equipment effective as far as the inner wall of the screw-containing barrel of S 1 , and to a process for preparing thermoplastically processable molding compositions, in particular additive masterbatches, from at least one thermoplastic component C 1 and at least one component C 2 , where the melting point or decomposition temperature T M C2 of C 2 is lower, by at least about 50° C., than the temperature T H C1 , which is the lower limit of the thermoforming range of C 1 , and where most of C 2 is melted only after contact with C 1.
-
公开(公告)号:DE59903334D1
公开(公告)日:2002-12-12
申请号:DE59903334
申请日:1999-08-06
Applicant: BASF AG
Inventor: ANDERLIK RAINER , KREMESKOETTER JENS , MAILAHN ELMAR , GUENTHERBERG NORBERT , ITTEMANN PETER , HOFMANN JUERGEN , SACK HEINRICH
-
公开(公告)号:DE59703819D1
公开(公告)日:2001-07-19
申请号:DE59703819
申请日:1997-09-12
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , HOFMANN JUERGEN , MAILAHN ELMAR , OHLIG HILMAR , CZAUDERNA BERNHARD , GRABOWSKI SVEN , BUS KLAUS
IPC: B29B7/48 , B29B7/58 , B29B13/06 , B29C48/40 , B29C48/67 , B29C48/76 , B29C63/00 , C08J3/20 , C08J3/205 , C08J5/18 , C08L21/00 , C08L51/04 , B29C47/40 , B29C47/64 , B29C47/76
Abstract: PCT No. PCT/EP97/05000 Sec. 371 Date Mar. 25, 1999 Sec. 102(e) Date Mar. 25, 1999 PCT Filed Sep. 12, 1997 PCT Pub. No. WO98/13412 PCT Pub. Date Apr. 2, 1998A process for preparing thermoplastics or polymer blends comprising (A) from 5 to 95% of a water-moist elastomer component containing up to 60% of residual water, (B) from 5 to 95% of a thermoplastic polymer, (C) from 0 to 95% of a further polymer, and (D) from 0 to 70% of additives, said process comprising mixing the components A to D in an extruder with mechanical dewatering of component A, wherein the extruder has at least two rotating screws and, in the conveying direction, is essentially composed of a metering section into which component A is fed, a squeeze section which serves for dewatering component A and contains a retarding element and an associated dewatering orifice which is present upstream of the retarding element by a distance corresponding to at least one screw diameter, a feed section in which the thermoplastic polymer B is introduced as a melt into the extruder, a plastication section with mixing or kneading elements, a devolatilization section with an orifice and in which the remaining water is removed as steam, and a discharge zone.
-
公开(公告)号:CZ9901076A3
公开(公告)日:2000-09-13
申请号:CZ107699
申请日:1997-09-12
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , HOFMANN JUERGEN , MAILAHN ELMAR , OHLIG HILMAR , CZAUDERNA BERNHARD , GRABOWSKI SVEN , BUS KLAUS
IPC: B29B7/48 , B29B7/58 , B29B13/06 , B29C47/40 , B29C47/64 , B29C47/76 , B29C63/00 , C08J3/20 , C08J3/205 , C08J5/18 , C08L21/00 , C08L51/04
CPC classification number: B29B13/06 , B29C47/0011 , B29C47/0019 , B29C47/0023 , B29C47/40 , B29C47/64 , B29C47/76 , C08J3/205 , C08L51/04
-
公开(公告)号:CA2339738A1
公开(公告)日:2000-02-17
申请号:CA2339738
申请日:1999-08-06
Applicant: BASF AG
Inventor: ANDERLIK RAINER , KREMESKOTTER JENS , GUNTHERBERG NORBERT , SACK HEINRICH , MAILAHN ELMAR , HOFMANN JURGEN , ITTEMANN PETER
IPC: C08J3/20 , A01N25/18 , A61L9/04 , C08J3/22 , C08J5/00 , C08K5/00 , C08K5/07 , C08L91/00 , C08L101/00
Abstract: The invention relates to a method for producing odorant polymers or plastics , wherein a crushed or fine particle first polymer material is mixed with the desired odorant, is allowed to swell during a predetermined period and then subjected to further treatment at a predetermined pressure and temperature. After swelling with the odorant, the first polymer material can be mixed wit h a second plastic material, wherein the first polymer material and the second plastic material can be identical or different from each. Odorant polymers c an also be obtained by using a polymer as second plastic material. The inventio n also relates to the odorant polymer or the odorant plastic produced accordin g to the inventive method and to a molding material or an object containing th e odorant polymer or the odorant plastic.
-
公开(公告)号:AT285885T
公开(公告)日:2005-01-15
申请号:AT01982395
申请日:2001-10-04
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , HOFMANN JUERGEN , MAILAHN ELMAR , OHLIG HILMAR
Abstract: The present invention relates to a mixing apparatus at least composed of a screw-based machine S 1 and a screw-based machine S 2 , where S 1 has heating equipment, at least in the plasticizing and homogenizing zone, and where the outlet from S 2 has been connected to the screw-containing barrel of S 1 , within the plasticizing or homogenizing zone of S 1 , a substantive feature of which is that the connection between S 1 and S 2 is brought about by a connector which has cooling equipment effective as far as the inner wall of the screw-containing barrel of S 1 , and to a process for preparing thermoplastically processable molding compositions, in particular additive masterbatches, from at least one thermoplastic component C 1 and at least one component C 2 , where the melting point or decomposition temperature T M C2 of C 2 is lower, by at least about 50° C., than the temperature T H C1 , which is the lower limit of the thermoforming range of C 1 , and where most of C 2 is melted only after contact with C 1.
-
公开(公告)号:DE19842203A1
公开(公告)日:2000-02-10
申请号:DE19842203
申请日:1998-08-07
Applicant: BASF AG
Inventor: ANDERLIK RAINER , KREMESKOETTER JENS , MAILAHN ELMAR
IPC: C08J3/20 , A01N25/18 , A61L9/04 , C08J3/22 , C08J5/00 , C08K5/00 , C08K5/07 , C08L91/00 , C08L101/00 , A61K7/46 , C11B9/00
Abstract: The invention relates to a method for producing odorant polymers or plastics, wherein a crushed or fine particle first polymer material is mixed with the desired odorant, is allowed to swell during a predetermined period and then subjected to further treatment at a predetermined pressure and temperature. After swelling with the odorant, the first polymer material can be mixed with a second plastic material, wherein the first polymer material and the second plastic material can be identical or different from each. Odorant polymers can also be obtained by using a polymer as second plastic material. The invention also relates to the odorant polymer or the odorant plastic produced according to the inventive method and to a molding material or an object containing the odorant polymer or the odorant plastic.
-
公开(公告)号:BR9712121A
公开(公告)日:1999-08-31
申请号:BR9712121
申请日:1997-09-12
Applicant: BASF AG
Inventor: GUNTHERBERG NORBERT , HOFMANN JURGEN , MAILAHN ELMAR , OHLIG HILMAR , CZAUDERNA BERNHARD , GRABOWSKI SVEN , BUS KLAUS
IPC: B29B7/48 , B29B7/58 , B29B13/06 , B29C48/40 , B29C48/67 , B29C48/76 , B29C63/00 , C08J3/20 , C08J3/205 , C08J5/18 , C08L21/00 , C08L51/04 , B29C47/40 , B29C47/64 , B29C47/76
Abstract: PCT No. PCT/EP97/05000 Sec. 371 Date Mar. 25, 1999 Sec. 102(e) Date Mar. 25, 1999 PCT Filed Sep. 12, 1997 PCT Pub. No. WO98/13412 PCT Pub. Date Apr. 2, 1998A process for preparing thermoplastics or polymer blends comprising (A) from 5 to 95% of a water-moist elastomer component containing up to 60% of residual water, (B) from 5 to 95% of a thermoplastic polymer, (C) from 0 to 95% of a further polymer, and (D) from 0 to 70% of additives, said process comprising mixing the components A to D in an extruder with mechanical dewatering of component A, wherein the extruder has at least two rotating screws and, in the conveying direction, is essentially composed of a metering section into which component A is fed, a squeeze section which serves for dewatering component A and contains a retarding element and an associated dewatering orifice which is present upstream of the retarding element by a distance corresponding to at least one screw diameter, a feed section in which the thermoplastic polymer B is introduced as a melt into the extruder, a plastication section with mixing or kneading elements, a devolatilization section with an orifice and in which the remaining water is removed as steam, and a discharge zone.
-
-
-
-
-
-
-
-
-