公开(公告)号:JPS63161133A
公开(公告)日:1988-07-04
申请号:JP30880487
申请日:1987-12-08
Applicant: DEGUSSA
Inventor: WAGNER RUDOLF , SCHIWIORA HARRY , STUEMKE MANFRED , GROLL WERNER
Abstract: Palladium alloys consisting of (a) 65 to 85% palladium, (b) 0 to 10% gold and/or 0 to 5% platinum, (c) 0.1 to 10% tin, (d) 1 to 10% gallium, (e) 1 to 12% copper, (f) 0.05 to 1.5% ruthenium and/or 0.05 to 0.7% rhenium as well as (g) 0.01 to 4% tungsten and/or 0.01 to 4% aluminum and/or 0.01 to 4% zinc are use to produce firmly seated and removable dentures. These alloys do not form oxide films when melted in air.
-
公开(公告)号:CA2389428C
公开(公告)日:2009-02-10
申请号:CA2389428
申请日:2000-10-26
Applicant: DEGUSSA
Inventor: HAAS THOMAS , CREUTZ MATTHIAS , WAGNER RUDOLF , SAUER JORG , GLENNEBERG JURGEN , VANHEERTUM RUDOLF
IPC: C01B15/023 , B01J8/02 , B01J10/00 , B01J23/44 , B01J35/02
Abstract: The hydrogenation step in the anthrachinone process for producing hydrogen peroxide in a hydrogenation reactor performed on a solid bed catalyst from particle-shaped catalyst is known in prior art. According to the invention, the residence time of a catalyst is increased by transporting working solution containing reaction support material and transporting a hydrogen-containing gas phase as a mixture from the downside to the upside through a hydrogenati on reactor. The empty pipe velocity of the working solution is 0.05 to 100 m/h, in particular 10 to 50 m/h.
-
公开(公告)号:PL361835A1
公开(公告)日:2004-10-04
申请号:PL36183501
申请日:2001-10-24
Applicant: DEGUSSA
Inventor: NORDHOFF STEFAN , CREUTZ MATTHIAS , GROSS STEFAN , WAGNER RUDOLF
IPC: B01D9/02 , C01B15/013
Abstract: A process for the continuous preparation of very highly concentrated hydrogen peroxide having a content of greater than 80 wt.%, especially over 98 wt.%, by suspension crystallization and after-treatment of the H2O2 crystals. The after-treatment takes the form of countercurrent washing in a hydraulic or mechanical washing column with a packed crystal bed. Hydrogen peroxide is disclosed having a concentration of from 99.9 to 100 wt.% and a content of TOC, nitrate, phosphate, nickel and tin of in each case less than 4 mg/l.
-
公开(公告)号:CA2436892A1
公开(公告)日:2002-06-06
申请号:CA2436892
申请日:2001-10-24
Applicant: DEGUSSA
Inventor: WAGNER RUDOLF , GROSS STEFAN , CREUTZ MATTHIAS , NORDHOFF STEFAN
IPC: B01D9/02 , C01B15/013
Abstract: The invention relates to a process for the continuous preparation of very highly concentrated hydrogen peroxide having a content of greater than 80 wt.%, especially over 98 wt.%, by suspension crystallisation and after- treatment of the H2O2 crystals. According to the invention, the after- treatment takes the form of countercurrent washing in a hydraulic or mechanical washing column with a packed crystal bed. The invention also provides hydrogen peroxide having a concentration of from 99.9 to 100 wt.% a nd a content of TOC, nitrate, phosphate, nickel and tin of in each case less th an 4 mg/l.
-
公开(公告)号:CA2427710A1
公开(公告)日:2002-05-10
申请号:CA2427710
申请日:2001-10-04
Applicant: DEGUSSA
Inventor: CREUTZ MATTHIAS , GLENNEBERG JURGEN , WAGNER RUDOLF , NORDHOFF STEFAN , MOLLER ROLF-DIETER
IPC: B01D9/02 , C01B15/013
Abstract: The invention is directed towards a process for the concentration of aqueous hydrogen peroxide, comprising discontinuous crystallisation. According to the invention, a cooling surface arranged in a crystallising vessel and first wetted with hydrogen peroxide is cooled at a high cooling rate, whereupon seed crystals form. The cooling rate is at least 1 K/s, preferably from 10 to 30 K/s. When the vessel has been filled with H2O2 starting material, the latter crystallises, starting from the seed crystals, and forms a crystal layer. When the mother liquor of lower H2O2 concentration has been discharged, there follows a sweating operation with a slow increase in temperature, as a result of which the H2O2 concentration in the crystal layer is increased further.
-
公开(公告)号:DE19953185A1
公开(公告)日:2001-05-23
申请号:DE19953185
申请日:1999-11-05
Applicant: DEGUSSA
Inventor: HAAS THOMAS , GLENNEBERG JUERGEN , WAGNER RUDOLF , CREUTZ MATTHIAS , SAUER JOERG , VANHEERTUM RUDOLF
IPC: B01J8/02 , B01J10/00 , B01J23/44 , B01J35/02 , C01B15/023
Abstract: The hydrogenation step in the anthrachinone process for producing hydrogen peroxide in a hydrogenation reactor performed on a solid bed catalyst from particle-shaped catalyst is known in prior art. According to the invention, the residence time of a catalyst is increased by transporting working solution containing reaction support material and transporting a hydrogen-containing gas phase as a mixture from the downside to the upside through a hydrogenation reactor. The empty pipe velocity of the working solution is 0.05 to 100 m/h, in particular 10 to 50 m/h.
-
公开(公告)号:AU1387501A
公开(公告)日:2001-05-14
申请号:AU1387501
申请日:2000-10-26
Applicant: DEGUSSA
Inventor: HAAS THOMAS , GLENNEBERG JURGEN , WAGNER RUDOLF , CREUTZ MATTHIAS , SAUER JORG , VANHEERTUM RUDOLF
IPC: B01J8/02 , B01J10/00 , B01J23/44 , B01J35/02 , C01B15/023
Abstract: In carrying out the hydrogenation stage of the anthraquinone process for the preparation of hydrogen peroxide in a hydrogenation reactor on a fixed bed catalyst of a particulate catalyst, the service life of the catalyst is increased in that the working solution comprising the reaction carrier and a gas phase comprising hydrogen, are passed through the hydrogenation reactor from the bottom upwards. The empty tube speed of the working solution is 0.05 to 100 m/h, preferably 10 to 50 m/h.
-
公开(公告)号:CA2389428A1
公开(公告)日:2001-05-10
申请号:CA2389428
申请日:2000-10-26
Applicant: DEGUSSA
Inventor: GLENNEBERG JURGEN , CREUTZ MATTHIAS , HAAS THOMAS , SAUER JORG , VANHEERTUM RUDOLF , WAGNER RUDOLF
IPC: B01J8/02 , B01J10/00 , B01J23/44 , B01J35/02 , C01B15/023
Abstract: The hydrogenation step in the anthrachinone process for producing hydrogen peroxide in a hydrogenation reactor performed on a solid bed catalyst from particle-shaped catalyst is known in prior art. According to the invention, the residence time of a catalyst is increased by transporting working soluti on containing reaction support material and transporting a hydrogen-containing gas phase as a mixture from the downside to the upside through a hydrogenati on reactor. The empty pipe velocity of the working solution is 0.05 to 100 m/h, in particular 10 to 50 m/h.
-
公开(公告)号:ES2020543B3
公开(公告)日:1991-08-16
申请号:ES87116065
申请日:1987-10-31
Applicant: DEGUSSA
Inventor: WAGNER RUDOLF , STUMKE MANFRED , GROLL WERNER , SCHIWIORA HARRY
-
公开(公告)号:AU8220287A
公开(公告)日:1988-06-16
申请号:AU8220287
申请日:1987-12-08
Applicant: DEGUSSA
Inventor: WAGNER RUDOLF , SCHIWIORA HARRY , STUMKE MANFRED , GROLL WERNER
Abstract: Palladium alloys consisting of (a) 65 to 85% palladium, (b) 0 to 10% gold and/or 0 to 5% platinum, (c) 0.1 to 10% tin, (d) 1 to 10% gallium, (e) 1 to 12% copper, (f) 0.05 to 1.5% ruthenium and/or 0.05 to 0.7% rhenium as well as (g) 0.01 to 4% tungsten and/or 0.01 to 4% aluminum and/or 0.01 to 4% zinc are use to produce firmly seated and removable dentures. These alloys do not form oxide films when melted in air.
-
-
-
-
-
-
-
-
-