MICROFIBRILLATED FILM
    142.
    发明专利

    公开(公告)号:CA3028587A1

    公开(公告)日:2017-12-28

    申请号:CA3028587

    申请日:2017-06-20

    Applicant: STORA ENSO OYJ

    Abstract: The invention concerns a method of producing an MFC film comprising reinforcement fibers, which film show excellent oxygen barrier properties and is easy to handle. The method of manufacturing the film comprises the steps of: - providing a suspension comprising a first microfibrillated cellulose (MFC) in an amount of at least 50 weight %, reinforcement fibers in an amount of at least 5 weight %, all percentages calculated on the total solid content of said suspension, and a formation aid, - mixing said suspension to form a mixture, - forming a fibrous web from the mixture, and - dewatering and/or drying said fibrous web to form a film having a basis weight of less than 40 g/m2, a specific formation number of below 0.45 g0,5/m2, and an Oxygen Transmission Rate (OTR) value of below 100 ml/m2/per 24 hours, preferably of below 50 ml/m2per 24 hours at 50% relative humidity. The invention further discloses a film and use of the film in food or liquid packaging applications.

    Método para producir partículas electrostáticamente

    公开(公告)号:ES2613705T3

    公开(公告)日:2017-05-25

    申请号:ES09714946

    申请日:2009-02-26

    Applicant: STORA ENSO OYJ

    Abstract: Un método para formar partículas o gotas de al menos una sustancia que comprende las etapas de; i) proporcionar un medio espumado, comprendiendo dicho medio espumado dicha sustancia, y proporcionándose dicho medio espumado al dispersar un gas en un líquido o en un sólido, comprendiendo dicho líquido o sólido dicha sustancia, o proporcionándose dicho medio espumado al dispersar un gas en un líquido o en un sólido por lo cual se forma una dispersión de un gas en un líquido o sólido, tras lo cual al menos una sustancia se incorpora en dicha dispersión, en la que el gas se dispersa en el líquido o en el sólido en una cantidad de 50-99% en volumen del total del medio espumado; ii) formar partículas o gotas de nano-tamaño de dicha sustancia por electrohilado o electropulverización de dicho medio espumado.

    A METHOD FOR PRODUCING A FILM HAVING GOOD BARRIER PROPERTIES

    公开(公告)号:CA2995478A1

    公开(公告)日:2017-03-23

    申请号:CA2995478

    申请日:2016-09-16

    Applicant: STORA ENSO OYJ

    Abstract: The present invention relates to a method for manufacturing a film having an oxygen transmission rate in the range of from 1 cc/m2/24h to 500 cc/m2/24h according to ASTM D-3985, at a relative humidity of more than 50 % at 25°C, or higher than 75% at 25°C, or higher than 85% at 25°C, wherein the method comprises the steps of: providing a first suspension comprising a microfibrillated cellulose, wherein the dry content of the suspension is in the range of from 0.1 to 10% by weight, adding a wet strength additive to said first suspension, at an amount of from 0.1 to 10 weight-% based on the amount of microfibrillated cellulose (dry/dry), thereby forming a mixture of the microfibrillated cellulose and the wet strength additive, applying said mixture to a substrate to form a fibrous web and drying said web to form said film. The present invention also relates to a film produced according to the method.

    A METHOD TO PRODUCE A FILM COMPRISING MICROFIBRILLATED CELLULOSE AND AN AMPHOTERIC POLYMER

    公开(公告)号:CA2995437A1

    公开(公告)日:2017-03-23

    申请号:CA2995437

    申请日:2016-09-16

    Applicant: STORA ENSO OYJ

    Abstract: A method for the production of a film from a fibrous web, wherein the method comprises the steps of: providing a fibrous suspension comprising a microfibrillated cellulose, wherein the content of the microfibrillated cellulose of said suspension is in the range of 60 to 99.9 weight-% based on total dry solid content, adding an amphoteric polymer to said suspension to provide a mixture of said microfibrillated cellulose and said amphoteric polymer, providing said mixture to a substrate to form a fibrous web, wherein the amount of amphoteric polymer in said mixture is in the range of 0.1 to 20 kg/metric ton based on total dry solid content; and dewatering said fibrous web to form a film having a basis weight of less than 40 g/m2 and a density in the range of from 700 to 1000 kg/m3