公开(公告)号:KR1020130050789A
公开(公告)日:2013-05-16
申请号:KR1020110116033
申请日:2011-11-08
Applicant: 한국전자통신연구원
Inventor: 김기현
CPC classification number: B32B37/12 , B32B7/02 , B32B7/12 , B32B2307/202 , B32B2307/7244 , B32B2307/7265 , H01B5/14
Abstract: PURPOSE: A method of laminating a plastic plate for optoelectronic is provided to be effective in the stability and the reliability of an element device by forming penetration preventing film or conduction film and laminating several films to a plastic plate. CONSTITUTION: A method of laminating a plastic plate for optoelectronic comprises the following steps. A barrier layer for preventing moisture or oxide from penetrating or a conductive layer is prepared. The plastic plate is stuck with a bonding layer. The plastic plate is layered. The plastic plate for optoelectronic(100) comprises a barrier layer(300) comprised of an organic, inorganic or both mixed materials. To bond the barrier layer and the plastic plate, an adhesive material or an adhesive sheet which is an adhesive layer(200) is formed.
Abstract translation: 目的:提供一种层压光电子塑料板的方法,通过形成穿透防止膜或导电膜并将多个膜层压到塑料板上,有效地保持元件装置的稳定性和可靠性。 构成:层压光电子塑料板的方法包括以下步骤。 制备用于防止水分或氧化物渗透的阻挡层或导电层。 塑料板粘贴有粘合层。 塑料板是分层的。 用于光电(100)的塑料板包括由有机,无机或两种混合材料组成的阻挡层(300)。 为了粘合阻挡层和塑料板,形成作为粘合剂层(200)的粘合剂材料或粘合片。
-
公开(公告)号:KR1020130042730A
公开(公告)日:2013-04-29
申请号:KR1020110106782
申请日:2011-10-19
Applicant: 한국전자통신연구원
CPC classification number: G02B26/005 , G02B2207/115
Abstract: PURPOSE: An eletrowetting display is provided to secure the stability of driving by safely controlling the moving direction and speed of a non-polarized fluid without the patterning process of a thin film or additional surface processing through forming a part of the pixel separation wall of the electrowetting display with conducting materials. CONSTITUTION: An eletrowetting display comprises a first substrate part(201) formed at the viewing side of the display. The eletrowetting display comprises a second substrate part(203) formed at the rear side of the display. The eletrowetting display comprises a pixel separation wall(213) formed between the first and second substrates for separating pixel regions and a part of the separation wall is formed with conducting materials. The eletrowetting display comprises polar fluids(215) and nonpolar fluids(217) filling the pixel region separated by the pixel separation wall.
Abstract translation: 目的:提供电镀显示器,以通过安全地控制非极化流体的移动方向和速度来确保驱动的稳定性,而无需薄膜的图案化处理或附加的表面处理,通过形成一部分像素分隔壁 导电材料电润湿显示。 构成:电泳显示器包括形成在显示器的观看侧的第一衬底部分(201)。 电镀显示器包括形成在显示器后侧的第二基板部分(203)。 电镀显示器包括形成在第一和第二基板之间的用于分离像素区域的像素分离壁(213),并且一部分隔离壁由导电材料形成。 电喷显示器包括填充由像素分隔壁分隔的像素区域的极性流体(215)和非极性流体(217)。
-
公开(公告)号:KR1020120127037A
公开(公告)日:2012-11-21
申请号:KR1020110045251
申请日:2011-05-13
Applicant: 한국전자통신연구원
Inventor: 김기현
CPC classification number: G01N3/20 , G01M5/005 , G01N3/22 , G01M13/025 , G01M13/026
Abstract: PURPOSE: A bending test device of a flexible substrate is provided to fix one side and the other side of a flexible substrate having various sizes with first and second electrode units, thereby enhancing the reliability of a test. CONSTITUTION: A bending test device of a flexible substrate comprises a table(10), a first electrode unit(30), a guide rail(40), a slider, and a second electrode(60). The first electrode unit fixes one side of the flexible substrate on the table. The guide rail is arranged to be adjacent to the first electrode unit and extended from one side of the flexible substrate to the other side of the flexible substrate. The slider is moved along the guide rail. The second electrode unit is connected to the slider and makes the other side of the flexible substrate approach the first electrode or separate from the first electrode unit.
Abstract translation: 目的:提供柔性基板的弯曲试验装置,用第一和第二电极单元固定具有各种尺寸的柔性基板的一侧和另一侧,从而提高试验的可靠性。 构成:柔性基板的弯曲试验装置包括台(10),第一电极单元(30),导轨(40),滑块和第二电极(60)。 第一电极单元将柔性基板的一侧固定在工作台上。 导轨配置成与第一电极单元相邻并且从柔性基板的一侧延伸到柔性基板的另一侧。 滑块沿着导轨移动。 第二电极单元连接到滑块,使柔性基板的另一侧接近第一电极或与第一电极单元分开。
-
公开(公告)号:KR1020110029881A
公开(公告)日:2011-03-23
申请号:KR1020090087734
申请日:2009-09-16
Applicant: 한국전자통신연구원
IPC: C09D133/04 , C08J7/04 , C08K5/151 , C08K3/20
CPC classification number: C08J7/16 , Y10T428/269 , Y10T428/31511 , Y10T428/31855 , Y10T428/31935
Abstract: PURPOSE: Plastic substrates and a method for manufacturing the same are provided to improve the stability and the reliability of elements using the substrates by forming a protective film on the substrates in order to complement the chemical resistance and the stiffness of the substrates. CONSTITUTION: A method for manufacturing plastic substrates includes the following: Compositions containing reactive monomers for a protective film are applied to organic substrates. The reactive monomers are polymerized to form the protective film on the organic substrates. The reactive monomers are represented by one chemical formula selected from a group including a chemical formula 1 to a chemical formula 3.
Abstract translation: 目的:提供塑料基板及其制造方法,以通过在基板上形成保护膜来提高使用基板的元件的稳定性和可靠性,以补充基板的耐化学性和刚度。 构成:用于制造塑料基材的方法包括以下:将含有保护膜的反应性单体的组合物施加到有机基材上。 将反应性单体聚合以在有机基材上形成保护膜。 反应性单体由选自化学式3至化学式3的化学式的一种化学式表示。
-
公开(公告)号:KR1020100033097A
公开(公告)日:2010-03-29
申请号:KR1020080092088
申请日:2008-09-19
Applicant: 한국전자통신연구원
CPC classification number: H01B13/0026 , B82Y30/00 , C01B32/158 , H01B5/14
Abstract: PURPOSE: A transparent conductive thin film and the manufacturing method thereof are provided to secure low sheet resistance and transparency by spraying a carbon nanotube on a substrate without using chemical means. CONSTITUTION: A manufacturing method of a transparent conductive thin film comprises the following steps: forming a bonding layer(20) to attach a carbon nanotube on a release sheet; forming a carbon nano tube layer(30) through a pulverized body coating method on the bonding layer; separating the release sheet attached on the bonding layer and attaching the release sheet to a substrate; and coating a conductive polymer on the carbon nano tube layer.
Abstract translation: 目的:提供一种透明导电薄膜及其制造方法,以通过在基板上喷涂碳纳米管而不使用化学方法来确保低的薄层电阻和透明度。 构成:透明导电薄膜的制造方法包括以下步骤:形成粘合层(20)以将碳纳米管附着在剥离片上; 在所述接合层上通过粉体涂覆方法形成碳纳米管层(30); 分离附着在接合层上的剥离片并将剥离片附着到基材上; 并在碳纳米管层上涂覆导电聚合物。
-
公开(公告)号:KR100902845B1
公开(公告)日:2009-06-16
申请号:KR1020080115278
申请日:2008-11-19
Applicant: 한국전자통신연구원
IPC: G02F1/1333 , H01L27/12 , B32B27/00
Abstract: 플라스틱 기판 및 그 형성 방법이 제공된다. 상기 형성 방법은 유기성 기판 상에 무기물 및 유기물을 포함하는 혼합물을 도포하여 코팅막을 형성하는 단계를 포함한다. 상기 코팅막으로부터 무기물층 및 유기물층을 포함하는 보호막이 형성된다.
플라스틱 기판, 수분 및 산소 차단, 무기물, 유기물-
公开(公告)号:KR1020080108212A
公开(公告)日:2008-12-12
申请号:KR1020080116800
申请日:2008-11-24
Applicant: 한국전자통신연구원
IPC: H01L21/304 , B08B3/00 , G02F1/13
CPC classification number: G02F1/1313 , B08B11/04 , G02F2001/1316
Abstract: A cleaning solution of the flexible substrate is provided to increase the yield of the manufacturing process of the flexible device without the change of the mass production facility of the existing semiconductor and display device. A cleaning solution of the flexible substrate comprises the following steps: the step for putting the flexible substrate(21); the step for removing the foreign materials attached on both main surfaces of the flexible substrate by taking advantage of adhesion using the first roller(22) positioned at each main surfaces of the flexible substrate; the step for transcribing the foreign materials from the first roller to the second roller and removing the foreign materials. The second roller has the adhesion greater than the first roller. The step for removing the foreign materials and the step for transferring the foreign materials and removing are performed under the inert atmosphere or the vacuum atmosphere.
Abstract translation: 提供柔性基板的清洁溶液以增加柔性装置的制造过程的产量,而不改变现有的半导体和显示装置的批量生产设备。 柔性基板的清洗液包括以下步骤:将柔性基板(21)放置的步骤; 通过利用位于柔性基板的每个主表面处的第一辊(22)的粘合力来去除附着在柔性基板的两个主表面上的异物的步骤; 将异物从第一辊转印到第二辊并除去异物的步骤。 第二辊具有大于第一辊的粘合力。 在惰性气氛或真空气氛下进行除去异物的步骤和转移异物和除去步骤。
-
公开(公告)号:KR1020080052022A
公开(公告)日:2008-06-11
申请号:KR1020060123976
申请日:2006-12-07
Applicant: 한국전자통신연구원
IPC: G02F1/167
CPC classification number: G02F1/167 , G02F2202/01
Abstract: A display device of electrophoresis type and a manufacturing method thereof are provided to improve efficiency motion of an ink particle by inducing the ink particle. A display device of electrophoresis type includes a plurality of capsules(33), a first substrate(31), a second substrate(32), and a dielectric layer(37). The plurality of capsules includes fluidity liquid. The fluidity liquid makes a first particle(34) and a second particle(35) flow. The first and the second particle have different color. The plurality of capsules are operated by applied electrical field distinguishably. The first substrate and the second substrate are formed the upper side and the lower side of the capsule and includes an electrode respectively. The dielectric layer is formed on at least one of the first and the second substrate to contact to the capsule.
Abstract translation: 提供电泳型显示装置及其制造方法,以通过诱导墨水颗粒来改善墨水颗粒的效率运动。 电泳型显示装置包括多个胶囊(33),第一基板(31),第二基板(32)和电介质层(37)。 多个胶囊包括流动性液体。 流动性液体使第一颗粒(34)和第二颗粒(35)流动。 第一颗粒和第二颗粒具有不同的颜色。 多个胶囊通过施加的电场可区分地操作。 第一基板和第二基板形成为胶囊的上侧和下侧,分别包括电极。 介电层形成在第一和第二基板中的至少一个上,以与胶囊接触。
-
公开(公告)号:KR100820170B1
公开(公告)日:2008-04-10
申请号:KR1020060082746
申请日:2006-08-30
Applicant: 한국전자통신연구원
CPC classification number: H01L27/1266 , C09J5/00 , C09J2400/143 , C09J2400/226 , C09J2423/006 , C09J2467/006 , C09J2479/086 , G02F1/133305 , H01L27/1214 , H01L27/1218 , H01L29/78603 , Y10T156/10
Abstract: 본 발명은 플렉시블 기판의 적층 방법에 관한 것이다. 본 플렉시블 기판의 적층 방법은, 캐리어 기판을 준비하는 단계; 상기 캐리어 기판 상에 접착층을 적층하는 단계; 및 라미네이팅 방법 또는 압착 방법을 이용하여 상기 접착층 상에 적어도 하나의 화상 표시 소자가 형성되는 플렉시블 기판을 적층하는 단계를 포함한다. 이에 따라, 기존의 디스플레이 구현을 위한 양산 설비의 변형 없이 플렉시블 기판을 제조하는 것이 용이하며, 이러한 방법을 이용하여 플렉시블한 경박단소(輕薄短小)형의 플렉시블 디스플레이 장치에 이용할 수 있다.
플렉시블 기판, 라미네이팅, 압착, 접착층-
公开(公告)号:KR1020080020024A
公开(公告)日:2008-03-05
申请号:KR1020060082746
申请日:2006-08-30
Applicant: 한국전자통신연구원
CPC classification number: H01L27/1266 , C09J5/00 , C09J2400/143 , C09J2400/226 , C09J2423/006 , C09J2467/006 , C09J2479/086 , G02F1/133305 , H01L27/1214 , H01L27/1218 , H01L29/78603 , Y10T156/10
Abstract: A flexible substrate adhesion method is provided to alleviate the warp of a flexible substrate effectively by removing a stress caused by a difference in thermal coefficient between the flexible substrate and a carrier substrate. A flexible substrate adhesion method includes the steps of: preparing a carrier substrate(110); stacking an adhesive layer(120) on a carrier substrate; and stacking the flexible substrate on which at least one image display element is formed on the adhesive layer by using a laminating method or a pressing method. The laminating method uses a laminator including an upper roller(140a) rotating in the adhesive layer or in an upper part of the flexible substrate and a lower roller(140b) rotating in a lower part of the carrier substrate. The pressing method uses a press including an upper pressing unit formed in a top part of the flexible substrate and movable in a vertical direction, a fixation pressing unit formed in a lower part of the carrier substrate or lower pressing units movable in the vertical direction.
Abstract translation: 提供了一种柔性基板粘附方法,通过去除由柔性基板和载体基板之间的热系数差引起的应力,有效地减轻柔性基板的翘曲。 柔性基板粘合方法包括以下步骤:制备载体基板(110); 将粘合剂层(120)堆叠在载体基材上; 并且通过使用层叠方法或压制方法将其上形成有至少一个图像显示元件的柔性基板堆叠在粘合剂层上。 层压方法使用包括在粘合剂层中旋转的上辊(140a)或柔性基板的上部的层压机和在载体基板的下部旋转的下辊(140b)。 压制方法使用包括形成在柔性基板的顶部中并可沿垂直方向移动的上压制单元的压制机,形成在载体基板的下部中的定影按压单元或可沿垂直方向移动的下压装置。
-
-
-
-
-
-
-
-
-