에탄올로부터 1,3-부타디엔 제조를 위한 규칙적인 메조세공 실리카계 촉매 및 이를 이용한 1,3-부타디엔의 제조방법
    161.
    发明公开
    에탄올로부터 1,3-부타디엔 제조를 위한 규칙적인 메조세공 실리카계 촉매 및 이를 이용한 1,3-부타디엔의 제조방법 有权
    用于生产1,3-丁二烯的订购的基于二氧化硅的催化剂及其使用的1,3-丁二烯的生产方法

    公开(公告)号:KR1020140050531A

    公开(公告)日:2014-04-29

    申请号:KR1020130107236

    申请日:2013-09-06

    CPC classification number: C07C1/20 Y02P20/584 C07C11/167

    Abstract: The present invention relates to a catalyst for preparing 1,3-butadiene in which a transition metal compound is supported on regular mesoporous silica, and a method for preparing 1,3-butadiene using the same. Specifically, the catalyst of the present invention can improve selectivity by optimizing the type and characteristics of the silica and specifying the type and content of a transition metal oxide; can increase the yield of 1,3-butadiene by highly dispersed active sites due to a high surface area; and facilitates a diffusion of a reactant and a product and the transfer of materials by having a regular mesoporous structure. In addition, since all of the active sites are not concentrated so as to be able to equally and uniformly participate in a reaction, the deterioration of activity is inhibited compared with a conventional silica catalyst in which micropores and mesopores coexist, thereby remarkably improving the lifetime of the catalyst compared with a conventional silica-based catalyst, and thus process operation efficiency can be improved due to a longer recycling period. Therefore, the catalyst of the present invention can be useful for preparing the 1,3-butadiene. [Reference numerals] (AA) Example 1; (BB) Example 2; (CC) Example 3; (DD) Example 4; (EE) Example 5; (FF) Example 6; (GG) Example 7; (HH) Example 8; (II) Example 9; (JJ) Example 10; (KK) Comparative example 1; (LL) Comparative example 2; (MM) Comparative example 3

    Abstract translation: 本发明涉及一种用于制备1,3-丁二烯的催化剂,其中过渡金属化合物负载在常规介孔二氧化硅上,以及使用其制备1,3-丁二烯的方法。 具体地说,本发明的催化剂可以通过优化二氧化硅的类型和特性并确定过渡金属氧化物的类型和含量来提高选择性; 可以通过高分散的活性位点由于高表面积而增加1,3-丁二烯的产率; 并且通过具有规则的介孔结构促进反应物和产物的扩散和材料的转移。 此外,由于所有的活性部位都不能浓缩以能够均匀地均匀地参与反应,与微孔和介孔共存的常规二氧化硅催化剂相比,活性的劣化被抑制,从而显着地提高了寿命 的催化剂,与常规的二氧化硅基催化剂相比,由于更长的回收期,可以提高工艺运行效率。 因此,本发明的催化剂可用于制备1,3-丁二烯。 (标号)(AA)实施例1; (BB)实施例2; (CC)实施例3; (DD)实施例4 (EE)实施例5; (FF)实施例6; (GG)实施例7 (HH)实施例8; (II)实施例9 (JJ)实施例10 (KK)比较例1; (LL)比较例2; (MM)比较例3

    고강도를 갖는 SAPO-34 미소구형체 촉매, 이의 제조방법 및 이를 이용한 경질올레핀의 제조방법
    163.
    发明授权
    고강도를 갖는 SAPO-34 미소구형체 촉매, 이의 제조방법 및 이를 이용한 경질올레핀의 제조방법 有权
    具有高性能和机械强度的微球硅铝磷酸-34催化剂,其制备方法和使用该轻质烯烃的制备方法

    公开(公告)号:KR101193973B1

    公开(公告)日:2012-10-24

    申请号:KR1020090100597

    申请日:2009-10-22

    Abstract: 본 발명은 고강도를 갖는 SAPO-34(silicoaluminophosphate-34) 미소구형체 촉매, 이의 제조방법 및 이를 이용한 경질올레핀의 제조방법에 관한 것으로서, 이를 더욱 자세하게 설명을 하면, 본 발명은 테트라에틸암모늄 하이드록사이드(TEAOH, Tetraethylammonium hydroxide) 등의 다양한 유기주형체를 단독 또는 혼합 사용하여 수열합성법으로 제조된 SAPO-34 슬러리에 매트릭스, 바인더 및 첨가제 등을 포함하는 혼합 슬러리를 분무건조시켜서 미소구형체를 제조한 후, 이를 소성하여 SAPO-34 미소구형체 촉매를 제조하는 방법 및 상기 제조방법으로 제조한 순환유동층 반응기용 SAPO-34 미소구형체 촉매에 관한 것이다. 본 발명의 상기 SAPO-34 미소구형체 촉매는 높은 강도를 가지면서도 반응활성이 우수하기 때문에, 촉매의 높은 강도를 요구하는 순환 유동층 반응기에 사용하기에 적합하다. 또한, 상기 SAPO-34 미소구형체 촉매는 고수명을 갖을 뿐만 아니라, C
    1 ~ C
    4 의 함산소화합물(oxygenates)의 전환율이 우수하기 때문에 에틸렌, 프로필렌, 부텐 등의 경질올레핀 제조에 사용하기에 적합하다.
    메탄올, 경질올레핀, SAPO-34, 분무건조, 미소구형체

    킬레이트된 전이 금속을 이용한 선택산화탈황용 촉매의 제조 방법
    165.
    发明公开
    킬레이트된 전이 금속을 이용한 선택산화탈황용 촉매의 제조 방법 有权
    使用电镀过渡金属生产选择性氧化脱硫催化剂的方法

    公开(公告)号:KR1020120040614A

    公开(公告)日:2012-04-27

    申请号:KR1020100102130

    申请日:2010-10-19

    Abstract: PURPOSE: A method for manufacturing catalyst for selective oxidative desulfurization using chelated transition metal is provided to expand the life of the catalyst and to improve the activity of the catalyst. CONSTITUTION: A method for manufacturing catalyst for selective oxidative desulfurization using chelated transition metal includes the following: a transition metal precursor and a chelate formulation are introduced into an organic solvent to be reacted in a first process. A support is introduced into an aqueous solution to be mixed in a second process. Resultant from the first and the second processes are mixed and stirred in a third process. The product from the third process is dried and plasticized in a forth process.

    Abstract translation: 目的:提供一种使用螯合过渡金属制备选择性氧化脱硫催化剂的方法,以延长催化剂的使用寿命并提高催化剂的活性。 构成:使用螯合过渡金属制备用于选择性氧化脱硫的催化剂的方法包括:将过渡金属前体和螯合剂制剂引入有机溶剂中以在第一种方法中反应。 在第二种方法中将载体引入待混合的水溶液中。 从第一和第二过程产生的混合并在第三个过程中搅拌。 来自第三种方法的产品在第四种方法中被干燥和塑化。

    디벤조티오펜설폰으로부터 비페닐의 제조방법
    168.
    发明公开
    디벤조티오펜설폰으로부터 비페닐의 제조방법 失效
    二苯并噻吩硫酮制备二苯乙烯的方法

    公开(公告)号:KR1020090131047A

    公开(公告)日:2009-12-28

    申请号:KR1020080056822

    申请日:2008-06-17

    Abstract: PURPOSE: A process for manufacturing biphenyl from dibenzothiophene sulfone is provided to improve a conversion ratio of dibenzothiophene sulfone and to prepare biphenyl at a high yield. CONSTITUTION: A process for manufacturing biphenyl from dibenzothiophene sulfone comprises a step for preparing biphenyl by removing sulfur dioxide from dibenzothiophene sulfone in the presence of a magnesium-containing mesoporous molecular sieve catalyst. The magnesium-containing mesoporous molecular sieve catalyst is MCM-41 containing magnesium. The magnesium-containing mesoporous molecular sieve catalyst includes 20~40 weight% magnesium.

    Abstract translation: 目的:提供二苯并噻吩砜制备联苯的方法,以提高二苯并噻吩砜的转化率,并以高产率制备联苯。 构成:从二苯并噻吩砜制造联苯的方法包括在含镁介孔分子筛催化剂存在下从二苯并噻吩砜中除去二氧化硫制备联苯的步骤。 含镁介孔分子筛催化剂是含镁的MCM-41。 含镁介孔分子筛催化剂含有20〜40重量%的镁。

    원유의 수소화 분해용 촉매 및 이를 이용한 수소화 분해방법
    169.
    发明授权
    원유의 수소화 분해용 촉매 및 이를 이용한 수소화 분해방법 有权
    원유의수소화분해용촉매및이를이용한수소화분해방

    公开(公告)号:KR100931036B1

    公开(公告)日:2009-12-10

    申请号:KR1020080025040

    申请日:2008-03-18

    Abstract: PURPOSE: A catalyst for hydrocracking crude oil and a method for hydrocracking using the same are provided to reduce energy and processing cost with environment-friendly effects by performing a hydrocracking process in a low temperature and a low pressure conditions. CONSTITUTION: A catalyst for hydrocracking crude oil is the catalyst of a foam shape in which a reactive metal is dipped in a porous carrier. The catalyst for hydrocracking the crude oil has the total pore volume of 0.5 ~ 2.5 cc/g. The catalyst includes an air bubble surface area of 100 ~ 300 m^2/g. The thickness of pore wall of the catalyst is 5 ~ 100 nm. A pore diameter of the catalyst is 30 ~ 500 nm.

    Abstract translation: 目的:通过在低温和低压条件下进行加氢裂化过程,提供一种加氢裂化原油的催化剂和使用该催化剂的加氢裂化方法,以降低能量和加工成本,并具有环境友好的效果。 组成:用于加氢裂化原油的催化剂是泡沫形状的催化剂,其中活性金属浸渍在多孔载体中。 用于加氢裂化原油的催化剂的总孔体积为0.5〜2.5cc / g。 该催化剂的气泡表面积为100〜300平方公尺/ g。 催化剂的孔壁厚度为5〜100nm。 催化剂的孔径为30〜500nm。