Abstract: PURPOSE: A continuously reinforced concrete pavement method using reinforcing bar guiding/fixing equipment is provided to automatically arrange longitudinal reinforcing bars on regular positions without lateral auxiliary reinforcing bars, thereby minimizing the amount of reinforcing bars and workloads and improving the construction speed. CONSTITUTION: A continuously reinforced concrete pavement method using reinforcing bar guiding/fixing equipment(100) includes: a step of driving and moving the reinforcing bar guiding/fixing equipment with guide tubes and reinforcing bar holding devices in order to longitudinally arrange the reinforcing bars on regular positions; a step of placing concrete on the upper side of the arranged reinforcing bars; and a step of finishing the placed concrete to be flattened with a paver(300). [Reference numerals] (AA) Driving direction
Abstract translation: 目的:使用钢筋导向/固定设备的连续钢筋混凝土路面方法,将纵向钢筋自动布置在常规位置上,无需侧向辅助钢筋,从而最大限度地减少钢筋数量和工作量,提高施工速度。 构成:使用钢筋引导/固定设备(100)的连续钢筋混凝土路面方法包括:用引导管和钢筋保持装置驱动和移动钢筋导向/固定设备的步骤,以便将钢筋纵向布置在 常规职位 将混凝土放置在布置的钢筋的上侧的步骤; 并且用摊铺机(300)整理待铺设的混凝土的步骤。 (标号)(AA)行驶方向
-
公开(公告)号:KR1020100136162A
公开(公告)日:2010-12-28
申请号:KR1020090054381
申请日:2009-06-18
Applicant: 강원대학교산학협력단 , (주)삼우아이엠씨
IPC: C04B24/04 , C04B14/04 , C04B103/30
Abstract: PURPOSE: A high early-strength concrete composition is provided to improve excellent early strength and water penetrability resistance by adding silica fume to 2 kinds of excellent properties. CONSTITUTION: A high early-strength concrete composition comprises silica fume 3-10 weight%(based on unit aggregate), polycarbonic acid-based water-reducing agent 0.01-1.5 weight% (based on unit volume of binder), and naphthalene-based water-reducing agent 0.01-1.5 weight%. The high early-strength concrete composition comprises fly ash.
Abstract translation: 目的:提供高的早强混凝土组合物,通过添加二氧化硅烟雾具有优异的性能,提高优异的早期强度和防水渗透性。 构成:高的早强混凝土组合物包含3-10重量%(基于单元骨料)的硅粉,0.01-1.5重量%的聚碳酸基减水剂(基于粘合剂的单位体积)和萘系 减水剂0.01-1.5重量%。 早期强度高的混凝土组成包括飞灰。
-
公开(公告)号:KR1020100109677A
公开(公告)日:2010-10-11
申请号:KR1020090028051
申请日:2009-04-01
Applicant: 강원대학교산학협력단 , 한국건설기술연구원 , (주)삼우아이엠씨
IPC: C04B18/08 , C04B24/04 , C04B28/04 , C04B103/30
CPC classification number: Y02W30/92 , C04B18/08 , C04B28/02 , C04B2103/302 , C04B2111/00068 , C04B2111/0075 , C04B2201/05
Abstract: PURPOSE: A concrete composition for road pavement repairing is provided to reduce the water-cement rate by inserting an early-strength type water reducing agent and ultrafine fly ash. CONSTITUTION: A concrete composition for road pavement repairing for an early traffic opening contains 10~20wt% of ultrafine fly ash and 0.5~1wt% of early-strength type water reducing agent for 312~420kg of quick-setting cement. The ultrafine fly ash includes more than 6,000 grains of particles. The early-strength type water reducing agent includes a polycarboxylic acid based water reducing agent. The water-cement rate of the composition is 36~41wt%.
Abstract translation: 目的:通过插入早强型减水剂和超细粉煤灰,提供道路修补的混凝土组合物,以降低水泥率。 构成:早期交通开放路面修复的具体构成包含超细粉煤灰10〜20wt%,早强型减水剂0.5〜1wt%,速凝水泥312〜420kg。 超细粉煤灰包含6,000多颗颗粒。 早强型减水剂包括基于多元羧酸的减水剂。 组合物的水泥率为36〜41wt%。
-
公开(公告)号:KR100774448B1
公开(公告)日:2007-11-08
申请号:KR1020060056461
申请日:2006-06-22
Applicant: (주)삼우아이엠씨 , 대상이앤씨(주) , 강원대학교산학협력단
CPC classification number: C04B28/02 , C04B2111/0075 , C04B2111/72 , C04B18/02 , C04B20/0076 , C04B24/2611 , C04B32/02 , C04B2103/50
Abstract: A latex-modified concrete composition using high strength cement is provided to be more inexpensive than a very early strength-latex modified concrete and help accomplish a relatively early traffic opening by a rapid completion of a construction work. A latex-modified concrete composition using high strength cement is used for a work for repairing broken portions of paving and comprises cement, coarse aggregate, and water. Latex is added to the concrete formed by high strength cement. A content of the latex is 10-15wt% based on the cement. The coarse aggregate in the concrete has a maximal dimension of 13-25mm. A ratio of the water-cement in the concrete is 29-35wt.%. An anti-foaming agent is added in a 0.3-0.6wt.% of amount.