Abstract:
본 발명은 나노 금속 촉매가 포함된 펌제용 산화성 조성물에 관한 것으로서, 더욱 상세하게는 나노 크기로 조절된 전이 금속과 인산을 반응시켜 제조한 산화촉매를 펌제용 산화성 조성물에 적용함으로써 산화성 조성물이 모발에 적용시 모발내 시스틴 결합의 환원과 산화에 대한 산화 반응의 활성 조절이 가능하여 기존의 펌제용 산화성 조성물을 사용한 것보다 모발의 웨이브 형성율을 크게 향상시킬 수 있는 효과를 나타내는 개선된 펌제용 산화성 조성물에 관한 것이다. 나노, 촉매, 산화반응, 웨이브제, 산화촉매
Abstract:
An oxidative composition comprising a nano metal catalyst for permanent wave is provided to enhance permanent wave formation rate of hair, inhibit hair damage by controlling reduction and oxidation speed of hair, and enhance hair health by increasing tension of hair. An oxidative composition for permanent wave comprises 0.001-5 wt.% of a nano transition metal catalyst having colloid phase with diameter of 1-100 nm and 0.0001-5 wt.% of a phosphoric acid co-catalyst, wherein the transition metal catalyst is zinc or cobalt and is prepared by (1) mixing a transition metal precursor with pure water, adding a reactive material into the mixture and dispersing it with agitation, (2) adding a reducing agent into the dispersion, cooling the solution to 25-30 deg.C and maturing it, and (3) adding an aqueous dispersant into the matured solution to stabilize it. The phosphoric acid is selected from the phosphoric acid and alkali metal salt of phosphoric acid such as sodium phosphate, potassium phosphate, sodium hydrogen phosphate, potassium hydrogen phosphate, sodium dihydrogen phosphate or potassium dihydrogen phosphate.
Abstract:
Provided is a self-molding hair modifier having self-molding effect, thereby capable of significantly improving the hair molding manner which uses equipment such as a conventional perm rod or a rubber band. The self-molding hair modifier comprises: a reduction composition including 1-25 wt.% of a reducing agent having a pH of 4-11, 0.5-10 wt.% of a metallic element having a valence of 2, and 0.01-10 wt.% of a softener selected from the group consisting of an inorganic acid, an organic acid, an addition salt thereof, and mineral; a molding composition which includes 0.1-25 wt.% of a sugar compound selected from the group consisting of arginine, carrageenan and a sugar derivative thereof and binds to the metallic element having a valence of 2 to induce the mold; and an oxidizing composition including 0.1-25 wt.% of an oxidizing agent.
Abstract:
A self-molding permanent agent having improved storage stability is provided to perform shaping to the desired hair without hair-shaping apparatus due to self-molding properties, and inhibit deterioration of the permanent agent by preventing phase separation through addition of locust bean gum as a stabilizer. The self-molding permanent agent having improved storage stability comprises (a) a reducing composition containing a reducing agent and a sugar compound selected from algine, carrageenan and sugar derivatives thereof, (b) a molding composition containing a divalent metal element capable of inducing molding by combining with the sugar compound, and inducing molding by combining with the divalent metal element, and (c) a softening composition containing a softening agent selected from inorganic acid, organic acid and acid salt thereof, and mineral, and dissociating the combination of sugar compound with divalent metal element, and further comprises locust bean gum as a stabilizer.
Abstract:
An improved self-molding hair modifier is provided to improve curl rigidity of modified hair, supply nutrients to the hair, make the desired shape of hair after removing hair-modifier, recover the excessively contracted hair and enhance convenience of curling process by eliminating continuous application of perm rod or band. The improved self-molding hair modifier comprises (a) a reducing composition containing a reducing agent and a divalent metal element, (b) a molding composition containing a sugar compound selected from algine, carrageenan and sugar derivatives thereof, and inducing molding by combining with the divalent metal element, and (c) a softening composition containing a softening agent selected from inorganic acid, organic acid and acid salt thereof, and mineral, and dissociating the combination of sugar compound and divalent metal element.
Abstract:
본 발명은 탈-롯드 및 탈-밴드형 퍼머방법에 관한 것으로서, 더욱 상세하게는 모발의 시스틴 내의 디설파이드 결합을 환원시키기 위해 사용하는 환원제와 스스로 조형화되어 모발을 고정화시키는 특성을 가지는 조형촉진제를 함유하는 환원 조성물(a)과, 상기 조형촉진제와 결합하여 조형화를 유도하는 조형화 조성물(b), 그리고, 상기 조형촉진제의 조형화를 해제시키는 연화 조성물(c)을 포함하여 이루어진 퍼머제가, 자체적으로 조형화되는 특성이 부여되어 모발 성형기구를 제거한 상태에서도 의도하는 대로 모발을 단시간에 성형할 수 있으므로 펌용 롯드(perm rod)나 고무밴드 등의 성형기구를 착용한 상태에서 모발성형을 수행하던 기존의 퍼머방법을 탈피할 수 있는 탈-롯드 및 탈-밴드형 퍼머방법에 관한 것이다. 탈-롯드, 자가조형, 조형촉진제, 2가 금속원소, 환원 조성물, 조형화 조성물, 연화 조성물
Abstract:
본 발명은 산화반응용 혼합산화물 촉매 및 이의 제조방법에 관한 것으로서, 더욱 상세하게는 서로 다른 조성 및 제조방법에 의해 제조된 피조절상( controlled phase)과 조절상(controlling phase)으로 이루어져 있고, 상기 피조절상의 외표면을 조절상이 둘러싸고 있으나, 불연속면인 조절상의 틈으로 피조절상의 일부가 노출된 불연속적 이중구조로 이루어져 있어서 피조절상과 조절상 간의 전자이동이 원활하게 진행되어 서로간의 상승효과를 증가시킬 수 있으며, 피조절상과 조절상 간의 원격조정이 가능하고, 올레핀이나 파라핀 등의 가암모니아 산화반응에 의한 니트릴화합물의 제조시 촉매로 사용되어 생산성 향상, 부산물 최소화 등 친환경적인 우수한 활성을 가지는 산화반응용 혼합산화물 촉매 및 이의 제조방법에 관한 것이다. 피조절상, 조절상, 가암모니아 산화반응, 혼합산화물 촉매
Abstract:
본 발명은 산화반응용 혼합산화물 촉매 및 이의 제조방법에 관한 것으로서, 더욱 상세하게는 서로 다른 조성 및 제조방법에 의해 제조된 피조절상( controlled phase)과 조절상(controlling phase)으로 이루어져 있고, 상기 피조절상의 외표면을 조절상이 둘러싸고 있으나, 불연속면인 조절상의 틈으로 피조절상의 일부가 노출된 불연속적 이중구조로 이루어져 있어서 피조절상과 조절상 간의 전자이동이 원활하게 진행되어 서로간의 상승효과를 증가시킬 수 있으며, 피조절상과 조절상 간의 원격조정이 가능하고, 올레핀이나 파라핀 등의 가암모니아 산화반응에 의한 니트릴화합물의 제조시 촉매로 사용되어 생산성 향상, 부산물 최소화 등 친환경적인 우수한 활성을 가지는 산화반응용 혼합산화물 촉매 및 이의 제조방법에 관한 것이다.