파우더 슬러쉬 몰딩 공정용 마이크로 펠릿형 열가소성 폴리우레탄 조성물 및 그 제조방법
    13.
    发明公开
    파우더 슬러쉬 몰딩 공정용 마이크로 펠릿형 열가소성 폴리우레탄 조성물 및 그 제조방법 有权
    微粉型热塑性聚氨酯弹性体组合物,用于粉末成型工艺及其制备方法

    公开(公告)号:KR1020120049074A

    公开(公告)日:2012-05-16

    申请号:KR1020100110653

    申请日:2010-11-08

    Abstract: PURPOSE: A micro pellet type thermoplastic polyurethane composition for powder slush molding process and a manufacturing method thereof are provided to enhance mechanical property, light-proof, heat resistance, anti-hydrolysis property, and releasability. CONSTITUTION: A micro pellet type thermoplastic polyurethane composition for powder slush molding process comprises 5-10 weight% of ester-based polyol, 5-10 weight% of ether based polyol, 30-70 weight% of polycarbonate diol, 10-50 weight% of isocyanate, 5-30 weight% of chain extender, and 0.1-5 weight% of light-resistant stabilizer. The ester based polyol is more than one kind which is selected from polycaprolactone polyol, butylene adipate, ethylene adipate, and diethylene diadipate. The ether based polyol is polypropylene glycol, polytetramethylene ether glycol, or a mixture thereof.

    Abstract translation: 目的:提供用于粉末搪塑成型的微丸型热塑性聚氨酯组合物及其制造方法,以提高机械性能,耐光性,耐热性,抗水解性和脱模性。 构成:用于粉末搪塑成型的微丸型热塑性聚氨酯组合物包含5-10重量%的酯基多元醇,5-10重量%的醚基多元醇,30-70重量%的聚碳酸酯二醇,10-50重量% 的异氰酸酯,5-30重量%的增链剂和0.1-5重量%的耐光稳定剂。 酯基多元醇是选自聚己内酯多元醇,己二酸丁二醇酯,己二酸亚乙酯和二亚乙基二亚乙基酯中的一种以上。 醚类多元醇是聚丙二醇,聚四亚甲基醚二醇或其混合物。

    TPO 시트 조성물, TPO 시트 및 이를 포함하는 자동차 내장재
    14.
    发明公开
    TPO 시트 조성물, TPO 시트 및 이를 포함하는 자동차 내장재 无效
    TPO板材组合物,TPO板材和车厢内部TRIM

    公开(公告)号:KR1020110020039A

    公开(公告)日:2011-03-02

    申请号:KR1020090077713

    申请日:2009-08-21

    Abstract: PURPOSE: A TPO sheet composition is provided to ensure excellent bondability with an aqueous coating agent such as an aqueous primer and a surface treating agent and to enable the manufacture of automobile interiors with excellent properties through female vacuum molding. CONSTITUTION: A TPO sheet composition comprises 35~45 weight% of partially crosslinked thermoplastic olefin resin, 5~15 weight% of non-crosslinked thermoplastic olefin resin, 10~20 weight% of polypropylene resin, 10~20 weight% of ethylene octene rubber, 10~20 weight% of linear low-density polyethylene resin and 5~10 weight% of inorganic filler. The partially crosslinked thermoplastic olefin resin has a hardness of Shore A 65.

    Abstract translation: 目的:提供TPO片材组合物以确保与水性底漆和表面处理剂等水性涂料的极好的粘合性,并且能够通过母体真空成型制造具有优异性能的汽车内饰件。 构成:TPO片组合物包含35〜45重量%的部分交联的热塑性烯烃树脂,5〜15重量%的非交联热塑性烯烃树脂,10〜20重量%的聚丙烯树脂,10〜20重量%的乙烯 - 辛烯橡胶 ,10〜20重量%的线性低密度聚乙烯树脂和5〜10重量%的无机填料。 部分交联的热塑性烯烃树脂具有肖氏A65的硬度。

    수성코팅용 열가소성 폴리올레핀계 엘라스토머 시트 조성물
    15.
    发明公开
    수성코팅용 열가소성 폴리올레핀계 엘라스토머 시트 조성물 有权
    用于水基涂层处理的热塑性聚烯烃弹性体片材组合物

    公开(公告)号:KR1020080090216A

    公开(公告)日:2008-10-08

    申请号:KR1020070033460

    申请日:2007-04-04

    Abstract: A thermoplastic polyolefin-based elastomer sheet composition for water-based coating is provided to realize excellent mechanical properties including elongation, heat resistance and moldability, and moisture- and chemical resistance. A thermoplastic polyolefin-based elastomer sheet composition for water-based coating comprises: (a) 40-45 wt% of partially crosslinked thermoplastic polyolefin-based elastomer resin; (b) 5-10 wt% of non-crosslinked thermoplastic polyolefin-based elastomer resin; (c) 15-20 wt% of a polypropylene resin; (d) 15-20 wt% of an ethylene octene rubber resin; (e) 2-5 wt% of a linear low density polyethylene resin having a specific gravity of 0.92-0.94; (f) 10-15 wt% of a polyethylene master batch containing 2-3 wt% of a lubricant; and (g) 4-5 wt% of an inorganic filler.

    Abstract translation: 提供了一种用于水性涂料的热塑性聚烯烃基弹性体片组合物,以实现优异的机械性能,包括伸长率,耐热性和成型性,以及耐湿和耐化学性。 用于水性涂料的热塑性聚烯烃基弹性体片组合物包括:(a)40-45重量%的部分交联的热塑性聚烯烃基弹性体树脂; (b)5-10重量%的非交联热塑性聚烯烃基弹性体树脂; (c)15-20重量%的聚丙烯树脂; (d)15-20重量%的乙烯辛烯橡胶树脂; (e)2-5重量%的比重为0.92-0.94的线性低密度聚乙烯树脂; (f)10-15重量%的含有2-3重量%润滑剂的聚乙烯母料; 和(g)4-5重量%的无机填料。

    폴리프로필렌 수지 조성물
    16.
    发明授权
    폴리프로필렌 수지 조성물 有权
    聚丙烯的树脂组合物

    公开(公告)号:KR100811922B1

    公开(公告)日:2008-03-10

    申请号:KR1020070015039

    申请日:2007-02-13

    Abstract: A polypropylene resin composition is provided to improve melt tension, fluidity and cooling velocity, to prevent the generation of swirl mark in case of injection molding and to enhance the foaming rate and impact resistance of foamed product. A polypropylene resin composition comprises 5-20 wt% of a polypropylene master batch which comprises a propylene homopolymer, a propylene-ethylene copolymer or their mixture; 35-60 wt% of a high crystalline polypropylene resin having a melt index of 60-100 g/10 min (230 deg.C) and an isotacticity of 99-100; 5-15 wt% of an ethylene-styrene copolymer rubber which contains 20-50 wt% of styrene and has a polydispersity index of 8-12 and a melt index of 10-30 g/10 min (230 deg.C); 5-15 wt% of an ethylene-alpha-olefin copolymer rubber; and an inorganic filler.

    Abstract translation: 提供聚丙烯树脂组合物以改善熔体张力,流动性和冷却速度,以防止在注射成型的情况下产生旋转痕迹,并提高发泡产品的起泡速率和抗冲击性。 聚丙烯树脂组合物包含5-20重量%的聚丙烯母料,其包含丙烯均聚物,丙烯 - 乙烯共聚物或它们的混合物; 35-60重量%的熔融指数为60-100克/ 10分钟(230℃)和等规度为99-100的高结晶聚丙烯树脂; 5-15重量%的乙烯 - 苯乙烯共聚物橡胶,其含有20-50重量%的苯乙烯,多分散指数为8-12,熔体指数为10-30克/ 10分钟(230℃); 5-15重量%的乙烯-α-烯烃共聚物橡胶; 和无机填料。

    자동차 내장재 표피재용 폴리프로필렌계 수지 조성물
    17.
    发明授权
    자동차 내장재 표피재용 폴리프로필렌계 수지 조성물 有权
    一种汽车内饰材料用聚丙烯树脂组合物

    公开(公告)号:KR100551787B1

    公开(公告)日:2006-02-13

    申请号:KR1020040047800

    申请日:2004-06-24

    Abstract: 본 발명은 자동차 내장재 표피재용 폴리프로필렌계 수지 조성물에 관한 것으로, 더욱 상세하게는 폴리프로필렌계 공중합체, 에틸렌-옥텐 고무와 에틸렌-α-올레핀 공중합체 고무에 가공유(Process Oil) 및 폴리프로필렌 왁스를 적정 함량으로 마스터 배치화하여 고무류의 함량이 높음에도 불구하고 고무 성분의 가교없이 사출 성형성이 우수할 뿐만 아니라 저온 충격성, 내열성이 우수하고 냄새가 없는 자동차 내장재 인스트루먼트 판넬(Instrument Panel, 이하 인판넬) 표피재, 도어트림 표피재 또는 필라류 표피재로 이용 가능한 폴리프로필렌계 수지 조성물에 관한 것이다.
    폴리프로필렌계 공중합체, 에틸렌-α-올레핀 공중합체 고무, 폴리프로필렌 왁스, 사출 성형, 자동차 내장 표피재