Abstract:
A terpolymer compositions comprising: A) From 80 wt% to 97 wt%; of a propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt% to 3.2 wt%; ii) the content of 1-butene derived units ranging from 7.2 wt% to 14.8 wt% B) From 20 wt% to 3 wt%; of a propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt% to 3.2 wt%; ii) the content of 1-butene derived units ranging from 14.4 wt% to 26.5 wt%; and the terpolymer composition has the melt flow rate, MFR, measured according to ISO 1133 at 230 °C with a load of 2.16 kg, ranging from 3.0 g/10 min to 20.0 g/10 min; the sum of the amounts of A) and B) being 100 wt%.
Abstract:
A propylene ethylene copolymer having: i) xylene soluble fraction at 25 °C ranging from 14 wt% to 27 wt% ii) intrinsic viscosity of the fraction soluble in xylene at 25°C ranging from 1.0 to 2.4 dl/g; iii) melt flow rate, MFR, ranging from 1.0 g/10 min to 50.0 g/10 min; iv) an ethylene derived units content ranging from 5.0 wt% to 12.0 wt% v) the ethylene derived units content on the fraction insoluble in xylene at 25 °C ranging from 2.5 wt% to 6.0 wt%; vi) the ethylene derived units content on the fraction soluble in xylene at 25 °C ranging from 15.2. wt% to 30.2 wt% vii) the C13 NMR sequences PEP measured on the fraction insoluble in xylene at 25°C ranging from 3.5mol% to 5.5mol% and the C13 NMR sequences PEP measured on the fraction soluble in xylene at 25°C ranging from 11.0 mol% to 14.2 mol%.
Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25 °C, higher than 90 %, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 47 to 90 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 40% to 34.5% extremes included of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 3 and 5 dl/g.
Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25 °C, higher than 90 %, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 47 to 90 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 40% to 34.5% extremes included of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 3 and 5 dl/g.
Abstract:
The present disclosure relates to propylene-ethylene copolymers comprising an ethylene content of 0.1-10% by weight, a molecular weight distribution (MWD), expressed in terms of Mw/Mn, of greater than 3.0 and a xylene soluble (XS) fraction content defined by values that fall below the line given by the equation XS=1.0296·e0.435C2. The propylene-ethylene copolymers advantageously exhibit high transparency and low melting temperatures.