Abstract:
A propylene 1-hexene copolymer containing from 5.7 to 7.7% by weight, of 1-hexene derived units having: a) solubility in xylene at 25° C ranging from 7.0 wt% to 15.0 wt%; b) the melting temperature, measured by DSC ranging from 143.0 °C to 148.0° C; c) Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, from 3.5 to 8.0 g/10 min. d) content of 1-hexene derived units in the fraction soluble in xylene at 25°C ranging from 13.5 wt% to 18.5 wt%
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: - molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; - the creep and recovery curve measured on the polymer fuse at 200°C measured accordingto the procedure reported in the characterizing section shows a maximum value between 600 and 200 seconds lower than 53x10 -4 1/Pa.
Abstract:
A terpolymer compositions comprising: A) From 80 wt% to 97 wt%; of a propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt% to 3.2 wt%; ii) the content of 1-butene derived units ranging from 7.2 wt% to 14.8 wt% B) From 20 wt% to 3 wt%; of a propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt% to 3.2 wt%; ii) the content of 1-butene derived units ranging from 14.4 wt% to 26.5 wt%; and the terpolymer composition has the melt flow rate, MFR, measured according to ISO 1133 at 230 °C with a load of 2.16 kg, ranging from 3.0 g/10 min to 20.0 g/10 min; the sum of the amounts of A) and B) being 100 wt%.
Abstract:
Polypropylene composition comprising: A) from 50 wt% to 90 wt%; of a propylene homopolymer; B) from 10 wt% to 50wt%; %; of a copolymer of propylene and ethylene having from 30.0 wt% to 70.0wt%, of ethylene derived units; the composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 2.2 and 4.0 dl/g; ii) a MFR L from 0.5 to 100 g/10 min; iii) a xylene soluble fraction ranging from 10 wt% to 50 wt%;
Abstract:
A polypropylene composition comprising: A) from 71 wt% to 91 wt% of a propylene homopolymer B) from 5 wt% to 15 wt%, of a copolymer of propylene and ethylene containing from 18 wt% to 32.0 wt%, of ethylene derived units; C) from 4 wt% to 15 wt%, of a copolymer of propylene and ethylene containing from 75 wt% to 90.0 wt%, of ethylene derived units.
Abstract:
A propylene/ 1-hexene copolymer in which: i) the content of 1-hexene derived units, measured by C13-NMR, ranges from 1.5 wt% to 2.5 wt% and the content of propylene derived units ranges from 97.5 to 98.5 wt. %; ii) melting temperature measured by DSC in the range 148-153°C; iii) the amount of fraction insoluble in xylene at 25°C is higher than 97.0%; iv) has a melt flow rate (MFR) measured according to ISO 1133, 230°C, 2.16 kg ranging from 35 to 65 g/10 min. The copolymer is useful for the production of injection molded articles in particular Twin- Wall injection molding articles.
Abstract:
A film comprising a polypropylene composition comprising: A) from 50 wt% to 90 wt%; of a propylene homopolymer; B) from 10 wt% to 50wt%; of a copolymer of propylene with from 30.0 wt% to 70.0wt%, of ethylene derived units; the sum of the amount of component A) and B) being 100; the composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 2.2 and 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 0.5 to 50 g/10 min; iii) a xylene soluble fraction ranging from 20 wt% to 50 wt%; the polypropylene composition being obtained by a two steps polymerization process wherein the catalyst system contains bismuth.
Abstract:
A propylene ethylene copolymer characterized by the following features: ethylene content of between 1.8 and 10.0% by weight; molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the content of xylene soluble fraction (XS) and ethylene content (C2) fulfill the following relation: XS
Abstract:
A polypropylene composition comprising: A) from 76 wt% to 95 wt% of a propylene homopolymer having: - fraction soluble in xylene at 25°C comprised between 2.0 wt% and 4.5 wt%; - melt flow rate (MFR L according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) ranging from 60.0 to 110.0 g/10 min; B) from 5 wt% to 24 wt%, of a copolymer of propylene and ethylene containing from 75 wt% to 90.0 wt%, of ethylene derived units; wherein in the polypropylene composition: the content of ethylene derived units in the fraction soluble in xylene at 25°C is lower than - the content of ethylene derived units of component B) and ranges from 51.0 wt% to 74.0 wt%, the polypropylene composition has at least two melting points, the higher ranging from 156.0 °C to 166.0 °C and the lower ranging from 90.0 °C to 125.0°C; and the sum of the amounts of component A) and B) being 100 wt%.
Abstract:
A polypropylene composition comprising: from 70 wt% to 90 wt% of a propylene 1-hexene copolymer containing from 1.0 wt% to 5.0 wt% of 1-hexene derived units and a polydispersity index (PI) comprised between 9.2 and 21.3; from 10 wt% to 30 wt%, of a copolymer of propylene and ethylene containing from 45.0 wt% to 65.0 wt%, of ethylene derived units; the sum A) + B) being 100.