公开(公告)号:BR9810666A
公开(公告)日:2000-09-26
申请号:BR9810666
申请日:1998-06-23
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , KOCH JUERGEN , ITTEMAN PETER , SEIBRING JOACHIM , GRABOWSKI SVEN , KEE GRAHAM EDMUND MC , MOSBACH NORBERT , CZAUDERNA BERBHARD , NIESSNER NORBERT , HEINEN HARTMUT
Abstract: A thermoplastic molding composition having little intrinsic color is produced from a graft copolymer and a thermoplastic polymer. The graft copolymer is produced from a soft elastomeric particulate graft base obtained by polymerization of a conjugated diene alone or with a small amount of a monoethylenically unsaturated monomer, upon which is grafted a vinylaromatic monomer and acrylonitrile and optionally another monoethylenically unsaturated monomer. The thermoplastic polymer is a copolymer of a vinylaromatic monomer and acrylonitrile and optionally an additional monoethylenically unsaturated monomer. The thermoplastic molding composition has a low level of intrinsic color coupled with good mechanical properties and can be processed by, for example, extrusion, injection molding, calendaring, blow molding, compression molding, or sintering.
-
公开(公告)号:CZ20000010A3
公开(公告)日:2000-07-12
申请号:CZ20000010
申请日:1998-06-23
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , KOCH JUERGEN , ITTEMANN PETER , SEIBRING JOACHIM , GRABOWSKI SVEN , MC KEE GRAHAM EDMUND , MOSBACH NORBERT , CZAUDERNA BERNHARD , NIESSNER NORBERT , HEINEN HARTMUT
IPC: C08F297/04 , C08L51/06 , C08L55/02
-
公开(公告)号:ES2144862T3
公开(公告)日:2000-06-16
申请号:ES97922967
申请日:1997-05-06
Applicant: BASF AG
Inventor: WEBER MARTIN , SEIBRING JOACHIM
-
公开(公告)号:CZ200010A3
公开(公告)日:2000-07-12
申请号:CZ200010
申请日:1998-06-23
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , KOCH JUERGEN , ITTEMANN PETER , SEIBRING JOACHIM , GRABOWSKI SVEN , MC KEE GRAHAM EDMUND , MOSBACH NORBERT , CZAUDERNA BERNHARD , NIESSNER NORBERT , HEINEN HARTMUT
IPC: C08F297/04 , C08L51/06 , C08L55/02
-
公开(公告)号:ZA9805868B
公开(公告)日:2000-01-10
申请号:ZA9805868
申请日:1998-07-03
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , KOCH JUERGEN , ITTEMANN PETER , SEIBRING JOACHIM , GRABOWSKI SVEN , KEE GRAHAM EDMUND MC , MOSBACH NORBERT , CZAUDERNA BERNHARD , NIEBNER NORBERT , HEINEN HARTMUT
CPC classification number: C08L25/12 , C08F279/04 , C08L25/14 , C08L51/04 , C08L2205/02 , C08L2666/02
-
公开(公告)号:CA2294918A1
公开(公告)日:1999-01-14
申请号:CA2294918
申请日:1998-06-23
Applicant: BASF AG
Inventor: HEINEN HARTMUT , SEIBRING JOACHIM , GUENTHERBERG NORBERT , ITTEMANN PETER , KOCH JUERGEN , MC KEE GRAHAM EDMUND , GRABOWSKI SVEN , NIESSNER NORBERT , MOSBACH NORBERT , CZAUDERNA BERNHARD
Abstract: The invention relates to thermoplastic molding material containing the constituents A) to F), 5 to 80 wt. % of a graft polymer A) with a bimodal particle size distribution, 20 to 95 wt. % of a thermoplastic polymer B) with a viscosity VZ of 50 to 120 ml/g and optionally other thermoplastic polymers C), D) and/or E) based on at least one vinyl-aromatic monomer, and optionally additives F). The inventive material can be obtained by 1) producing the graft polymers A) according to the emulsion polymerization method, 2) mixing the graft polymer A) with polymer B) and, insofar as they are available, the other constituents C), D), E) and/or F) in a mixing device, whereby a substantially molten polymer mixture arises and 3) rapidly cooling the substantially molten polymer mixture.
-
公开(公告)号:DE59503546D1
公开(公告)日:1998-10-15
申请号:DE59503546
申请日:1995-11-14
Applicant: BASF AG
Inventor: MC KEE GRAHAM , MOORS RAINER , GAUSEPOHL HERMANN , SEIBRING JOACHIM
IPC: C08F2/18 , C08F4/04 , C08F4/28 , C08F220/12 , C08F265/04 , C08L51/04
Abstract: PCT No. PCT/EP95/04474 Sec. 371 Date May 12, 1997 Sec. 102(e) Date May 12, 1997 PCT Filed Nov. 14, 1995 PCT Pub. No. WO96/15166 PCT Pub. Date May 23, 1996In the preparation of a rubber-modified molding material, in a first stage, a first mixture (A) contains at least one alkyl acrylate or methacrylate (a) of the formula (I) where R1 is hydrogen or methyl and R2 is alkyl of 1 to 32 carbon atoms, at least one first monomer (b) which forms free radicals on thermal decomposition and, if required, a second monomer (c) or a plurality thereof is polymerized, preferably with free radicals, to give a rubber (B), in a second stage, the resulting rubber (B) is mixed with a third monomer (d) or a plurality thereof, preferably dissolved or swollen therein, to form a second mixture (C), and in a third stage, the second mixture (C) is polymerized with free radicals to give the rubber-modified molding material (D).
-
-
-
-
-
-